| RECALESCENCE EFFECT SIMULATION AND MICROSTRUCTURE EVOLUTION OF UNDERCOOLED Fe82B17Si1 ALLOY |
CHEN Zheng1,2( ), YANG Yanan1, CHEN Qiang1, XU Junfeng2, TANG Yueyue1, LIU Feng2 |
1 School of Materials Science and Engineering, China University of Mining and Technology, Xuzhou 221116 2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi′an 710072 |
|
Cite this article:
CHEN Zheng, YANG Yanan, CHEN Qiang, XU Junfeng, TANG Yueyue, LIU Feng. RECALESCENCE EFFECT SIMULATION AND MICROSTRUCTURE EVOLUTION OF UNDERCOOLED Fe82B17Si1 ALLOY. Acta Metall Sin, 2014, 50(7): 795-801.
|
|
|
Abstract 通过熔融玻璃净化与循环过热相结合的方法获得过冷度ΔT=6~280 K范围内的Fe82B17Si1共晶合金的凝固组织演变; 结合突变方程和JMAK模型拟合凝固过程的冷却曲线, 拟合结果符合Fe82B17Si1共晶合金的组织类型及形态随过冷度的变化规律. 结果表明, 当6 K≤ΔT<75 K时, Fe82B17Si1合金中形成了复杂规则共晶及准规则共晶组成的混合共晶组织; 当75 K≤ΔT<180 K时, 凝固组织由混合共晶组织和深过冷非规则共晶组织组成; 当180 K≤ΔT<250 K时, 凝固组织由不同含量的初生a-Fe相和枝晶间深过冷非规则共晶组织组成; 当ΔT >250 K时, 凝固组织为完全非规则共晶组织.
|
|
Received: 13 December 2013
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.51101169), Fundamental Research Funds for the Central Universities (No.2014QNA07) and China Postdoctoral Science Foundation (No.2013M540475) |
| [1] |
Yang C L, Yang G C, Lu Y P, Chen J Q, Zhou Y H. Acta Metall Sin, 2005; 41: 1053
|
|
(杨长林, 杨根仓, 卢一平, 陈甲琪, 周尧和. 金属学报, 2005; 41: 1053)
|
| [2] |
Goetzinger R, Barth M, Herlach D M. J Appl Phys, 1998; 84: 1643
|
| [3] |
Leonhardt M, Loser W, Lindenkreuz H G. Mater Sci Eng, 1999; A271: 31
|
| [4] |
Lu Y P, Yang G C, Xi Z Z, Wang H P, Zhou Y H. Mater Lett, 2005; 59: 1558
|
| [5] |
Lu Y P, Yang G C, Liu F, Wang H P, Zhou Y H. Mater Lett, 2007; 61: 987
|
| [6] |
Merz G D, Kattamis T Z. Metall Trans, 1977; 8A: 295
|
| [7] |
Croker M N, Fidler R S, Smith R W. Proc Roy Soc Lond, 1973; 335A: 15
|
| [8] |
Lu Y P, Yang G C, Liu F, Wang H P, Zhou Y H. Eur Phys Lett, 2006; 74: 281
|
| [9] |
Lu Y P, Liu F, Yang G C, Yang C L, Zhou Y H. Appl Phys Lett, 2006; 89: 241902
|
| [10] |
Wei B, Yang G C, Zhou Y H. Acta Metall, 1991; 39: 1249
|
| [11] |
Chu M G, Shionara Y, Flemings M C. Metall Trans, 1984; 15A: 1303
|
| [12] |
Murty Y, Kattamis T Z. J Cryst Growth, 1974; 22: 219
|
| [13] |
Wang H P, Yao W J, Wei B. Appl Phys Lett, 2006; 89: 201905
|
| [14] |
Bottinger W J, Aziz M J. Acta Metall, 1989; 37: 3379
|
| [15] |
Battezzati L, Antonione C, Baricco M. J Alloys Compd, 1997; 247: 164
|
| [16] |
Loser W, Hermann R, Leonhardt R. Mater Sci Eng, 1997; A224: 53
|
| [17] |
Lu Y P, Yang G C, Yang C L,Wang H P, Zhou Y H. Progress Nat Sci, 2006; 16: 287
|
| [18] |
Duhaj P, Švec P. Mater Sci Eng, 1997; A226-228: 245
|
| [19] |
Schroers J, Holland-Moritz D, Herlach D M. Mater Sci Eng A, 1997; 226-228: 990
|
| [20] |
Luborsky F E. Amorphous Metallic Alloys. London: Butterworth & Co., 1983: 381
|
| [21] |
Zhang Z Z. PhD Dissertation, Northwestern Polytechnical University, Xi′an, 1993
|
|
(张振忠. 西北工业大学博士学位论文, 西安, 1993)
|
| [22] |
Saleh A M, Clemente R A. J Appl Phys, 2004; 43: 3624
|
| [23] |
Emadi D, Whiting L, Djurdjevic M, Kierkus W T, Sokolowski J. MJoM, 2004; 10: 91
|
| [24] |
Gandin Ch-A, Mosbah S, Volkmann Th, Herlach D M. Acta Mater, 2008; 56: 3023
|
| [25] |
Yang W, Liu F, Liu H, Wang H F, Yang G C, Zhou Y H. J Cryst Growth, 2009; 311: 3225
|
| [26] |
Liu F, Sommer F, Mittemeijer E J. J Mater Sci, 2004; 39: 1621
|
| [27] |
Xu J F, Liu F, Zhang K, Gong M M. Mater Sci Technol, 2012; 28: 274
|
| [28] |
Christian J W. The Theory of Transformation in Metals and Alloys. OXford: Pergamon Press, 2002: 623
|
| [29] |
Xu J F, Liu F, Zhang K, Gong M M. Mater Sci Technol, 2012; 28: 274
|
| [30] |
Valiev R Z, Korasilnikov N A, Tzenev N K. Mater Sci Eng, 1991; A137: 35
|
| [31] |
Zhang Z Z, Song G S, Yang G C. Progress Nat Sci, 2000; 10: 560
|
|
(张振忠, 宋广生, 杨根仓. 自然科学进展, 2000; 10: 560)
|
| [32] |
Fras E, Lopez H F. Metall Mater Trans, 1999; 30B: 927
|
| [33] |
Saleh A M, Clemente R A. J Appl Phys, 2004; 43: 3624
|
| [34] |
Raghavan V. Phase Diagrams of Ternary Iron Alloys Part 6A. New Delhi: Electronic Publishing Center, Green Park Extension. 1993: 11, 406
|
| [35] |
Boettinger W J, Coriell S R, Trivedi R. Principles Technol, 1988; (IV): 13
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|