					Cite this article:
						|  |  
    					|  |  
    					| INFLUENCE OF TEMPERATURE ON PITTING CORROSION RESISTANCE OF Cr26Mo1 ULTRA PURE HIGH CHROMIUM FERRITE STAINLESS STEEL IN 3.5%NaCl SOLUTION |  
						| WEI Xin1,2, DONG Junhua1, TONG Jian1, ZHENG Zhi1,KE Wei1 |  
						| 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2. College of Materials Science and Engineering, Dalian University ofTechnology, Dalian 116024
 |  
						|  |  
					
			      WEI Xin, DONG Junhua, TONG Jian, ZHENG Zhi,KE Wei. INFLUENCE OF TEMPERATURE ON PITTING CORROSION RESISTANCE OF Cr26Mo1 ULTRA PURE HIGH CHROMIUM FERRITE STAINLESS STEEL IN 3.5%NaCl SOLUTION. Acta Metall Sin, 2012, 48(4): 502-507.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  The remarkable uniform corrosion resistance of ultra pure high chromium ferrite stainless steel in various rigorous corrosive environments is based on the formation of a passive film on its surface. However, it is suspected that this stainless steel was easy to suffer from pitting corrosion. In this work, the influences of temperature on the pitting corrosion resistance of Cr26Mo1 ultra pure high chromium ferrite stainless steel were studied by electrochemical methods such as cyclic polarization curves, Mott-Schottky curves and electrochemical impedance spectroscopy in 3.5%NaCl solution. The results showed that with the increase of the temperature, open-circuit corrosion potential and pitting corrosion potential decreased, corrosion current density increased, the impedance of passive film decreased. The semi-conductive styles and properties of passive film changed at different temperatures. Also, the pregnancy time of pitting shortened and the sensitivity of pitting increased remarkably as the temperature increased. In addition, the cyclic polarization curves indicated that the repassivation of existing pits was more difficult when the potential was swept toward the negative direction. |  
															| Received:  27 July 2011 |  
            
									            
									               
																												  
															| [1] Ilevbare G O, Burstein G T.  Corros Sci, 2003; 45: 1545[2] Sekine I, Okano C, Yuasa M.  Corros Sci, 1990; 30: 351[3] Hiraide N.  World Iron Steel, 2004; 6: 33[4] You X M, Jiang Z H, Li H B, Shen M H, Cao Y.  China Metall,2006; 16(11): 16    (游香米, 姜周华, 李花兵, 申明辉, 曹阳. 中国冶金, 2006; 16(11): 16 )[5] Latanision R M, Kloppers M J, Bellucci F.  Corrosion, 1992; 48: 229[6] Kaneko M, Isaaca H S.  Corros Sci, 2002; 44: 1825[7] Shan Y T, Luo X H, Hu X Q, Liu S.  J Mater Sci Technol, 2011; 27: 352[8] Ernst P, Newman R C.  Corros Sci, 2007; 49: 3705[9] Rosenfeld I L, Danilov I S, Oranskaya R N.  J Electrochem Soc,1978; 125: 1728[10] Stockert L, Hunkeler F, Bohni H.  Corrosion, 1985; 41: 676[11] Carmezim M J, Simoes A M, Montemor M F, Da C B M.  Corros Sci,2005; 47: 581[12] Ferreira M G S, Hakiki N E, Goodlet G, Faty S, Simoes A M P, Da C B M. Electrochim Acta, 2001; 46: 3767[13] McCafferty E.  Corros Sci, 2003; 45: 301[14] Jin B, Zheng M S, Zhu J W.  Corros Sci Prot Technol, 2006; 18: 348     (金波, 郑茂盛, 朱杰武. 腐蚀科学与防护技术, 2006; 18: 348)[15] Lin Y H, Du R G, Hu R G, Lin C J.  Acta Phys Chim Sin, 2005; 21: 740     (林玉华, 杜荣归, 胡融刚, 林昌健. 物理化学学报, 2005; 21: 740)[16] Li W S, Luo J L.  Electrochem Commun, 1999; 1: 349[17] Paola A P, Shukla D, Stimming U.  Electrochim Acta, 1991; 36: 345[18] Sunseri C, Piazza S, Di Quarto F.  J Electrochem Soc,1990; 137: 2411[19] Montemor M F, Ferreira M G S, Hakiki N E, Da C B M.  Corros Sci,2000; 42: 1635[20] Macdonald D D, Urquidi-Macdonald M.  J Electrochem Soc,1990; 137: 2395[21] Eghbali F, Moayed M H, Davoodi A, Ebrahimi N.  Corros Sci,2011; 53: 513[22] Moayed M H, Newman R C.  Corros Sci, 2006; 48: 1004[23] Cao C N.  Principles of Electrochemistry of Corrosion.Beijing: Chemical Industry Press, 2008: 248     (曹楚南, 腐蚀电化学原理, 北京: 化学工业出版社, 2008: 248)[24] Eghbali F, Moayed M H, Davoodi A, Ebrahimi N.  Corros Sci,2011; 53: 513[25] Ningshen S, Mudali U K, Mittal V K, Khatak H S.  Corros Sci,2007; 49: 481 |  
             
								                
															
																| 
																																																																									