Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (2): 145-147    DOI:
Current Issue | Archive | Adv Search |
MEASURED AND CALCULATED BaB_2O4-BaF_2 BINARY PHASE DIAGRAM
RAO Guanghui Institute of Physics; Academia Sinica; Beijing; QIAO Zhiyu University of Science and Technology Beijing; LIANG Jingkui Institute of Physics; Academia Sinica; Beijing
Cite this article: 

RAO Guanghui Institute of Physics; Academia Sinica; Beijing; QIAO Zhiyu University of Science and Technology Beijing; LIANG Jingkui Institute of Physics; Academia Sinica; Beijing. MEASURED AND CALCULATED BaB_2O4-BaF_2 BINARY PHASE DIAGRAM. Acta Metall Sin, 1991, 27(2): 145-147.

Download:  PDF(263KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To explore a suitable flux for growth of β-BaB_2O_4 single crystal, thephase diagram of BaB_2O_4-BaF_2 binary system has been determined by means of DTAand X-ray diffraction. The coupled thermodynamical parameters of the binary systemhave been also calculated by optimum analysis. The calculated phase diagram is ingood agreement with the experimental one. A congruent compound, BaBO_2F, withM. P. 867℃ and the eutectic reactions L?β-BaB_2O_4+BaBO_2F and L?BaBO_2F+BaF_2with eutectic temperatures of 749.1 and 815.4℃ respectively were found. It may bebelieved that the BaBO_2F is a potentially favourable flux.
Key words:  phase diagram      β-BaB_2O_4 single crystal      flux     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/145

1 Levin E M, McKurde H F. J Res Nat Bur Stard, 1949; 42: 131
2 梁敬魁,张玉苓,黄清镇.化学学报,1982;40:994
3 王国富,黄清镇.物理学报,1985;34:562
4 Rao G H, Liang J K. Qiao Z Y, Huang Q Z. CALPHAD, 1989; 13: 169
5 黄清镇,梁敬魁.物理学报,1981;30:559
6 JANAF Thermodynamical Tables (Supplement Vol. 1974, 1975, 1978) , Tokyo, 1977
7 乔芝郁,王明生,郑朝贵,段淑贞.中国稀土学报,1989;7(4) :16
8 饶光辉.中国科学院物理研究所博士论文,198
[1] QI Xiaoyong, LIU Wenbo, HE Zongbei, WANG Yifan, YUN Di. Phase-Field Simulation of the Densification Process During Sintering of UN Nuclear Fuel[J]. 金属学报, 2023, 59(11): 1513-1522.
[2] WANG Cong, ZHANG Jin. Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview[J]. 金属学报, 2021, 57(9): 1126-1140.
[3] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[4] Ming HE, Xianliang LI, Qingwei WANG, Lianyu WANG, Qiang WANG. Influence of Magnetic Shielding on the Power Loss of Induction Heating Power Supply in the Electro-magnetic Induction Controlled Automated Steel Teeming System[J]. 金属学报, 2019, 55(2): 249-257.
[5] ZHAO Bo, WU Chuansong,JIA Chuanbao, YUAN Xin. NUMERICAL ANALYSIS OF THE WELD BEAD PROFILES IN UNDERWATER WET FLUX-CORED ARC WELDING[J]. 金属学报, 2013, 49(7): 797-803.
[6] CAI Zhaozhen ZHU Miaoyong. SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD I. Mathematical Model[J]. 金属学报, 2011, 47(6): 671-677.
[7] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[8] FENG Mingjie WANG Engang HE Jicheng. NUMERICAL SIMULATION ON UNSTEADY STATE HEAT TRASFER OF WORK ROLLS DURING CONTINUOUS HOT STRIP ROLLING[J]. 金属学报, 2010, 46(8): 1009-1017.
[9] WANG Hui HE Siyuan CHU Xuming HE Deping . INTERFACIAL STRUCTURE AND MECHANICAL PROPERTIES OF ALUMINIUM FOAM JOINTS FLUXLESS--SOLDERED WITH Zn--Al--Cu BASE ALLOY[J]. 金属学报, 2009, 45(6): 723-728.
[10] MENG Xiangning ZHU Miaoyong. ANALYSIS OF LIQUID FLUX CONSUMPTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2009, 45(4): 485-489.
[11] XU Xiujie DENG Anyuan WANG Engang ZHANG Lintao ZHANG Yongjie HE Jicheng. EFFECT MECHANISM OF HIGH FREQUENCY ELECTROMAGNETIC FIELD ON THE SURFACE QUALITY AND EQUIAXED CRYSTAL RATIO OF 15CrMo BILLET[J]. 金属学报, 2009, 45(11): 1330-1335.
[12] ;. The nanocrystalline structures of Fe-Ni-P-B alloy solidified at large undercooling and the liquid Spinonal decomposition of alloy melt[J]. 金属学报, 2006, 42(8): 870-874 .
[13] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[14] LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang. Mold Flux Channel Dynamic Pressure in Electromagnetic Continuous Casting[J]. 金属学报, 2004, 40(5): 546-550 .
[15] SU Xiaodong;YANG Zongquan; WANG Yongzhong;ZHANG Cheng; HUA Ling; TANG Hong;QIAO Guiwen (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: SU Xiaodong; Tel: (024)25843531-55842; E-mail: xdsu@imr.ac.cn. THE ENHANCEMENT OF FLUX PINNING PROPERTIES OF (BiPb)_2Sr_2Ca_2Cu_3O(10+δ) WITH ADDITION OF NANO-SiC[J]. 金属学报, 1998, 34(9): 999-1004.
No Suggested Reading articles found!