Acta Metall Sin  2019, Vol. 55 Issue (9): 1095-1114    DOI: 10.11900/0412.1961.2019.00078
Overview Current Issue | Archive | Adv Search |
Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques
ZHANG Beijiang(),HUANG Shuo,ZHANG Wenyun,TIAN Qiang,CHEN Shifu
High Temperature Materials Research Division, Central Iron & Steel Research Institute, Beijing 100081, China
Cite this article: 

ZHANG Beijiang,HUANG Shuo,ZHANG Wenyun,TIAN Qiang,CHEN Shifu. Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques. Acta Metall Sin, 2019, 55(9): 1095-1114.

Download:  HTML  PDF(51115KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The newly developed high-performance cast-wrought alloys have been widely applied in advanced turbine engines in recent years, particularly, served as turbine disc and compressor disc. The significant breakthrough has been made on the processing techniques for these highly alloyed disc alloys, including the triple-melting of the large-scale ingots with the diameter more than 500 mm, conversion of the large-scale ingot and the processing of fine-grained billets with the diameter more than 300 mm, customization of the microstructures and properties of disc forgings. The chemical compositions can be well controlled on vacuum arc remelting (VAR) ingots, including the ultra-low carbon content lower than 0.011%. The white spots and freckles have been found to be the primary defects on large-scale VAR ingots, which is triggered by the improper re-melting parameters. The metallurgical defects can be identified on fine-grained billets via supersonic inspection. The investigations have shown that the existence of the micro-duplex structure opens a window for the processing of these highly alloyed disc alloys with up to more than 60% mass fraction of precipitates. Via a multicycle thermal-mechanical processing technique, the hot working process of the disc alloys, can be achieved in a cost-effective way, and the un-recrystallized grains can also be eliminated efficiently. The above-mentioned techniques have greatly promoted the development and application of the high-performance disc alloys, such as GH4065, GH4720, GH4175 and GH4975, et al. These alloys can provide a promising solution of high reliability combined with low life cycle cost for military and commercial gas turbines. Nonetheless, in order to maximize the advantageous of cast-wrought disc alloys on reliability and cost-effective ratio, the comprehensive understanding about the prevention and identification of metallurgical defects, increase in the yield rate of materials during conversion, processing of fine-grained billets and dual-property disc forgings, is still needed.

Key words:  Ni-based superalloy      disc forging      chemical composition      processing      microstructure and property     
Received:  22 March 2019     
ZTFLH:  TG146.1  
Fund: Supported by National Science and Technology Major Project(2017-VI-0015-0087,2017-VI-0018-0090)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2019.00078     OR     https://www.ams.org.cn/EN/Y2019/V55/I9/1095

Fig.1  Development of cast-wrought disc superalloys abroad
AlloyMass fraction ofMass fraction of γ′γ-γ′ mismatch at 760 ℃γ′ solvus temperature
Al+Ti+Nb / %at 760 ℃ / %%℃
GH45865.029-0.3551072
GH47427.837+0.2731095
GH40656.636-0.0161113
GH40798.546+0.1311132
GH47207.543+0.0881158
GH41569.053+0.0031165
GH41519.954-0.1281171
GH417511.055-0.0801176
GH49759.264-0.0791210
Table 1  Characteristic parameters of highly alloyed cast-wrought disc alloys[3,4,5,8,14,23,24,25,26,27,28]
Fig.2  Relationship between stress rupture property and the concentration of alloying elements of disc alloys
