HOT DEFORMATION OF CAST Pr-Fe-B MAGNETS
CHEN Zhongmin;SHI Zhengxing;WANG Leyi;FU Hengzhi Northwestern Polytechnical University; Xi'an
Cite this article: 

CHEN Zhongmin;SHI Zhengxing;WANG Leyi;FU Hengzhi Northwestern Polytechnical University; Xi'an. HOT DEFORMATION OF CAST Pr-Fe-B MAGNETS. Acta Metall Sin, 1992, 28(3): 75-80.

Download:  PDF(1170KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Whatever the cast Pr_(19)Fe_(74.5)B_5Cu_(1.5) magnet deforms in various processes, itseasy-axes are aligned parallel to the compressive strain direction. During hot deformation, thecrushing of Pr_2Fe_(14)B matrix grains, the relative slip and rotation between the grains and thesqueezing out of Pr--rich melt of the magnet take place. Then a fine, dense and well--alignedmicrostructure may be formed in the fully deformed magnets with improved properties, B_r=990mT, _iH_c=880 kA / m and (BH)m=191 kJ / m~3. The increase of coercivity is attributed to thefine Pr_2Fe_(14)B grains and the thin Pr--rich phase layer continuously distributed at the grainbounbaries. The increasing remanence is resulted primarily from the development of theeasy--axis alignment as well as from the densification of the Pr_2Fe_(14)B matrix. The easy--axisalignment is developed by the relative slip and rotation of the crushed Pr_2Fe_(14)B grains. A fulland slow hot deformation is necessary for a good easy--axis alignment and high magnetic prop-erties.
Key words:  Pr-Fe-B magnet      hot deformation      microstructure      magnetic property     
Received:  18 March 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I3/75

1 Shimoda T, Akioka K, Kobayashi O, Yamagami T. J Appl Phys, 1988; 64: 5290
2 Mukai T, Sakamoto H. Appl Phys Lett, 1989; 54: 1957
3 陈钟敏,谢发勤,史正兴,王乐仪,傅恒志.中国稀土学报,1990;8:281
4 Chen Z M, Shi Z X, Wang L Y, Fu H Z. J Less--Common Met, to be published
5 Mishra R K. J Appl Phys. 1987; 62: 967
6 Li L, Graham C D Jr. J Appl Phys, 1990; 67: 4756
7 Nozawa Y, Iwasaki K, Tanigawa S, Tokunaga M, Harada H. J Appl Phys, 1988; 64: 5285
8 陈钟敏,谢发勤,史正兴,王乐仪,傅恒志.金属学报,1991;27:B345
9 Livingston J D. IEEE Trans Magn, 1987; MAG-23: 2109
10 Hamano M, Takahashi S. Proc 10th Int Workshop on Rare-Earth Magnets and their Applications, Kyoto, Japan, 16--19 May, 1989, Tokyo: The Society of Non-Traditional Technology, 1989: 595
11 罗阳,张宁.金属学报,1988,24:B227
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[9] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[10] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!