| Effect of Adding Methods of Nucleating Agent on Microstructure and Mechanical Properties of Zr Modified Al-Cu-Mg Alloys Prepared by Selective Laser Melting |
WANG Kaidong, LIU Yunzhong( ), ZHAN Qiangkun, HUANG Bin |
| National Engineering Research Center of Near-Net-Shape Forming for Metallic Materials, South China University of Technology, Guangzhou 510640, China |
|
Cite this article:
WANG Kaidong, LIU Yunzhong, ZHAN Qiangkun, HUANG Bin. Effect of Adding Methods of Nucleating Agent on Microstructure and Mechanical Properties of Zr Modified Al-Cu-Mg Alloys Prepared by Selective Laser Melting. Acta Metall Sin, 2022, 58(10): 1281-1291.
|
|
|
Abstract Selective laser melting (SLM) technology is gaining increasing attention in the field of additive manufacturing. Al-Cu-Mg alloy parts manufactured using SLM technology exhibit significant advantages in lightweight design and the integrated formation of complex structural parts in the aerospace field. However, because of their wide freezing ranges, Al-Cu-Mg alloys have a high cracking tendency at a high cooling rate. SLM technology was used to prepare Zr-modified Al-Cu-Mg alloys in this study. Al3Zr particles were synthesized to directly add to Al-Cu-Mg alloy powders, and ZrH2 particles were chosen to form Al3Zr in-situ during SLM processes. The differences between the effects of adding Al3Zr particles directly and forming Al3Zr in-situ on the microstructures and the mechanical properties of SLMed Al-Cu-Mg alloys were analyzed. The results show that the common hot tearing in as-built Al-Cu-Mg alloys all disappear due to the addition of Al3Zr nucleating agent and the in-situ formed Al3Zr is more conducive to refining grains and improving the plasticity and the processing efficiency of SLMed Al-Cu-Mg alloys. When the laser energy density is 370 J/mm3, the grain size of the samples containing Al3Zr and in-situ formed Al3Zr particles are 1.88 and 1.28 μm, respectively. L12-Al3Zr and undissolved or unmelted Al3Zr particles are the nucleation particles generated by initial Al3Zr particles; whereas, they are all metastable Al3Zr (L12-Al3Zr) synthesized in-situ. L12-Al3Zr has a better nucleation ability than initial Al3Zr particles. The ultimate strength of the heat-treated samples with initial Al3Zr particles or in-situ formed Al3Zr can reach (493 ± 2) or (485 ± 10) MPa, respectively. The elongation of the samples with the in-situ formed Al3Zr is more than 30% higher than that of the samples containing Al3Zr particles. SLMed Al-Cu-Mg alloys with in-situ formed Al3Zr are more suitable for medium-high-speed processes because strong Marangoni flow aroused by high laser energy density is unnecessary for in-situ formed Al3Zr to realize the dispersion of the grain refiner.
|
|
Received: 09 February 2021
|
|
|
| Fund: Research and Development Program Project in Key Areas of Guangdong Province(2019B090907001);Major Special Project for Science and Technology Program of Guangdong Provinces(2014B010129002) |
About author: LIU Yunzhong, professor, Tel: (020)87110081, E-mail: yzhliu@scut.edu.cn
|
| 1 |
Zhu H H, Liao H L. Research status of selective laser melting of high strength aluminum alloy [J]. Laser Optoelectron. Prog., 2018, 55: 011402
|
|
朱海红, 廖海龙. 高强铝合金的激光选区熔化成形研究现状 [J]. 激光与光电子学进展, 2018, 55: 011402
|
| 2 |
Aboulkhair N T, Simonelli M, Parry L, et al. 3D printing of aluminium alloys: Additive manufacturing of aluminium alloys using selective laser melting [J]. Prog. Mater. Sci., 2019, 106: 100578
doi: 10.1016/j.pmatsci.2019.100578
|
| 3 |
Zhang L C, Attar H. Selective laser melting of titanium alloys and titanium matrix composites for biomedical applications: A review [J]. Adv. Eng. Mater., 2016, 18: 463
doi: 10.1002/adem.201500419
|
| 4 |
Nie X J, Zhang H, Zhu H H, et al. Analysis of processing parameters and characteristics of selective laser melted high strength Al-Cu-Mg alloys: From single tracks to cubic samples [J]. J. Mater. Process. Technol., 2018, 256: 69
doi: 10.1016/j.jmatprotec.2018.01.030
|
| 5 |
Gui Q W. The influence of heat treatment process on the precipitates and properties of 2024 aluminum alloy [D]. Changsha: Hunan University, 2012
|
|
桂奇文. 热处理工艺对2024铝合金析出相及性能的影响 [D]. 长沙: 湖南大学, 2012
|
| 6 |
DebRoy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components-process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112
doi: 10.1016/j.pmatsci.2017.10.001
|
| 7 |
Casati R, Lemke J N, Alarcon A Z, et al. Aging behavior of high-strength Al alloy 2618 produced by selective laser melting [J]. Metall. Mater. Trans., 2017, 48A: 575
|
| 8 |
Montero-Sistiaga M L, Mertens R, Vrancken B, et al. Changing the alloy composition of Al7075 for better processability by selective laser melting [J]. J. Mater. Process. Technol., 2016, 238: 437