Fig.3  Relationship between formation temperature of MC carbides and C content in alloy GH4065(a) phase diagram (b) details of MC carbides formation temperature
Fig.4  Schematic of standard processing route of cast-wrought disc forgings and associated key techniques (VIM—vacuum induction melting, ESR—electroslag remelting, VAR—vacuum arc remelting)
Fig.5  Clean white spot identified on a GH4586 disc forging produced via double-melting technique(a) macro-scale morphology (b) optical image
Fig.7  Coarse-grained macrostructures on billet induced by improper conversion techniques(a) low-magnification (b) residual as-cast structures
Fig.8  Super-plasticity of γ+γ' microduplex of disc alloys with various γ' mass fractions (deformed at the temperature of 100 ℃ lower than γ' solvus temperature and the strain rate of 1×10-3 s-1)
Fig.6  A freckle identified on the billet of alloy GH4065 with diameter of 300 mm(a~c) macro-scale morphologies of the freckle under various conditions of incident light ((a, b) transverse, (c)longitudinal)(d~h) EPMA mappings of alloying elements distribution
Fig.9  Numerical simulation of the trigger and growth of freckles during the VAR re-melting process (f—solid fraction in mushy zone)(a) f map (b, c) solute distribution (d) macro-scale flow pattern of liquid phase in the mushy zone
Fig.10  Morphological evolution of freckles during conversion and their supersonic identification on GH4065 billets(a) a freckle in coarse-grained structure(b, c) morphologies of the freckle in γ+γ' microduplex(d) C-scan plot showing a freckle on fine-grained billet indicated by arrow (Color scale is for C-scan map)
Fig.11  Discrete dirty white spot on GH4065 disc forging identified by supersonic inspection(a) macro-scale morphology of white spot (blue arrow) and stringers (red arrows)(b) optical image of stringers (indicated by red arrows in Fig.11a)(c) C-scan plot showing a defect on disc forging(d~k) EPMA analyses identified the stringer as inclusions
Fig.12  Interaction between dislocations and γ' precipitates during hot working process of disc alloys(a) dens dislocations induced by strain ageing effect in alloy GH4586(b) low dislocation density in γ+γ' microduplex in alloy GH4065(c) HRTEM image of γ-γ' interface in Fig.12b
Fig.13  Special γ-γ' configurations developed during hot working process of alloy GH4065 due to the mechanism of strain induced discontinuous precipitation of γ' phase(a) original structure in single austenite region(b) fine and dispersed γ' precipitate during deformation in two-phase region(c, d) optical and SEM images of discontinuous precipitated γ', respectively(e, f) EBSD phase map and low angle misorientation (5°), respectively
Fig.14  Hot working plasticity of alloy GH4065 characterized by percent area reduction of tension tests(a) as-cast structures after solutioning treatment (b) γ+γ' microduplex (c) schematic of original specimen
Fig.15  Morphologies of γ+γ' microduplex of disc alloys with various γ' mass fractions during superplastic deformation at the temperature of 100 ℃ lower than γ' solvus temperature (given in Table 1) and strain rate of 1×10-3 s-1(a) GH4065 (b) GH4720 (c) GH4175 (d) GH4975
Fig.16  Large-scale disc forgings and the macrostructural homogeneity of alloy GH4065(a) compressor blisk and low-pressure turbine disc(b) macrostructure of disc forging
Fig.17  As-solutioning microstructures of the full-scale disc forgings optical images of alloy GH4065 (a, b) and GH4175 (c), TEM image of dislocation free γ+γ' microduplex in Fig.17a (d), TEM images of small un-recrystallized grains indicated by arrows in Fig.17b (e, f)
