DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY |
WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an |
|
Cite this article:
WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY. Acta Metall Sin, 1990, 26(5): 119-124.
|
Abstract Large undercooling up to 397 K (0.283T_E) have been obtained for Ni-32.5%Sn eutectic alloy melt by superheating-cooling cycles and denucleating withinorganic glasses. The predominant dissipation of heat for highly undercooled alloymelt is through radiation. An approximate method was consequently derived to cal-culate its mean specific heat from measured cooling curves. With the aid of highspeed cinematography, it was revealed that the surface or interface heterogeneousnucleation takes place in preference to homogeneous nucleation even though theundercooling exceeded 0.2T_E.
|
Received: 18 May 1990
|
1 Sahm P R, Jones H, Adam C M. Science and Technology of the Undercooled Melt, Dordrecht, Netherlands: Martinus Nijhoff Publishers, 1986 2 魏炳波.杨根仓.航空学报,1988;9:B589 3 Flemings M C, Shiohara Y. Mater Sci Eng, 1984; 65: 157 4 Powell G L F. J Aust Inst Met, 1965; 10: 233 5 Perepezko J H. Mater Sci Eng, 1984; 65: 125 6 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976: 186, 940 7 Holloman J H, Turnbull D. Prog Met Phys, 1953; 4: 333 8 Nielsen H J V. Z Metallk, 1979; 70: 606 9 Davies H A. In: Cantor B ed, Rapidly Quenched Metals Ⅲ, Vol. Ⅰ, London: The Metals Society, 1978: 1 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|