CHARACTERISTICS OF MARTENSITE IN A HIGH-CARBON FERROALLOY
LIU Yumen;WU Shanghua Xi'an Jiaotong University
Cite this article: 

LIU Yumen;WU Shanghua Xi'an Jiaotong University. CHARACTERISTICS OF MARTENSITE IN A HIGH-CARBON FERROALLOY. Acta Metall Sin, 1988, 24(5): 325-330.

Download:  PDF(1854KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Some characteristics of plate martensite in a 1.03%C ferroalloy hasbeen studied by using the transmission electron microscopy. The habit plane of theplate martensite in this ferroalloy was found to be close to {224}_f. The morpholo-gy, distribution, coalescence and curving of martensite as well as the substructurein both martensite and austenite have been observed. The mechanism of both nucle-ation and growth of the martensite have been discussed.
Key words:  high-carbon ferroalloy      martensite      substructure      habit plane      nucleation     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/325

1 Kajiwara S. Philips Mag, A, 1981; 43: 1483
2 Shimizu K. Oka M, Wayman C M. Acta Metall, 1970; 18: 1005
3 Wechsler M S, Licberman D S, Read T A. Trans AIME, 1953; 197: 1503
4 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224
5 Shimizu K, Oka M, Wayman C M. Acta Metall, 1971; 19: 1
6 Umemoto M, Tamura I. J Phys (Paris), Colloq. C-4, 1982; 43 Suppl. No. 12: 551
7 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2469
8 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905, 1915
9 刘禹门,李汾兰.金属热处理学报,1988
10 Sandvik B P J, Wayman C M. Metall Trans, 1983; 14A: 2455
11 Umemoto M, Hyodo T, Maeda T. Acta Metall, 1984; 32: 1191
[1] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[4] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[5] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[6] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[7] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[8] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[9] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[10] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[11] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[12] LUO Haiwen,SHEN Guohui. Progress and Perspective of Ultra-High Strength Steels Having High Toughness[J]. 金属学报, 2020, 56(4): 494-512.
[13] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[14] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
[15] Juan DU, Xiaoxing CHENG, Tiannan YANG, Longqing CHEN, Frédéric Mompiou, Wenzheng ZHANG. In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates[J]. 金属学报, 2019, 55(4): 511-520.
No Suggested Reading articles found!