EFFECTS OF RARE EARTH ELEMENTS ON MICROSTRUCTURAL TRANSFORMATION OF LOW OR MEDIUM CARBON Si-Mn-V STEELS DURING QUENCHING AND TEMPERING
WANG Xiaotian;YAO Yinliang;SHAO Tanhua Xi'an Jiaotong University
Cite this article: 

WANG Xiaotian;YAO Yinliang;SHAO Tanhua Xi'an Jiaotong University. EFFECTS OF RARE EARTH ELEMENTS ON MICROSTRUCTURAL TRANSFORMATION OF LOW OR MEDIUM CARBON Si-Mn-V STEELS DURING QUENCHING AND TEMPERING. Acta Metall Sin, 1990, 26(6): 40-45.

Download:  PDF(1980KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructural transformation of four different low or mediumcarbon steels: 20SiMn2V, 20SiMn2VRE, 40SiMn2V and 40SiMn2VRE, during quen-ching and tempering have been examined by TEM, X--ray diffraction and dilatometer.It was shown that the rare earth elements added may make not only the fine aus-tenite grains of the low or medium carbon steels, but also the fine packet of lathmartensite and lath size, lower the M_s temperature and raise the relative Percenta-ge of dislocation substructure of martensite in medium carbon steel, but influenceno more the volume fraction and thermal stability of retained austenite within que-nching and tempering structure of low or medium carbon steels. The rare earthelements may remarkably inhibit the decomposition of low carbon martensite duringlow temperature tempering, retard the precipitation of cementite plates in lath gra-ins and delay the spheroidization of carbides. They may also restrain obviously theprecipitation and spheroidization of cementite in medium carbon martensite duringhigh temperature tempering.
Key words:  rare earth element      tempering      transformation      SiMnV steel      microstructure     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/40

1 Zhang Shouhua (章守华), Wu Chengjian(吴承建). 3rd Int Congress on Heat Treatment of Materials, Shanghai, China, 1983: 3--25
2 余宗森.钢中稀土.北京:冶金工业出版社,1982
3 俞德刚,谈育煦.钢的组织强度学.上海科技出版社,1983
4 王新瑞,陈宝琴.兵器材料科学与工程,1985;(10) :13$
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[10] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!