[1] ReedR C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 236
[2] DonachieM J, DonachieS J. Superalloys: A Technical Guide [M]. 2nd Ed., Ohio: ASM International, 2002: 120
[3] ShiC X, ZhongZ Y. Forty years of superalloy R & D in China [J]. Acta Metall. Sin., 1997, 33: 1
[3] 师昌绪, 仲增墉. 中国高温合金40年 [J]. 金属学报, 1997, 33: 1
[4] JiangH F. Requirements and forecast of turbine disk materials [J]. Gas Turb. Exp. Res., 2002, 15(4): 1
[4] 江和甫. 对涡轮盘材料的需求及展望 [J]. 燃气涡轮试验与研究, 2002, 15(4): 1)
[5] WangX D, WangH C. Improved development superalloys, promote the aero-engine development [A]. The Thirteenth Session of the Annual China Superalloys Conference [C]. Beijing: Metallurgical Industry Press, 2015: 3
[5] (王旭东, 王海川. 改进发展高温合金, 推动航空发动机研制 [A]. 第十三届中国高温合金年会论文集 [C]. 北京: 冶金工业出版社, 2015: 3)
[6] SimsC T, StoloffN S, HagelW C. Superalloys II—High Temperature Materials for Aerospace and Industrial Power [M]. New York: John Wiley & Sons, 1987: 32
[7] DevauxA, GeorgesE, HéritierP. Development of new C&W superalloys for high temperature disk applications [J]. Adv. Mater. Res., 2011, 278: 405
[8] High Temperature Material Branch of the Chinese Society for Metals. China Superalloys Handbook (Volume One) [M]. Beijing: China Standards Press, 2012: 891
[8] (中国金属学会高温材料分会. 中国高温合金手册/上卷: 变形高温合金 焊接用高温合金丝 [M]. 北京: 中国标准出版社, 2012: 891)
[9] WilliamsJ C, Starke JrE A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775
[10] FangB, JiZ, LiuM, , et al. Study on constitutive relationships and processing maps for FGH96 alloy during two-pass hot deformation [J]. Mater. Sci. Eng., 2014, A590: 255
[11] CarterJ L W, KuperM W, UchicM D, , et al. Characterization of localized deformation near grain boundaries of superalloy René-104 at elevated temperature [J]. Mater. Sci. Eng., 2014, A605: 127
[12] FindleyK O, SaxenaA. Low cycle fatigue in René 88DT at 650 ℃: Crack nucleation mechanisms and modeling [J]. Metall. Mater. Trans., 2006, 37A: 1469
[13] ViswanathanG B, SarosiP M, HenryM F, , et al. Investigation of creep deformation mechanisms at intermediate temperatures in René 88 DT [J]. Acta Mater., 2005, 53: 3041
[14] HuangQ Y, LiH K. Superalloy [M]. Beijing: Metallurgical Industry Press, 2000: 385
[14] 黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 385)
[15] DeckerR F. The evolution of wrought age-hardenable superalloys [J]. JOM, 2006, 58(9): 32
[16] PreliF R, FurrerD. Lessons learned from the development, application and advancement of alloy 718 [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 3
[17] HayesR W, UnocicR R, NasrollahzadehM. Creep deformation of allvac 718Plus [J]. Metall. Mater. Trans., 2015, 46A: 218
[18] LiuY C, ZhangH J, GuoQ Y, , et al. Microstructure evolution of Inconel 718 superalloy during hot working and its recent development tendency [J]. Acta Metall. Sin., 2018, 54: 1653
[18] 刘永长, 张宏军, 郭倩颖等. Inconel 718变形高温合金热加工组织演变与发展趋势 [J]. 金属学报, 2018, 54: 1653
[19] DevauxA, PicquéB, GervaisM F, , et al. AD730TM—A new nickel-based superalloy for high temperature engine rotative parts [A]. Superalloys 2012 [C]. Warrendale, PA: TMS, 2012: 911
[20] CrozetC, DevauxA, ForestierR, , et al. Effect of ingot size on microstructure and properties of the new advanced AD730TM superalloy [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 437
[21] HeaneyJ A, LasondeM L, PowellA M, , et al. Development of a new cast and wrought alloy (René 65) for high temperature disk applications [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 67
[22] ReedR C, MotturaA, CruddenD J. Alloys-by-design: Towards optimization of compositions of nickel-based superalloys [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 15
