EFFECT OF MARTENSITE ORDERING ON SME IN A Cu-Zn-Al ALLOY
QI Xuan;JIANG Bohong;XU Zuyao(T.Y. Hsu) Shanghai Jiaotong UniversityDept.Mater. Sci. and Eng.;Shanghai Jiaotong University;Shanghai
Cite this article: 

QI Xuan;JIANG Bohong;XU Zuyao(T.Y. Hsu) Shanghai Jiaotong UniversityDept.Mater. Sci. and Eng.;Shanghai Jiaotong University;Shanghai. EFFECT OF MARTENSITE ORDERING ON SME IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1988, 24(4): 228-235.

Download:  PDF(1366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The correlation between the shape memory effect (SME) and theordering degree of martensite formed during various heat treatment processes, e. g.ice water quenching, step-quenching and quenching plus aging, has been studied ina Cu-Zn-Al alloy. The ordering degree of martensite is characterized by the spacingdifference, Δd, of some pairs of diffracting planes, the indices of which satisfy theequation (h_1~2-h_2~2)/3=(k_2~2-k_1~2)/n. It is shown that the SME depends on Δd monoto-nically. The ordering extent of the DO_3 parent phase and of the martensite in turnincreases with the holding duration in the course of step-quenching, which may bethe main factor for enhancing the shape recovery rate η. The stabilization of themartensite may be associated with the clustering of vacancies which results in thelowering of the ordering degree. The decrease of the SME upon aging at highertemperature or holding at step-quenching temperature for longer time is due to theaccumulation of solute atoms and the precipitation of α-phase, which lowers theordering extent.
Key words:  Cu-Zn-Al alloy      martensite      ordering      shape memory effect     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/228

1 Otsuka K, Shimisu K. Scr Metall, 1970; 4: 469
2 江伯鸿,陈树川,漆璿,刘和,王承宝,徐祖耀.全国形状记忆合金学术交流会文集,第3册,中国有色金属学会,1985
3 Stice J D, Wayman C M. Metall Trans, 1982, 13A: 1687
4 Schofield D, Miodownik A P. Met Technol, 1980; 4: 167
5 鲁小叶,曹明盛.全国形状记忆合金学术交流会文集,第3册,中国有色金属学会,1985
6 冯继文,桂嘉年,王子孝.全国形状记忆合金学术交流会文集,第3册,中国有色金属学会,1985
7 Delaey L, Deruyttere A, Aernoudt E, Roos J K. Report 78 R1, Department Metallkunde Katholieke Universiteit, 1978: 38
8 Dunne D P, Kennon N F. Scr Metall, 1982; 16: 729
9 Scarsbrook G, Cook J M, Stobbs W M. Metall Trans, 1984; 15A: 1977
10 Abu-Arab A, Chandrasekaran M. Ahlers M. Scr Metall. 1984; 18: 709
11 王仁卉,赵兴中,黄颐,桂嘉年.全国形状记忆合金学术交流会文集,第3册.中国有色金属学会,1985
12 Delaey L. Z Metallk, 1967; 58: 388
13 Cook J M, Brown L M. Scr Metall, 1978; 12: 949
14 Janssen J, Van Humbeeck J, Chandrasekaran M, Mwamba n, Delaey L. J Phys, Colloc C4, Suppl, 1982; 43: C4-715
15 赵兴中.Cu-Zn-Al形状记忆合金马氏体结构和相交的研究,武汉大学硕士学位论文,1984j
[1] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[2] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[3] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[4] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[5] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[6] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[7] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[8] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[9] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[10] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[11] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[12] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[13] LUO Haiwen,SHEN Guohui. Progress and Perspective of Ultra-High Strength Steels Having High Toughness[J]. 金属学报, 2020, 56(4): 494-512.
[14] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[15] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
No Suggested Reading articles found!