| MICROSTRUCTURE AND FATIGUE PROPERTIES OF RAIL STEELS |
| ZHOU Qingyue;ZHOU Chenguang (China Academy of Railway Sciences; Beijing Engineer;Metal and Chemistry Research Institute;China Academy of Railway Sciences;Beijing 100081 |
|
Cite this article:
ZHOU Qingyue;ZHOU Chenguang (China Academy of Railway Sciences; Beijing Engineer;Metal and Chemistry Research Institute;China Academy of Railway Sciences;Beijing 100081. MICROSTRUCTURE AND FATIGUE PROPERTIES OF RAIL STEELS. Acta Metall Sin, 1990, 26(4): 73-78.
|
|
|
Abstract The subcritical propagation of fatigue crack and the microstructure ofthe rail steels with relation to stress ratio have been studied. The effect of micros-tructure of the rail steels on their fatigue lives has been discussed preliminarily.
|
|
Received: 18 April 1990
|
1 周清跃.铁道部科学研究院硕士论文,1986 2 Gan D, Weertman J. Eng Fract Mech, 1981; 15; 87 3 Gray G T III, Thompson A W, Williams, J. C. Metall Trans, 1985; 16A: 753 4 Bouse G K, Bernstein I M, Stone D H, ASTM STP 644, 1978: 145--166 5 周晨光,周镇国,邵扬道.铁道学报,1985;7(1) :99S |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|