[23] ShiC X, ZhongZ Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281
[23] 师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281
[24] LongZ D, ZhuangJ Y, DengB, , et al. A new method to improve the hot workability of high strength Ni-based superalloys [J]. Acta Metall. Sin., 1999, 35: 1211
[24] 龙正东, 庄景云, 邓 波等. 一种提高高强化高温合金热加工性能的新方法 [J]. 金属学报, 1999, 35: 1211
[25] ZhongZ Y, ZhuangJ Y. Development of several important problems on producing technologies of wrought superalloy [J]. J. Iron Steel Res., 2003, 15: 1
[25] 仲增墉, 庄景云. 变形高温合金生产工艺中几个重要问题的研究和进展 [J]. 钢铁研究学报, 2003, 15: 1
[26] DongJ X, LiL H, LiH Y, , et al. Effect of extent of homogenization on the hot deformation recrystallization of superalloy ingot in cogging process [J]. Acta Metall. Sin., 2015, 51: 1207
[26] 董建新, 李林翰, 李浩宇等. 高温合金铸锭均匀化程度对开坯热变形的再结晶影响 [J]. 金属学报, 2015, 51: 1207
[27] DuJ H, ZhaoG P, DengQ, , et al. Development of wrought superalloy in China [J]. J. Aeron. Mater., 2016, 36(3): 27
[27] 杜金辉, 赵光普, 邓 群等. 中国变形高温合金研制进展 [J]. 航空材料学报, 2016, 36(3): 27)
[28] ZhangB J, ZhaoG P, ZhangW Y, , et al. Investigation of high performance disc alloy GH4065 and associated advanced processing techniques [J]. Acta Metall. Sin., 2015, 51: 1227
[28] 张北江, 赵光普, 张文云等. 高性能涡轮盘材料GH4065及其先进制备技术研究 [J]. 金属学报, 2015, 51: 1227
[29] ZhangB J, ZhaoG P, ZhangW Y, , et al. Deformation mechanisms and microstructural evolution of γ+γ' duplex aggregates generated during thermomechanical processing of nickel-base superalloys [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 487
[30] Van Den AvyleJ A, BrooksJ A, PowellA C. Reducing defects in remelting processes for high-performance alloys [J]. JOM, 1998, 50(3): 22
[31] AuburtinP, WangT, CockcroftS L, , et al. Freckle formation and freckle criterion in superalloy castings [J]. Metall. Mater. Trans., 2000, 31B: 801
[32] WangZ X, HuangS, ZhangB J, , et al. Study on freckle of a high-alloyed GH4065 Nickel base wrought superalloy [J]. Acta Metall. Sin., 2019, 55: 417
[32] 王资兴, 黄 烁, 张北江等. 高合金化GH4065镍基变形高温合金点状偏析研究 [J]. 金属学报, 2019, 55: 417
[33] GenereuxP D, BorgC A. Characterization of freckles in a high strength wrought nickel superalloy [A]. Superalloys 2000 [C]. Warrendale, PA: TMS, 2000: 19
[34] CharpagneM A, CharpagneM A, BillotT, , et al. Heteroepitaxial recrystallization observed in René 65TM and Udimet 720TM: A new recrystallization mechanism possibly occurring in all low lattice mismatch γ-γ' superalloys? [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 417
[35] AndrewW, AudeL, AudeL, , et al. Thermal stability of cast and wrought alloy Rene 65 [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 793
[36] WlodekS T, KellyM, AldenD A. The structure of René 88 DT [A]. Superalloys 1996 [C]. Warrendale, PA: TMS, 1996: 129
[37] BryantD J, McIntoshD G. The manufacture and evaluation of a large turbine disc in cast and wrought alloy 720Li [A]. Superalloys 1996 [C]. Warrendale, PA: TMS, 1996: 713
[38] ZhangB J, ZhaoG P, JiaoL Y, , et al. Influence of hot working process on microstructures of superalloy GH4586 [J]. Acta Metall. Sin., 2005, 41: 351
[38] 张北江, 赵光普, 焦兰英等. 热加工工艺对GH4586合金微观组织的影响 [J]. 金属学报, 2005, 41: 351
[39] ZhangB J, ZhaoG P, XuG H, , et al. Hot deformation behavior and micro-structure evolution of superalloy GH742 [J]. Acta Metall. Sin., 2005, 41: 1207
[39] 张北江, 赵光普, 胥国华等. GH742合金热变形行为与微观组织演化 [J]. 金属学报, 2005, 41: 1207
[40] SchafrikR E. Materials for a non-steady-state world [J]. Metall. Mater. Trans., 2016, 47B: 1505
[41] SunX F, YinF S, LiJ G, , et al. Solidification behavior of a cast nickel-base superalloy [J]. Acta Metall. Sin., 2003, 39: 27
[41] 孙晓峰, 殷凤仕, 李金国等. 一种铸造镍基高温合金的凝固行为 [J]. 金属学报, 2003, 39: 27
