Please wait a minute...
Acta Metall Sin  2013, Vol. 49 Issue (11): 1374-1380    DOI: 10.3724/SP.J.1037.2013.00398
Current Issue | Archive | Adv Search |
EFFECTS OF GROWTH RATE ON PRIMARY PHASE AND MICROSTRUCTURES OF DIRECTIONALLY SOLIDIFIED Ti-46Al-2Cr-2Nb ALLOY
ZHANG Yuan, LIU Guohuai, LI Xinzhong, CHEN Ruirun, SU Yanqing, GUO Jingjie, FU Hengzhi
School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
Cite this article: 

ZHANG Yuan, LIU Guohuai, LI Xinzhong, CHEN Ruirun, SU Yanqing, GUO Jingjie, FU Hengzhi. EFFECTS OF GROWTH RATE ON PRIMARY PHASE AND MICROSTRUCTURES OF DIRECTIONALLY SOLIDIFIED Ti-46Al-2Cr-2Nb ALLOY. Acta Metall Sin, 2013, 49(11): 1374-1380.

Download:  PDF(1592KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

TiAl alloys with fully lamellar structure has been intensively studied for excellent fracture toughness and creep properties. Directional solidification is an effective way to control the lamellar structure. Thus it is important to investigate the effect of solidification parameters on the structure of TiAl alloys during directional solidification. In this work, microstructures of directionally solidifiedTi-46Al-2Cr-2Nb (atomic fraction, %) alloy has been investigated throughBridgman-type directional solidification experiment at constant temperaturegradient and wide range of growth rates (v=10-120 μm/s). The type of primary phase,the primary dendritic arm spacing (λ1), the secondary dendritic arm spacing (λ2) and the lamellar spacing (λe) are investigated. It is found that: the primary phase of the specimenstransformed from β phase to α phase with the increase of growth rates; the transformation trend of primary phases with growth rates can be predicted by the phase selection model based on the highest interface temperature criterion. λ1, λ2, andλe all decrease with the increasing of v. The relationship between λ1 and v is not affected by the transformation of primary phases, which follows λ1=700.6v-0.24 relationship. However the relationship between λ2 and v is associated with the type of primary phases, λ2 and v followsλ2=44.0v-0.10 relationship when β is the primary phases, while follows λ2=57.3v-0.23 relationship when the primary phase has transformed to α phase. The relationship between λe and v can be expressed by λe=16.4v-0.76.Compared with TiAl binary alloys, lamellar spacing is more effectively refined by increasing the growth rates in Ti-46Al-2Cr-2Nb alloy.

Key words:  TiAl alloy      directional solidification      primary phase      microstructure     
Received:  10 July 2013     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2013.00398     OR     https://www.ams.org.cn/EN/Y2013/V49/I11/1374

[1] Yamaguchi M, Johnson D R, Lee H N, Inui H.  Intermetallics, 2000; 8: 511

[2] Kim S E, Lee Y T, Oh M H, Inui H, Yamaguchi M.  Intermetallics, 2000; 8: 399
[3] Zollinger J, Lapin J, Daloz D, Combeau H.  Intermetallics, 2007; 15: 1343
[4] Chen G L, Lin J P.  Physical Metallugry for Ordered Intermetallics. Beijing: Metallurgical Industry Press, 1999: 183
(陈国良, 林均品. 有序金属间化合物结构材料物理金属学基础. 北京: 冶金工业出版社, 1999: 183)
[5] Johnson D R.  Acta Mater, 1997; 45: 2523
[6] Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T.  Acta Mater, 2006; 54: 1077
[7] Xiao Z X.  PhD Dissertation, Beihang University, 2011
(肖志霞. 北京航空航天大学博士学位论文, 2011)
[8] Xiao Z X, Zheng L J, Yang L L, Yan J, Zhang H.  Acta Metall Sin, 2010; 10: 1223
(肖志霞, 郑立静, 杨莉莉, 闫洁, 张虎. 金属学报, 2010; 10: 1223)
[9] Fan J L, Li X Z, Su Y Q, Chen R R, Guo J J, Fu H Z.  J Cryst Growth, 2011; 337: 52
[10] Fan J L, Li X Z, Su Y Q, Chen R R, Guo J J, Fu H Z.  Appl Phys, 2011; 105A: 239
[11] Li X Z, Sun T, Yu C X, Su Y Q, Cao Y Z, Guo J J, Fu H Z.  Acta Metall Sin, 2009; 45: 1479
(李新中, 孙涛, 于彩霞, 苏彦庆, 曹勇智, 郭景杰, 傅恒志. 金属学报, 2009; 45: 1479)
[12] Thomas M, Bacos M T.  High Temp Mater, 2011; 3: 7
[13] Nie G.  PhD Dissertation, Harbin Institute of Technology, 2012
(聂革. 哈尔滨工业大学博士学位论文, 2012)
[14] Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, Wee D M.  Mater Sci Eng, 1997; A239-240: 570
[15] Su Y Q, Liu C, Li X Z, Guo J J, Li B S, Jia J, Fu H Z.  Intermetallics, 2005; 13: 267
[16] Hunt J D. In: Argent B B ed.,  International Conference on Solidification and Casting of Metals. London: The Metals Society, 1979: 3
[17] Kurz W, Fisher D J.  Acta Mater, 1981; 29: 11
[18] Trivedi R.  Metall Mater Trans, 1984; 15A: 977
[19] Fan J L, Li X Z, Su Y Q, Chen R R, Guo J J, Fu H Z.  Mater Chem Phys, 2011; 130: 1232
[20] Fan J L.  PhD Dissertation, Harbin Institute of Technology, 2012
(樊江磊. 哈尔滨工业大学博士学位论文, 2012)
[21] Fan J L, Li X Z, Su Y Q, Guo J J, Fu H Z.  Mater Des, 2012; 34: 552
[22] Liu C.  PhD Dissertation, Harbin Institute of Technology, 2007
(刘畅. 哈尔滨工业大学博士学位论文, 2007)
[23] Zheng Y B, Li S M, Li Z X, Zhu P C, Fu H Z.  J Aeronaut Mater, 2009; 29: 12
(郑元斌, 李双明, 李臻熙, 朱鹏超, 傅恒志. 航空材料学报, 2009; 29: 12
[24] Muto S, Yamanaka T, Lee H N, Johnson D R, Inui H, Yamaguchi M.  Adv Eng Mater, 2001; 3: 391
[25] Johnson D R, Inui H, Yamaguchi M.  Intermetallics, 1998; 6: 647
[26] Spinelli J E, Rosa D M, Ferreira I L, Garcia A.  Mater Sci Eng, 2004; A383: 271
[27] Appel F, Paul J D H, Oehring M.  Gamma Titanium Aluminide Alloys: Science and Technology. Weinheim: Wiley, 2011: 33
[28] Trivedi R, Kurz W.  Solidification Processing of Eutectic Alloys.Pennsylvania: Metallurgical Society, 1988: 3
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[15] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
No Suggested Reading articles found!