doi: 10.1016/j.jmatprotec.2016.08.003
|
| 9 |
Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys [J]. Nature, 2017, 549: 365
doi: 10.1038/nature23894
|
| 10 |
Zhang H, Zhu H H, Nie X J, et al. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy [J]. Scr. Mater., 2017, 134: 6
doi: 10.1016/j.scriptamat.2017.02.036
|
| 11 |
Wang P, Gammer C, Brenne F, et al. A heat treatable TiB2/Al-3.5Cu-1.5Mg-1Si composite fabricated by selective laser melting: microstructure, heat treatment and mechanical properties [J]. Composites, 2018, 147B: 162
|
| 12 |
Bi J, Lei Z L, Chen Y B, et al. Microstructure and mechanical properties of a novel Sc and Zr modified 7075 aluminum alloy prepared by selective laser melting [J]. Mater. Sci. Eng., 2019, A768: 138478
|
| 13 |
Zhang S Y. Effect of nucleating agent on microstructure and mechanical properties of additive manufactured aluminum alloys [D]. Jinan: Shandong University, 2020
|
|
张书雅. 形核剂对增材制造铝合金显微组织及力学性能的影响 [D]. 济南: 山东大学, 2020
|
| 14 |
Tan Q Y, Zhang J Q, Sun Q, et al. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles [J]. Acta Mater., 2020, 196: 1
doi: 10.1016/j.actamat.2020.06.026
|
| 15 |
Hu L. Effect of nano-TiB2 particles on microstructures and mechanical properties of 2024 aluminum alloy prepared by selective laser melting [D]. Guangzhou: South China University of Technology, 2019
|
|
胡 亮. 纳米TiB2颗粒对激光选区熔化成形2024铝合金显微组织与力学性能的影响 [D]. 广州: 华南理工大学, 2019
|
| 16 |
Nie X J, Zhang H, Zhu H H, et al. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys [J]. J. Alloy. Compd., 2018, 764: 977
doi: 10.1016/j.jallcom.2018.06.032
|
| 17 |
Nayak S S, Pabi S K, Murty B S. High strength nanocrystalline L12-Al3(Ti,Zr) intermetallic synthesized by mechanical alloying [J]. Intermetallics, 2007, 15: 26
doi: 10.1016/j.intermet.2006.02.003
|
| 18 |
Mehta A, Dickson J, Newell R, et al. Interdiffusion and reaction between Al and Zr in the temperature range of 425 to 475oC [J]. J. Phase Equilib. Diffus., 2019, 40: 482
doi: 10.1007/s11669-019-00729-9
|
| 19 |
Simchi A. Direct laser sintering of metal powders: Mechanism, kinetics and microstructural features [J]. Mater. Sci. Eng., 2006, A428: 148
|
| 20 |
Zhang B, Li Y T, Bai Q. Defect formation mechanisms in selective laser melting: A review [J]. Chin. J. Mech. Eng., 2017, 30: 515
doi: 10.1007/s10033-017-0121-5
|
| 21 |
Li D W, Sun T, Yao G C, et al. Preparation of foam aluminum with small pores by melt-based route of ZrH2 [J]. Chin. J. Nonferrous Met., 2010, 20: 143
|
|
李大武, 孙 挺, 姚广春 等. 氢化锆熔体发泡法制备小孔径泡沫铝 [J]. 中国有色金属学报, 2010, 20: 143
|
| 22 |
Dorin T, Ramajayam M, Lamb J, et al. Effect of Sc and Zr additions on the microstructure/strength of Al-Cu binary alloys [J]. Mater. Sci. Eng., 2017, A707: 58
|
| 23 |
Gao Y H, Cao L F, Kuang J, et al. Assembling dual precipitates to improve high-temperature resistance of multi-microalloyed Al-Cu alloys [J]. J. Alloys Compd., 2020, 822: 153629
doi: 10.1016/j.jallcom.2019.153629
|
| 24 |
Zhang F R. Numerical simulation and analysis of the molten pool flow characteristics of laser deep penetration welding [D]. Harbin: Harbin Institute of Technology, 2014
|
|
张芙蓉. 激光深熔焊过程熔池流动特性数值模拟与分析 [D]. 哈尔滨: 哈尔滨工业大学, 2014
|
| 25 |
Tradowsky U, White J, Ward R M, et al. Selective laser melting of AlSi10Mg: influence of post-processing on the microstructural and tensile properties development [J]. Mater. Des., 2016, 105: 212
doi: 10.1016/j.matdes.2016.05.066
|
| 26 |
Zhang D Y, Qiu D, Gibson M A, et al. Additive manufacturing of ultrafine-grained high-strength titanium alloys [J]. Nature, 2019, 576: 91
doi: 10.1038/s41586-019-1783-1
|
| 27 |
Tan Q Y, Zhang J Q, Mo N, et al. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles [J]. Addit. Manuf., 2020, 32: 101034
|
| 28 |
Hunt J D. Steady state columnar and equiaxed growth of dendrites and eutectic [J]. Mater. Sci. Eng., 1984, 65: 75
|
| 29 |
Li Y L. Numerical investigation on temperature field and stress field during selective laser melting of AlSi10Mg [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2015
|
|
李雅莉. 选区激光熔化AlSi10Mg温度场及应力场数值模拟研究 [D]. 南京: 南京航空航天大学, 2015
|
| 30 |
Li B Q. Selective laser melting of AlSi10Mg: Simulation and experiments [D]. Taiyuan: North University of China, 2019
|
|
李保强. 选区激光熔化AlSi10Mg成形过程数值模拟与实验研究 [D]. 太原: 中北大学, 2019
|
| 31 |
Srinivasan D, Chattopadhyay K. Non-equilibrium transformations involving L12-Al3Zr in ternary Al-X-Zr alloys [J]. Metall. Mater. Trans., 2005, 36A: 311
|
| 32 |
Croteau J R, Griffiths S, Rossell M D, et al. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting [J]. Acta Mater., 2018, 153: 35
doi: 10.1016/j.actamat.2018.04.053
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|