| PREPARATION AND PHYSICAL PROPERTIES OF AMORPHOUS Ti-Pd ALLOYS |
| ZHANG Shengliang;SUMIYAMA Kenji;NAKAMURA Yoji Department of Physics;Nanjing University; Nanjing 210008 Kyoto University; Japan |
|
Cite this article:
ZHANG Shengliang;SUMIYAMA Kenji;NAKAMURA Yoji Department of Physics;Nanjing University; Nanjing 210008 Kyoto University; Japan. PREPARATION AND PHYSICAL PROPERTIES OF AMORPHOUS Ti-Pd ALLOYS. Acta Metall Sin, 1990, 26(3): 142-145.
|
|
|
Abstract The amorphous alloys with wider stoichiometrical composition, Ti_(1-x)Pd_x (0.25
|
|
Received: 18 March 1990
|
1 Chien C L, Uniuh K M. Phys Rev, 1983; B28: 1214 2 Mader S. J Vac Sci Technol, 1965; 2: 35 3 Massalski T B. Binary Alloy Phase Diagrams, Ohio: ASM, 1986: 1879 4 Liu Z, Jin D, Jin Z, Ma M, Zhao Z, Luo Q. Chin Phys, 1982: 2: 486 5 Zhang S L, Sumiyama K, Nakamura Y. Trans Jpn Inst Met, Suppl., 1988; 29: 359 6 Turnbull D. Metall Trans. 1981; 12A: 695 7 Buschow K H J, Beekmans N M. Phys Rev, 1979; B19: 3843 8 Miedema A R. Z Metallk, 1979; 70: 345 9 Faber T E. Introduction to the Theory of Liquid Metals, London: Cambridge, 1972: 455 10 Meisel L V, Cote P J. Phys Rev, 1984; B30: 1743 11 Mizutani U. Mater Sci Eng, 1988; 99: 1653 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|