| RELATIONSHIP BETWEEN MICROSTRUCTURE AND PROPERTIES IN Al-2.2Li-2.5Cu-0.2Mg ALLOY |
| ZHANG Yun;ZHAO Hong'en;YAO Daping;GAO Guozhong;CHEN Jizhi;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
ZHANG Yun;ZHAO Hong'en;YAO Daping;GAO Guozhong;CHEN Jizhi;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang. RELATIONSHIP BETWEEN MICROSTRUCTURE AND PROPERTIES IN Al-2.2Li-2.5Cu-0.2Mg ALLOY. Acta Metall Sin, 1989, 25(3): 5-11.
|
|
|
Abstract The relationship between the microstructures, properties and the phasetransformation in Al-2.2Li-2.5Cu-0.2Mg alloy after various treatments have beenstudied by optical microscopy and TEM observations. It is verified that solutiontreated at 525℃ for 1h is satisfactory for this alloy in which all the alloying ele-menis are dissolved in the α-Al matrix, and aging at 190℃ for 16h is the peak-aged con-dition, the alloy subjected to treatment is strengthened only by T_1 phase. In over-aged or underaged conditions, the alloy are strengthened by two phases, in thesecases, the strengthening effect is smaller than that by one phase. The deformationprlor to aging would develop the plasticity and do not decrease the strength of theexperimenial alloy.
|
|
Received: 18 March 1989
|
1 宫木美光,日野光雄.金属,1984;54(1) :11 2 Gregson P J, Flower H M. Acta Metall, 1985; 33 (3) : 527 3 Grimes R, Cornish A J, Miller W S, Reynolds M A. Met Mater, 1985: 1: 357 4 Kar R J, Bohlen J W, Chanani G R. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, TMS-AIME, 1984: 255 5 White J, Miller W S, Palmer I G, Davis R, Saini T S. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 530 6 Starke E A Jr, Sanders T H Jr., Palmer I G. J Met, 1981; 33 (8) : 24 7 Feng W X, Lin F S, Starke E A Jr. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, TMS-AIME, 1984: 235 8 Bischler P J E, Martin J W. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 539 9 Ahmad M, Ericsson T. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 509 10 Miller W S, White J, Lloyd D J. J Phys (Paris), 1987; 48 (9) : C3--139 11 Damerval C, Raviart J L, Lapasset G. J Phys (Paris), 1987; 48 (9) : C3--661 12 Thomas G, Bell W L, Otte H M. Phys Status Solidi, 1965; 12: 353 13 Tosten M H, Vasudevan A K, Howell P R. Metall Trans, 1988; 19A: 51 14 Rioja R J, Ludwiczak E A. In; Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 471 15 Silcock J M. J Inst Met, 1959--60; 88: 357 16 Mondolfo L F. Aluminum Alloys: Structure and Properties, London: Butterworth, 1976 17 Vasudevan A K, Fricke W G Jr., Malcolm R C, Bucci R J, Przystupa M A, Barlat F. Metall Trans, 1988; 19A: 731 18 Palmer I G, Lewis R E, Crooks D D, Starke E A Jr., Crooks R E. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ. TMS-AIME, 1984: 9 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|