| CHARACTERISTICS OF MARTENSITE IN A HIGH-CARBON FERROALLOY |
| LIU Yumen;WU Shanghua Xi'an Jiaotong University |
|
Cite this article:
LIU Yumen;WU Shanghua Xi'an Jiaotong University. CHARACTERISTICS OF MARTENSITE IN A HIGH-CARBON FERROALLOY. Acta Metall Sin, 1988, 24(5): 325-330.
|
|
|
Abstract Some characteristics of plate martensite in a 1.03%C ferroalloy hasbeen studied by using the transmission electron microscopy. The habit plane of theplate martensite in this ferroalloy was found to be close to {224}_f. The morpholo-gy, distribution, coalescence and curving of martensite as well as the substructurein both martensite and austenite have been observed. The mechanism of both nucle-ation and growth of the martensite have been discussed.
|
|
Received: 18 May 1988
|
1 Kajiwara S. Philips Mag, A, 1981; 43: 1483 2 Shimizu K. Oka M, Wayman C M. Acta Metall, 1970; 18: 1005 3 Wechsler M S, Licberman D S, Read T A. Trans AIME, 1953; 197: 1503 4 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224 5 Shimizu K, Oka M, Wayman C M. Acta Metall, 1971; 19: 1 6 Umemoto M, Tamura I. J Phys (Paris), Colloq. C-4, 1982; 43 Suppl. No. 12: 551 7 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2469 8 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905, 1915 9 刘禹门,李汾兰.金属热处理学报,1988 10 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2455 11 Umemoto M, Hyodo T, Maeda T. Acta Metall, 1984; 32: 1191 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|