[42] ZhangJ, HuangT W, LiuL, , et al. Advances in solidification characteristics and typical casting defects in nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2015, 51: 1163
[42] 张 军, 黄太文, 刘 林等. 单晶高温合金凝固特性与典型凝固缺陷研究 [J]. 金属学报, 2015, 51: 1163
[43] ZhangJ, LouL H. Basic research in development and application of cast superalloy [J]. Acta Metall. Sin., 2018, 54: 1637
[43] 张 健, 楼琅洪. 铸造高温合金研发中的应用基础研究 [J]. 金属学报, 2018, 54: 1637
[44] Carter JrW T, JonesR M F. Nucleated casting for the production of large superalloy ingots [J]. JOM, 2005, 57(4): 52
[45] MonajatiH, TaheriA K, JahaziM, , et al. Deformation characteristics of isothermally forged UDIMET 720 nickel-base superalloy [J]. Metall. Mater. Trans., 2005, 36A: 895
[46] RobsonJ D. Modeling competitive continuous and discontinuous precipitation [J]. Acta Mater., 2013, 61: 7781
[47] CantwellP R, TangM, DillonS J, , et al. Grain boundary complexions [J]. Acta Mater., 2014, 62: 1
[48] BondB J, O'BrienC M, RussellJ L, , et al. René 65 billet material for forged turbine components [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 107
[49] LarrouyB, VillechaiseP, CormierJ, , et al. Influence of both temperature and γ' distribution on the development of strain incompatibilities at grain boundaries at low temperature in the UdimetTM 720 Li superalloy [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 713
[50] ValitovV A. Formation of nanocrystalline structure upon severe thermomechanical processing and its effect on the superplastic properties of nickel base alloys [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 739
[51] TileyJ, ViswanathanG B, SrinivasanR, , et al. Coarsening kinetics of γ' precipitates in the commercial nickel base Superalloy René 88 DT [J]. Acta Mater., 2009, 57: 2538
[52] MacSleyneJ, UchicM D, SimmonsJ P, , et al. Three-dimensional analysis of secondary γ' precipitates in René-88 DT and UMF-20 superalloys [J]. Acta Mater., 2009, 57: 6251
[53] RadisR, SchafferM, AlbuM, , et al. Multimodal size distributions of γ' precipitates during continuous cooling of UDIMET 720 Li [J]. Acta Mater., 2009, 57: 5739
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[4] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[5] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[6] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[7] XIONG Tianying, WANG Jiqiang. Research Progress of Cold Spray in Institute of Metal Research, Chinese Academy of Sciences[J]. 金属学报, 2023, 59(4): 537-546.
[8] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[9] PENG Liming, DENG Qingchen, WU Yujuan, FU Penghuai, LIU Ziyi, WU Qianye, CHEN Kai, DING Wenjiang. Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review[J]. 金属学报, 2023, 59(1): 31-54.
[10] REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao. Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition[J]. 金属学报, 2022, 58(2): 206-214.
[11] JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying. Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP[J]. 金属学报, 2021, 57(6): 703-716.
[12] ZHU Yuping, Naicheng SHENG, XIE Jun, WANG Zhenjiang, XUN Shuling, YU Jinjiang, LI Jinguo, YANG Lin, HOU Guichen, ZHOU Yizhou, SUN Xiaofeng. Precipitation Behavior of W-Rich Phases in a High W-Containing Ni-Based Superalloys K416B[J]. 金属学报, 2021, 57(2): 215-223.
[13] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[14] LIU Jian, PENG Qin, XIE Jianxin. Grain Structure and Metallurgical Defects Regulation of Selective Laser Melted René 88DT Superalloy[J]. 金属学报, 2021, 57(2): 191-204.
[15] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
No Suggested Reading articles found!