Abstract The thermal fatigue behaviour and microstructure in a direction-ally solidified DZ38G alloy have been investigated. It was found that DZ38G alloyhas larger thermal fatigue resistance than that of original M38G alloy because of theelimination of the transverse grain boundaries and the increasing of elastic modulus.Detailed observations show that the microcrack is initiated at the grain boundariesor the phase interface and propagates along interdendrites, grain boundaries and,sometimes, the defined crystallographic directions. After thermal fatigue test, theamount of carbides at grain boundaries increases and the morphology of γ′ phasebecome irregular. Both γ′denudation and recrystallization have been observed onboth sides of the crack.
|
|
Received: 18 April 1988
|
1 朱景鹏,姚德良,李其娟.航空材料,1980;(4) :21 2 杨富.航空材料,1984;(1) ;37 3 Organ F E, Gell M. Metall Trans, 1971; 2: 943 4 Mowbray D F, Mcconnelee J E. In: Spera D A, Mowbray D F eds., Thermal Fatigue of Materials and Components, ASTM STP 612, Philadephia: ASTM. 1975: 18 5 Woodford D A, Mowbray D F. Mater Sci Eng, 1974; 16: 5 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|