| EFFECT OF 0.037%H ON HIGH TEMPERATURE DEFORMATION BEHAVIOR OF A CAST Ti-45Al-5Nb-0.8Mo-0.3Y ALLOY |
| WEN Daosheng, ZONG Yingying, XU Wenchen, YANG Danmei, SHAN Debin |
| Department of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001 |
|
Cite this article:
WEN Daosheng, ZONG Yingying, XU Wenchen, YANG Danmei, SHAN Debin. EFFECT OF 0.037%H ON HIGH TEMPERATURE DEFORMATION BEHAVIOR OF A CAST Ti-45Al-5Nb-0.8Mo-0.3Y ALLOY. Acta Metall Sin, 2013, 49(11): 1428-1432.
|
|
|
Abstract TiAl-based alloys have been regarded as potential structural materials for the aerospace industry because of their high specific strength at elevated temperature, good creep properties and excellent resistance to oxidation. However, their low room temperature ductility and bad high temperature deformability are the considerable barriers to wide application of such alloys. It has been reported that thermo hydrogen treatment (THT) was an effective way to improve the formability of Ti-Al binary alloys. However, up to now few works have been done about the effect of THT on the mechanical properties of utilizable TiAl-based intermetallic compounds. So, the effect of hydrogen on high temperature deformation behaviors of a utilizable TiAl-based intermetallic compound, Ti-45Al-5Nb-0.8Mo-0.3Y alloy, was investigated. Isothermal hot compression tests of the cast Ti-45Al-5Nb-0.8Mo-0.3Y alloy containing 0 and 0.037%H (mass fraction) were carried out by use of a hot simulator at 1150 and 1200℃, with strain rates of 0.1 and 0.01 s-1, and their microstructures were studied using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results showed that hydrogen was able to decrease high temperature deformation flow stress and refine microstructure, which led to an improvement of the hot formability. Comparing with the unhydrogenated alloy, the hydrogenated alloy presented a reduction of peak flow stress, approximately 25% when deformed at 1200℃ and strain rate of 0.01 s-1.The lamellar spacing of Hydrogenated Ti-45Al-5Nb-0.8Mo-0.3Y alloy was 265 nm, 77 nm less than that of the unhydrogenated alloy, which was mainly owing to hydrogen-increased β phase content. Besides, the increase of β phase with good high temperature plasticity was one of the main reasons for the decrease of flow stress of the hydrogenated alloy. Hydrogen made the peak strain of true stress and strain curves of the hydrogenated alloy occur earlier than that of the unhydrogenated alloy, which indicated that hydrogen promoted dynamic recrystallization of the hydrogenated alloy to decrease the flow stress. The dynamic recrystallization of β phase was found in the hydrogenated alloy, but not in the unhydrogenated alloy. Comparing with the unhydrogenated alloy, the density of dislocation of the hydrogenated alloy was lower because hydrogen induced the movement of dislocation. More twinning of γ phase occurred in the hydrogenated alloy, which assisted the alloy in high temperature deformation to some extent. In summary, hydrogen-induced dislocation movement, hydrogen-promoted dynamic recrystallization and twinning, and hydrogen-increased β phase content were the main reasons for the decrease of high temperature deformation flow stress of the hydrogenated Ti-45Al-5Nb-0.8Mo-0.3Y alloy.
|
|
Received: 22 August 2013
|
| [1] Loria E A. Intermetallics, 2001; 9: 997
[2] Li C G, Fu H Z, Yu Q. Materials in Aerospace. Beijing: National Defense Industry Press,2002: 16
(李成功, 傅恒志, 于翘. 航空航天材料. 北京: 国防工业出版社, 2002: 16)
[3] Venkatesware R K T, Kim Y W, Muhlstein C L, Ritchie R O. Mater Sci Eng, 1995; A192-193: 474
[4] Kim Y W. JOM, 1995; 47(7): 39
[5] Wu X H. Intermetallics, 2006; 14: 1114
[6] Chen Y Y, Niu H Z, Kong F T, Xiao S L. Intermetallics, 2011; 19: 1405
[7] Anisimova L I. Met Sci Heat Treat, 1992; 34(2): 143
[8] Li F, Chen Y X, Wan X J, Wang Q J, Liu Y Y. Aata Metall Sin, 2006; 42: 143
(李芳, 陈业新, 万晓景, 王青江, 刘羽寅. 金属学报, 2006; 42: 143)
[9] Shen C C, Yu C Y, Perng T P. Acta Mater, 2009; 57: 868
[10] Zhang Y, Zhang S Q. Scr Mater, 1997; 37: 1315
[11] Zong Y Y. PhD Dissertation, Harbin Institute of Technology, 2007
(宗影影. 哈尔滨工业大学博士学位论文, 2007)
[12] Zhang Y, Zhang S Q, Tao C H. Aata Metall Sin, 1996; 32: 235
(张勇, 张少卿, 陶春虎. 金属学报, 1996; 32: 235)
[13] Liu X W. PhD Dissertation, Harbin Institute of Technology, 2011
(刘鑫旺. 哈尔滨工业大学博士学位论文, 2011)
[14] Lin J P, Cheng G L. Mater China, 2009; 28(1): 31
(林均品, 陈国良. 中国材料进展, 2009; 28(1): 31)
[15] Sakai T. J Mater Process Technol, 1995; 53: 349
[16] Goken M, Kempf M, Nix W D. Acta Mater, 2001; 49: 903
[17] Liu X W, Su Y Q, Luo L S, Liu J P, Guo J J, Fu H Z. Int J Hydrogen Energy, 2010; 35: 13322
[18] Liu X W, Su Y Q, Luo L S, Li K, Dong F Y, Guo J J, Fu H Z. Int J Hydrogen Energy, 2011; 36: 3260
[19] Senkov O N, Froes F H. Int J Hydrogen Energy, 1999; 24: 565
[20] Murzinova M A, Salishchev G A, Afonichev D D. Int J Hydrogen Energy, 2002; 27: 775
[21] Bashkin I O, Ponyatovskiy Y G, Senkov O N, Malyshev V Y. Phys Met Metallogr, 1990; 69(2): 67
[22] Shan D B, Zong Y Y, Lv Y, Guo B. Scr Mater, 2008; 58: 449
[23] Semiatin S L, Seetharaman V, Weiss I. Mater Sci Eng, 1999; A263: 257
[24] Semiatin S L, Bieler T R. Acta Mater, 2001; 49: 3565
[25] Zong Y Y, Shan D B, Lv Y, Guo B. Int J Hydrogen Energy, 2007; 32: 3936
[26] Yuan B G, Li C F, Yu H P, Sun D L. Mater Sci Eng, 2010; A527: 4185 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|