Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 471-475    DOI:
Current Issue | Archive | Adv Search |
GROWTH OF SHORT CRACKS OF A537CL1 STEEL UNDER FATIGUE LOADING IN 3.5% NaCl SOLUTICN
PEI Hongxun;YANG Jingjun;KE Wei Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang
Cite this article: 

PEI Hongxun;YANG Jingjun;KE Wei Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. GROWTH OF SHORT CRACKS OF A537CL1 STEEL UNDER FATIGUE LOADING IN 3.5% NaCl SOLUTICN. Acta Metall Sin, 1988, 24(6): 471-475.

Download:  PDF(422KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of environmental media, both in atmosphere and in 3.5%NaCl aqueous solution, on the growth of short cracks in comparison with thelong ones have been investigated under fatigue loading on the specimens of single-edge crack about 0.05--0.15 mm for A537CL 1 steel. The growth rate of short cracksis faster than those of long ones around the threshold stress intensity. The thresh-old stress intensity for short crack growth decreases with decreasing crack length.The acceleration effect of the salt water, as compared with atmosphere environ-ment, on the growth of short cracks under fatigue is much greater than that on thegrowth of long cracks.
Key words:  Short fatigue crack      offshore platform steel      environment medium      threshold stress intensity     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/471

1 Suresh S, Ritchie R O. Int Met Rev, 1984; 29: 445
2 Yu Weicheng, Yuan Jincai, Ke Wei, Shi Changxu (C H Shih). In: Fong J J, Wei R P eds., Proc of Fundamental Questions and Critical Experiments in Fatigue, Dallas, 1984,
3 Lankford J. Fatigue Eng Mater Struct, 1983; 6: 15
4 Taylor D, Knott J F. Fatigue Eng Mater Struct, 1981; 4: 147
5 ElHaddad M H, Topper T H, Smith K N. Eng Fract Mech, 1979; 11: 573
6 Tanaka K, Nakai Y, Yamashita M. Int J Fract, 1981; 17: 519
7 James M R, Morris W L. Metall Trans, 1983; 14A: 153
8 Minakawa K, Newman J C Jr., McEvily A J. Fatigue Eng Mater Struct, 1983; 6: 359
9 Duggan T V. In: Backlund J, Blom A F, Beevers C J eds., Fatigue Threshold, Vol. Ⅱ, Warley, UK: Engineering Materials Advisory Services Ltd, 1982: 809
10 Zaiken E, Ritchie R O. Scr Metall, 1984; 18: 847
11 McCarver J F, Ritchie R O. Mater Sci Eng, 1982; 55: 63
12 柯伟.金属断裂失效分析,中科院金属研究所,1985:139
13 Gangloff R P. In: Beevers C J ed, Advances In Crack Length Measurement, Warley, UK: Engineering Materials Advisory Services Ltd, 1983: 175
[1] ZHOU Yanlei XU Yang CHEN Jun LIU Zhenyu. EXPERIMENTAL STUDY OF THE IMPACT FRACTURE BEHAVIOR OF FH550 OFFSHORE PLATFORM STEEL[J]. 金属学报, 2011, 47(11): 1382-1387.
[2] CUI Zhenqi;XU Kewei; HU Naisai(National Laboratory for Mechanical Behaviour of Metallic Materials;xi'an Jiaotong University). MODEL AND EXPERIMENTS ON FATIGUE SHORT CRACK GROWTH IN RESIDUAL STRESS FIELD[J]. 金属学报, 1994, 30(2): 65-69.
[3] LI Yongjun Xi'an Jiaotong University. FATIGUE FRACTURE BEHAVIOUR OF LOWCARBON MARTENSITE AND MARTENSITE/ BAINITE DUPLEX STRUCTURE IN 20CrMnMo STEEL[J]. 金属学报, 1991, 27(6): 70-75.
[4] CHEN Zheng Northwestern Polytechnical University; Xi'an. THRESHOLD OF SHORT FATIGUE CRACK FOR 8090 Al-Li ALLOY[J]. 金属学报, 1990, 26(5): 62-65.
[5] WANG Zhengfu;KE Wei;ZHU Zuming Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang Institute of Metal Research; Academia Sinica; Shenyang Institute of Corrosion and Protection of Metals;Academia Sinica; Shenyang 110015. ACOUSTIC EMISSION BEHAVIOUR DURING CORROSION FATIGUE[J]. 金属学报, 1990, 26(1): 102-106.
[6] HONG Youshi;LU Yonghua;ZHENG Zhemin C. M. Cheng Institute of Mechanics; Academia Sinica; Beijing Institute of Mechanics;Academia Sinica;Beijing 100080. SHORT FATIGUE CRACK BEHAVIOUR IN ISO-STRESS SPECIMENS[J]. 金属学报, 1990, 26(1): 46-52.
No Suggested Reading articles found!