| RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY |
| NING Yongquan, YAO Zekun |
| School of Material Science and Engineering, Northwestern Polytechnical University, Xi’an 710072 |
|
Cite this article:
NING Yongquan YAO Zekun. RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY. Acta Metall Sin, 2012, 48(8): 1005-1010.
|
|
|
Abstract FGH4096 is regarded as a promising powder metallurgy superalloy for high–temperature/pressure turbine disc in aerospace industries due to its high resistance/defect tolerance and high working temperature up to 750 ℃. In the present work, OM and TEM have been employed to study the recrystallization nucleation and microstructure evolution in FGH4096 powder metallurgy superalloy. It is proved that there exist three types of recrystallization mechanisms: nucleation from previous particle boundary (PPB), strain–induced nucleation from butterfly γ' phase (SIP) and twins superposition (TS) nucleation. The physical explanation for this is given from the view of point of micro–segregation, formation of the bend fold boundary and twins superposition, atomic diffusion and dislocation movement.
|
|
Received: 05 March 2012
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.51101119) and China Postdoctoral Science Foundation (No.20110491686) |
| [1] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2nd Ed., Oxford: Elseriver, 2004: 10[2] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2011; A528: 8065[3] Ning Y Q, Fu M W, Yao W. Mater Sci Eng, 2012; A539: 101[4] Ning Y Q, Yao Z K, Xie X H, Guo H Z, Tan L J, Tao Y. Acta Metall Sin, 2010; 45: 58(宁永权, 姚泽坤, 谢兴华, 郭鸿镇, 谭立军, 陶宇. 金属学报, 2010; 45: 58)[5] Ning Y Q, Yao Z K, Yue TW, Guo H Z, Tao Y, Zhang Y W. Rare Met Mater Eng, 2010; 39: 1235(宁永权, 姚泽坤, 岳太文, 郭鸿镇, 陶 宇, 张义文. 稀有金属材料与工程, 2010; 39: 1235)[6] Reed R C. The Superalloys Fundamentals and Applications. New York: Cambridge University Press, 2006: 6[7] Ning Y Q, Yao Z K, Guo H Z, Tao Y, Zhang Y W. Key Eng Mater, 2009; 407–408: 694[8] Zhao M L, Sun WR, Yang S L, Qi F, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 79(赵美兰, 孙文儒, 杨树林, 祈峰, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 79)[9] Viswanathan G B, Sarosi P M, Henry M F, Whitis D D, Milligan W W, Mills M J. Acta Mater, 2005; 53: 3041[10] Tiley G, Viswanathan G B, Srinivasan R, Banerjee R, Dimiduk D M, Fraser H L. Acta Mater, 2009; 57: 2538[11] MacSleyne J, Uchic M D, Simmons J P, Graef M D. Acta Mater, 2009; 57: 6251[12] Dunlavy M A, Shivpuri R, Semiatin S L. Mater Sci Eng, 2003; A359: 210[13] Viswanathan G B, Sarosi P M, Whitis D H, Mills M J. Mater Sci Eng, 2005; A400–401: 489[14] Cao F L, Qing H, Gu Y X, Guan C B, Zhou Q. Gas Turbine Exp Res, 2007; 20(3): 15(曹凤兰, 卿华, 古远兴, 关长波, 周全. 燃气涡轮试验与研究, 2007; 20(3): 15)[15] Liu F J, Zhang M C, Dong X, Zhang Y W. Acta Metall Sin (Engl Lett), 2007; 20: 102[16] Zhou X M, Wang W X, Tang D Z, Yan M G. Mater Eng, 2006; (11): 53(周晓明, 汪武祥, 唐定中, 颜鸣皋. 材料工程, 2006; (11): 53)[17] Liu J T, Liu G Q, Hu B F, Song Y P, Qin Z R, Zhang Y W. J Univ Sci Technol Beijing, 2006; 13: 319[18] Tian G F, Jia C C, Wen Y, Hu B F. J Univ Sci Technol Beijing, 2008; 15: 729[19] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Mater Sci Eng, 2010; A527: 961[20] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Chin J Mech Eng, 2009; 22: 925[21] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2010; A527: 6968[22] Xie X H, Yao Z K, Ning Y Q, Guo H Z, Tao Y, Zhang Y W. J Aero Mater, 2011; 31: 22(谢兴华, 姚泽坤, 宁永权, 郭鸿镇, 陶 宇, 张义文. 航空材料学报, 2011; 31: 22)[23] Ozols A, Sirkin H R, Vicente E E. Mater Sci Eng, 1999; A262: 64[24] Sun X Y, Song H M, Lin Q. J Chin Soc Rare Earths, 2004; 22: 177(孙学义, 宋红梅, 林勤. 中国稀土学报, 2004; 22: 177)[25] Yang P, Fu Y Y, Cui Y E. Acta Metall Sin, 2001; 37: 601(杨平, 傅云义, 崔月娥. 金属学报, 2001; 37: 601)[26] Yi M, Xiong H B, Lin Z. Shougang Sci Technol, 2008; (1): 1(易敏, 熊化冰, 林志. 首钢科技, 2008; (1): 1) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|