| MOLECULAR DYNAMICS SIMULATION OF THE ATOM CLUSTER EVOLUTION IN COPPER MELT DURING SOLIDIFICATION PROCESS |
| JIAN Zengyun1, LI Na1, CHANG Fang'e1, FANG Wen1, ZHAO Zhiwei1, DONG Guangzhi1,JIE Wanqi2 |
1. School of Materials Science and Chemical Engineering, Xi'an Technological University, Xi'an 710032
2. State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
|
Cite this article:
JIAN Zengyun, LI Na, CHANG Fang'e, FANG Wen, ZHAO Zhiwei, DONG Guangzhi,JIE Wanqi. MOLECULAR DYNAMICS SIMULATION OF THE ATOM CLUSTER EVOLUTION IN COPPER MELT DURING SOLIDIFICATION PROCESS. Acta Metall Sin, 2012, 48(6): 703-708.
|
|
|
Abstract The structure evolution of atom cluster in copper melt and the microstructure of solidificated copper during the solidification process were investigated by using the molecular dynamics simulation method. It was found that the solidificated structure is composed of crystal phase and amorphous phase when the cooling rate is ranged from 1012.6 to 1014.5 K/s. All the structures of the growing crystal, the critical nuclei and the atom cluster in copper melt are the layer mosaic structure constructed by fcc and hcp structure, which indicates that the layer mosaic structure of copper originates from the nucleation. When the cooling rate is lower than 1013.3 K/s, the atom number of hcp structure in the layer mosaic structure in the amorphous matrix is less than that of fcc structure, but when the cooling rate is higher than 1013.3 K/s, the atom number of fcc structure in the layer mosaic structure is less than that of hcp structure. When the size of the atom cluster with the crystalline structure in copper melt is smaller than the critical size of the homogenous nucleation nuclei, radial distribution function cannot reflect out the feature of crystalline structure though the HA bond--type index have confirmed the presence of a certain number of atom bond of crystalline structure.
|
|
Received: 30 September 2011
|
| Fund: National Natural Science Foundation of China |
| [1] Gibson J M. Science, 2009; 326: 942[2] Bernal J. Nature, 1959; 183: 141[3] Qi D W, Wang S. Phys Rev, 1991; 44B: 884[4] Liu R S, Dong K J, Tian Z A, Liu H R, Peng P, Yu A B. J Phys: Comdens Matter, 2008; 19: 196103[5] Wang R S, Hou H Y, Chen G L. Acta Metall Sin, 2009; 45: 692 (王荣山, 候怀宇, 陈国良. 金属学报, 2009; 45: 692)[6] Mondal K, Murty B S. J Non--Crystalline Solids,2006; 352: 5257[7] Li Y D, Hao Q H, Cao Q L, Liu C S. Phy Rev, 2008; 78B: 174202[8] Cheng Z N, Luo X C, Ma J P, Shao J, Chen N Y. Sci China, 1991; 4A: 440 (程兆年, 罗学才, 马剑鹏, 邵俊, 陈念贻.中国科学, 1991; 4A: 440)[9] Hui X D, Liu X J, Gao R, Hou H Y, Fang H Z, Liu X K, Chen G L. Sci China, 2008; 38G: 406 (惠希东, 刘雄军, 高蕊, 侯怀宇, 方华志, 刘梓葵, 陈国良.中国科学, 2008; 38G: 406)[10] Liu H R, Liu R S, Zhang A L, Hou Z Y, Wang X, Tian Z A. Chin Phys, 2007; 16, 3747[11] Li J Y, Liu R S, Zhou Z, Xie Q, Peng P. J Mater Sci Technol, 1998; 14: 461[12] Ten Wolde P R, Ruiz-Montero M J, Frenkel D. J Chem Phys, 1996; 104: 9932[13] Malley B O, Snook I. Phys Rev Lett, 2003; 90: 085702[14] Jian Z Y, Chen J, Chang F E, Zeng Z, He T, Jie W Q. Sci China, 2010; 53E: 3203[15] Liu C S, Xia J C, Zhu Z G, Sun D Y. J Chem Phys,2001; 114: 7506[16] Mishin Y, Mehl M J, Papaconstantopoulos D A, Voter A F, Kress J D. Phys Rev, 2001; 63B: 224106[17] Morris J R, Wang C Z, Ho K M, Chan C T. Phys Rev,1994; 49B: 3109[18] Honeycutt J D, Andersen H C. J Phys Chem, 1987; 91: 4950[19] Zhao Y, Hu Z Q, Zhao J Z. Acta Metall Sin,2008; 44: 1157 (赵毅, 胡壮麒, 赵九洲. 金属学报, 2008; 44: 1157)[20] Turkdogen E T. Physical of High Temperature Techonlogy.New York: Academic Press, 1980: 1[21] Jian Z Y, Li N, Zhu M, Chen J, Chang F E, Jie W Q. Acta Mater, 2012; 60: 3590[22] David R. CRC Handbook of Chemistry and Physics.Tokyo: CRC Press, 1989: 1[23] Jian Z Y, Chang F E, Ma W H, Yan W. Sci China, 2000; 30E: 10[24] Brandes E A, Brook G B. Smithells Metals Refrence Book.7th ed., Oxford: Butterworth, 1992: 1[25] Guthrie R I L, Iida T. Mater Sci Eng, 1994; A178: 35[26] Barin I, Knacke O. Thermochemical Properties of Inorganic Substances. Berlin: Springer-Verlag, 1973: 1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|