| SHAPE MEMORY EFFECT OF POLYCRYSTALLINE Fe-Mn-Si ALLOYS |
| ZHAO Qinghua;TAN Shusong Central South University of Technlogy; Changsha |
|
Cite this article:
ZHAO Qinghua;TAN Shusong Central South University of Technlogy; Changsha. SHAPE MEMORY EFFECT OF POLYCRYSTALLINE Fe-Mn-Si ALLOYS. Acta Metall Sin, 1988, 24(6): 453-456.
|
|
|
Abstract The influence of quenching temperature on the shape memory effect (SME) of theFe-Mn-Si polycrystalline alloys and their martensitic transformation temperature have beenstudied. The SME of the hot rolled alloy specimen may be remarkably raised by selected quench-ing temperature, namely, 600--800℃. It is influenced not only by the distribution of ε-phasemorphology but also by its pre-existence.
|
|
Received: 18 June 1988
|
1 Enami K, Nagasawa A. Scr Metall, 1975; 9: 941 2 Sato A, Chishima E, Soma K. Mori T, Acta Metall, 1982; 30: 1177 3 Murakami M, Otsuka H, Sueuki H. G, Matsuda S. In: Proc Int Conf on Martensitic Transformations, The Japan Institute of Metals, 1986: 985 4 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:5 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|