DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY
WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an
Cite this article: 

WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY. Acta Metall Sin, 1990, 26(5): 119-124.

Download:  PDF(821KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Large undercooling up to 397 K (0.283T_E) have been obtained for Ni-32.5%Sn eutectic alloy melt by superheating-cooling cycles and denucleating withinorganic glasses. The predominant dissipation of heat for highly undercooled alloymelt is through radiation. An approximate method was consequently derived to cal-culate its mean specific heat from measured cooling curves. With the aid of highspeed cinematography, it was revealed that the surface or interface heterogeneousnucleation takes place in preference to homogeneous nucleation even though theundercooling exceeded 0.2T_E.
Key words:  undercooling      rapid solidification      nucleation      eutectic alloy      specific heat     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/119

1 Sahm P R, Jones H, Adam C M. Science and Technology of the Undercooled Melt, Dordrecht, Netherlands: Martinus Nijhoff Publishers, 1986
2 魏炳波.杨根仓.航空学报,1988;9:B589
3 Flemings M C, Shiohara Y. Mater Sci Eng, 1984; 65: 157
4 Powell G L F. J Aust Inst Met, 1965; 10: 233
5 Perepezko J H. Mater Sci Eng, 1984; 65: 125
6 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976: 186, 940
7 Holloman J H, Turnbull D. Prog Met Phys, 1953; 4: 333
8 Nielsen H J V. Z Metallk, 1979; 70: 606
9 Davies H A. In: Cantor B ed, Rapidly Quenched Metals Ⅲ, Vol. Ⅰ, London: The Metals Society, 1978: 1
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[3] FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. 金属学报, 2022, 58(9): 1129-1140.
[4] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[5] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[6] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[7] XU Junfeng, ZHANG Baodong, Peter K Galenko. Model of Eutectic Transformation Involving Intermetallic Compound[J]. 金属学报, 2021, 57(10): 1320-1332.
[8] Juan DU, Xiaoxing CHENG, Tiannan YANG, Longqing CHEN, Frédéric Mompiou, Wenzheng ZHANG. In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates[J]. 金属学报, 2019, 55(4): 511-520.
[9] Yun LI, Lianjie LIU, Xinming LI, Jinfu LI. Solidification of Undercooled Co75B25 Alloy[J]. 金属学报, 2018, 54(8): 1165-1170.
[10] Kuanhui HU, Xinping MAO, Guifeng ZHOU, Jing LIU, Zhifen WANG. Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel[J]. 金属学报, 2018, 54(8): 1105-1112.
[11] Jianfeng ZHANG, Qing LAN, Qichi LE. Investigation on the Change of Thermoelectric Power of Al-Fe Hypoeutectic Alloy Melt Caused by AC Magnetic Field[J]. 金属学报, 2018, 54(7): 1042-1050.
[12] Shubo LI, Wenbo DU, Xudong WANG, Ke LIU, Zhaohui WANG. Effect of Zr Addition on the Grain Refinement Mechanism of Mg-Gd-Er Alloys[J]. 金属学报, 2018, 54(6): 911-917.
[13] Dandan FAN, Junfeng XU, Yanan ZHONG, Zengyun JIAN. Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt[J]. 金属学报, 2018, 54(6): 844-850.
[14] Zengyun JIAN, Tao XU, Junfeng XU, Man ZHU, Fang'e CHANG. Development of Solid-Liquid Interfacial Energyof Melt-Crystal[J]. 金属学报, 2018, 54(5): 766-772.
[15] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
No Suggested Reading articles found!