Acta Metall Sin  1990, Vol. 26 Issue (5): 125-130    DOI:
Current Issue | Archive | Adv Search |
EXPLOSIVE CONSOLIDATION OF METAL UNDER CYLINDRICAL CONVERGING SHOCK WAVE
GAO Juxian;SHAO Binghuang;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing
Cite this article: 

GAO Juxian;SHAO Binghuang;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EXPLOSIVE CONSOLIDATION OF METAL UNDER CYLINDRICAL CONVERGING SHOCK WAVE. Acta Metall Sin, 1990, 26(5): 125-130.

Download:  PDF(1216KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Two-dimensional explosive consolidation under the cylindrical con-verging shock wave has been studied by use of coated fine iron wire compacts toreplace conventional metallic powder, so the randomness of three-dimensional spa-tial distribution of metallic powder might be avoided. The deformation and surfaceflow pattern of particles as well as the mechanism of consolidation have been cla-rified experimentally. The distribution of high temperature area is in agreementwith the result of numerical simulation by Williamson. A model for the explosiveconsolidation was given.
Key words:  explosive consolidation      shock wave      metallic powder     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/125

1 Perry R W, Kantrowitz A. J Appl Phys, 1951; 22: 878
2 Payne R B. J Fluid Mech, 1957; 2: 185
3 Carroll M M, Holt A C. J Appl Phys, 1972; 43: 1626
4 Williamson R L, Berry R A. In: Gupta Y M ed, Shock Waves in Condensed Matter-1985, New York: Plenum, 1986: 341
5 Flinn J E, Williamson R L, Berry R A, Wright R N, Gupta Y M, Williams M. J Appl Phys, 1988; 64: 1446
6 McQueen R G, Marsh S P, Taylor J W, Fritz J N, Carter W J. In: Kinslow R ed, High Velocity Impact Phenomena, New York: Academic, 1970: 530s
[1] FENG Aixin NIE Guifeng XUE Wei CAO Yupeng XU Xiaoxiang LI Bin SHI Fen . EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET[J]. 金属学报, 2012, 48(2): 205-210.
[2] LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04). CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE[J]. 金属学报, 1996, 32(8): 862-866.
[3] CHEN Liangshan; ZHAO Tiemin ;SI Zhongyao (Institute of Metal Research;Chinese Academy of Sciences; Shenyang)(Manuscript received 18 November;1993; in revised form 21 January;1994). EFFECT OF REFLECTED TENSION SHOCK WAVE ON MICROSTRUCTURE AND FATIGUE PROPERTY OF 16Mn STEEL WELD[J]. 金属学报, 1994, 30(23): 519-523.
[4] ZHAO Tiemin;CHEN Liangshan;SI Zhongyao(Institute of Metal Research;Chinese Academy of Scicnces; Shenyang);TAN Shengyu;CUI Guangyuan (ShenyangInstitute of Artillery). EFFECT OF EXPLOSION SHOCK WAVE INTENSITY ON DISLOCATION STRUCTURE IN FERRITE OF STEEL 16Mn WELD[J]. 金属学报, 1994, 30(15): 130-135.
[5] CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015. REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS[J]. 金属学报, 1993, 29(6): 38-42.
[6] GAO Juxian;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EFFECT OF EXPLOSIVE CONSOLIDATION PARAMETERS ON CONSOLIDATION QUALITY[J]. 金属学报, 1990, 26(6): 159-161.
No Suggested Reading articles found!