| DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn |
| XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing |
|
Cite this article:
XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing. DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn. Acta Metall Sin, 1993, 29(1): 65-68.
|
|
|
Abstract Studies were made of the dissolution equilibrium of Bi vapour in liquid Fe at1873 K, using vapour-liquid equilibrium method in a sealed Mo reaction chamber, as well asthe influence of a third element Ni or Mn on Bi solubility. The Bi solubility in liquid Fe at1873 K was determined to be 0.16 wt-%, and enhanced by Ni or Mn. The activity interactioncoefficient obtained is: e_(Bi)~(Ni)=-0.20, e_(Bi)~(Mn)=-0. 19.
|
|
Received: 18 January 1993
|
1 Xu Jianlun, Sen Caipin, Yang Senglun, Jiang Guochang, Zhu Yuru, Wang Liguo, Chen Jikai, Chang Li. Bull Bismuth Inst, 1991; 62: 2 2 Jiang Guochang, Huang Keli, Zhuang Yunqian, Yang Senglong, Xu Kuangdi, Bull Bismuth Inst, 1989; 56: 2 3 木村笃良,中村贞行,柴田范嘉.日本金属学会会报,1987;26:425 4 Han Qiyong, Zhang Xiaodong, Chen Dong, Wang Pengfei. Metall Trans, 1988; 19B: 617 5 Zhang Xiaodong, Han Qiyong, Chen Dong. Proe of the 5th China-Japan Symposium on Science and Technology of Iron and Steel, Bejing: International Academic Publishers, 1989: 301 6 Hultgren R. Selected Values of the Thermodynamic Properties of the Elements, Metals Park, Ohio: ASM, 1973: 77 7 Lupis C H P. Chemiclal Thermodynamics of Materials. New York: North-Holland, 1983: 530 8 Fuwa T, Chipman J. Trans AIME, 1959; 215: 708 |