Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (1): 65-68    DOI:
Current Issue | Archive | Adv Search |
DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn
XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing
Cite this article: 

XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing. DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn. Acta Metall Sin, 1993, 29(1): 65-68.

Download:  PDF(280KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the dissolution equilibrium of Bi vapour in liquid Fe at1873 K, using vapour-liquid equilibrium method in a sealed Mo reaction chamber, as well asthe influence of a third element Ni or Mn on Bi solubility. The Bi solubility in liquid Fe at1873 K was determined to be 0.16 wt-%, and enhanced by Ni or Mn. The activity interactioncoefficient obtained is: e_(Bi)~(Ni)=-0.20, e_(Bi)~(Mn)=-0. 19.
Key words:  Bi      liquid Fe      dissolution equilibrium      interaction coefficient     
Received:  18 January 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I1/65

1 Xu Jianlun, Sen Caipin, Yang Senglun, Jiang Guochang, Zhu Yuru, Wang Liguo, Chen Jikai, Chang Li. Bull Bismuth Inst, 1991; 62: 2
2 Jiang Guochang, Huang Keli, Zhuang Yunqian, Yang Senglong, Xu Kuangdi, Bull Bismuth Inst, 1989; 56: 2
3 木村笃良,中村贞行,柴田范嘉.日本金属学会会报,1987;26:425
4 Han Qiyong, Zhang Xiaodong, Chen Dong, Wang Pengfei. Metall Trans, 1988; 19B: 617
5 Zhang Xiaodong, Han Qiyong, Chen Dong. Proe of the 5th China-Japan Symposium on Science and Technology of Iron and Steel, Bejing: International Academic Publishers, 1989: 301
6 Hultgren R. Selected Values of the Thermodynamic Properties of the Elements, Metals Park, Ohio: ASM, 1973: 77
7 Lupis C H P. Chemiclal Thermodynamics of Materials. New York: North-Holland, 1983: 530
8 Fuwa T, Chipman J. Trans AIME, 1959; 215: 708
[1] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[4] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[5] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[6] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[7] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[8] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[9] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[10] ZHANG Bin, TIAN Da, SONG Zhuman, ZHANG Guangping. Research Progress in Dwell Fatigue Service Reliability of Titanium Alloys for Pressure Shell of Deep-Sea Submersible[J]. 金属学报, 2023, 59(6): 713-726.
[11] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[12] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[13] LI Shujun, HOU Wentao, HAO Yulin, YANG Rui. Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique[J]. 金属学报, 2023, 59(4): 478-488.
[14] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[15] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
No Suggested Reading articles found!