| SENSITIVITY ANALYSIS OF THE EFFECT OF INTERFACIAL HEAT TRANSFER COEFFICIENT ON DISTORTION SIMULATION DURING QUENCHING |
| CHENG Baisong, XIAO Namin, LI Dianzhong, LI Yiyi |
| Shenyang National Laboratory for Materials Sciences, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
CHENG Baisong, XIAO Namin, LI Dianzhong, LI Yiyi. SENSITIVITY ANALYSIS OF THE EFFECT OF INTERFACIAL HEAT TRANSFER COEFFICIENT ON DISTORTION SIMULATION DURING QUENCHING. Acta Metall Sin, 2012, 48(6): 696-702.
|
|
|
Abstract The distortions of C-ring and cut cylinder of austenitic stainless steel after water quenching were investigated using simulation and experiment methods. The results indicated that the accurate measurement of temperature had a major influence on interfacial heat transfer coefficient (IHTC) which is calculated using the inverse analysis method. The sparse data of the high temperature stage due to low sampling frequency resulted in the lower value of IHTC. The simulated distortion during water quenching was mostly decided by the change of IHTC. The simulation results showed that the trend and magnitude of distortion predicted by the IHTCH (calculated from the data of high sampling frequency) agreed better with the experiments than that by the IHTCL (calculated from the data of low sampling frequency). The further analysis showed that the IHTC at high temperature had the great influence on the calculated yield behavior of materials. The high values of IHTC caused that the work piece kept in the yield status at higher temperature and wider temperature range. So the simulation using the IHTCH predicted more serious plastic deformation and larger rigid movement. Further analysis showed that the simulation result of distortions was sensitive to the variation of IHTC at the high temperature stage, while insensitive to the variation at the low temperature stage.
|
|
Received: 26 March 2012
|
| [1] Liu Y Y, Wang H, Ji C T, Wang B S. Met Heat Treat, 2005; 30: 46 (刘云旭, 王淮, 季长涛, 王柏树. 金属热处理, 2005; 30: 46)[2] Pan J S, Wang J, Han L Z, Gu J F. Met Heat Treat, 2008; 33: 1 (潘健生, 王婧, 韩利战, 顾剑锋. 金属热处理, 2008; 33: 1)[3] Zhang W M, Pan J S, Qian C J, Li Y J, Zhang G. Trans Mater Heat Treat, 2001; 22: 60 (张伟民, 潘健生, 钱初均, 李勇军, 张戈. 材料热处理学报, 2001; 22: 60)[4] Ye J S, Li Y J, Pan J S, Hu M J. Mater Mech Eng, 2002; 26: 12 (叶健松, 李勇军, 潘健生, 胡明娟. 机械工程材料, 2002; 26: 12)[5] Hernandez--Morales B, Barba--Mendez O, Ingalss--Cruz A, Barrera--Godinez J A. Int J Mater Prod Technol, 2005; 24: 306[6] Ferguson B L, Petrus G J, Pattok T. Proc 3rd Int Conf on Quenching and Control of Distortion, Materials Park, OH: ASM International, 1999: 291[7] Arimoto K, Lambert D, Li G, Arvind A, Wu W T. In: Wallis R A, Walton H eds., Proc 18th Conf on Heat Treating, Materials Park, OH: ASM International, 1998: 639[8] Brooks B E, Beckermann C. Proc 61st Technical and Operating Conference, Chicago: Steel Founder's Society of America, 2007: 1[9] Inoue T, Wang Z G. Mater Sci Technol, 1985; 1: 845[10] Inoue T, Yamaguchi T, Wang Z G. Mater Sci Technol, 1985; 1: 872[11] Ju D Y, Zhang W M, Zhang Y. Mater Sci Eng, 2006; A438--440: 246[12] Lee S J, Lee Y K. Acta Mater, 2008; 56: 1482[13] Pan J S, Zhang W M, Tian D, Gu J F, Hu M J. Eng Sci, 2003; 5: 47 (潘健生, 张伟民, 田东, 顾剑锋, 胡明娟. 中国工程科学, 2003; 5: 47)[14] Michel F, Louchez P R, Samuel F H. Trans Am Foundry-men's Soc, 1995; 103: 278[15] Guthrie R I L, Isac M, Kim J S, Tavares R P. Metall Mater Trans, 2000; 31B: 1031[16] Hallam C P, Griffiths W D, Butler N D. Mater Sci Forum, 2000; 329--330: 467[17] Santos C A, Quaresma J W V, Garcia A. J Alloys Compd, 2001; 319: 174[18] Nelson C W. In: the Society of Die Casting Engineers ed., 6th SDCE International Die Casting Congress, Cleveland, OH: SDCE, 1970: 1[19] Hong S, Backman D G, Mehrabian R. Metall Mater Trans, 1979; 10B: 299[20] Dour G, Dargusch M, Davidson C, Nef A. J Mater Process Technol, 2005; 169: 223[21] Hamasaiid A, Dour G, Dargusch M, Loulou T, Davidson C, Savage G.In: Gandin C A, Bellet M eds., Modeling of Casting,Welding and Advanced Sollidification Processes. Vol.XI, Warrendale, PA: Minerals,Metals and Materials Society, 2006: 1205[22] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2008; 44: 433 (郭志鹏, 熊守美, 曺尚铉, 崔正吉. 金属学报, 2008; 44: 433)[23] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1155 (郭志鹏, 熊守美, 曺尚铉, 崔正吉. 金属学报, 2007; 43: 1155)[24] Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1149 (郭志鹏, 熊守美, 曺尚铉, 崔正吉. 金属学报, 2007; 43: 1149)[25] Hou Z L, Yao S, Wang T L, Zhang X G, Jin J Z. Trans Mater Heat Treat, 2008; 29: 157 (候忠霖, 姚山, 王廷利, 张兴国, 金俊泽. 材料热处理学报, 2008; 29: 157) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|