| ON THE MICROSTRUCTURES OF MILD STEELS AND CORROSION FATIGUE |
| XING Zhiqiang;HUANG Shuju;SONG Yujiu; TU Mingjing Xi'an Jiaotong University |
|
Cite this article:
XING Zhiqiang;HUANG Shuju;SONG Yujiu; TU Mingjing Xi'an Jiaotong University. ON THE MICROSTRUCTURES OF MILD STEELS AND CORROSION FATIGUE. Acta Metall Sin, 1988, 24(6): 476-481.
|
|
|
Abstract The fatigue crack propagation behaviour of two mild steels with vari-ous microstructures in 3.5% NaCl solution or atmosphere was studied. It is revealedthat the microstructures of steel and frequency have considerable influence on thecorrosion fatigue strength. The relation between crack closure effect and electroche-mical conditions is discussed. The corrosion fatigue mechanisms, which considerthe effect of hydrogen embrittlement and anode dissolution respectively, are pro-posed. A fracture mechanism-map is worked.
|
|
Received: 18 June 1988
|
1 Tomkins B. Met Sci, 1979; 13: 387 2 Torronen K. ASTM STP 801, 1982: 289 3 Rhodes D, Radon J C. Int J Fract, 1979; 15: R65 4 Endo K, Komai K, Matsuda Y. Bull JSME, 1981; 24: 1319 5 Tu?nbull A, Thomas J G N. J Electrochem Soc, 1982; 129: 1412 6 Brown B F. In: Scully J C ed, The Theory of Stress Corrosion Cracking in Alloys, England: University of Leeds, 1971: 186 7 Parkins R N. Craig I H. In: Swann P R, Ford F P, Westwood A R C eds., Mechanism of Environment Sensitive Cracking of Materials Guildford. University of Surrey, 1977: 32 8 Bristoll P, Rp?leveld J A. European offshore Steels Research Seminar, Session V, Cambridge, UK, 1978: 18 9 Wei R P. In: Gu H, He J eds., Proc Int Symposium on Microstrudture and Mechanical Behaviour of Materials, Xi'an Jiaotong University, China, 1985: 5074 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|