DIVERSE TECHNOLOGICAL PARAMETERS FOR CONFORM CONTINUOUS EXTRUSION FROM Al GRANULE FEEDS
SONG Baoyun Dalian Railway Institute; ZHOU Chuanhe Changchun Passenger Train Warks
Cite this article: 

SONG Baoyun Dalian Railway Institute; ZHOU Chuanhe Changchun Passenger Train Warks. DIVERSE TECHNOLOGICAL PARAMETERS FOR CONFORM CONTINUOUS EXTRUSION FROM Al GRANULE FEEDS. Acta Metall Sin, 1991, 27(2): 140-144.

Download:  PDF(1120KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of diverse technological parameters on the performanceand structure of product extruded from the atomized Al granule has been studiedon a 250 CONFORM continuous extrusion machine. The favourable extruding tem-perature is 350--450℃. The extrusion ratio is greater than 20. The finer the Algranule is, the better the mechanical properties of the product are. It may be im-proved over 50% in comparison with that from rod feed.
Key words:  continuous extrusion      Al granule      extrusion parameter     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/140

1 Pardoe J A. The Continuous Extrusion of Wire and Sections from Non-Ferrous Metal Particulates by the CONFORM Process, Meta1s Society Conference on The Efficient Use of Energy and Equipment in the Powder Metallurgy Industry, Scarborough, 26--28, October. 1981
2 Kumar A.J. Jain P C. Mehta M L. J Mech Working Technol, 1985; 11:275--290
3 Колпашников А И,Ефремоф А В著,周光垓,薛永春,朱子琴译.颗粒材料.北京:国防工业出版社,1986
4 宋宝韫,刘建华,樊志新,戴焕海,刘元文.大连铁道学院学报,1990;(1) :1-7
No related articles found!
No Suggested Reading articles found!