| ON THE PUSHING BEHAVIOUR OF PARTICULATES REINFORCED Al-4%Mg COMPOSITES DURING SOLIDIFICATION |
| XIE Guohong; LI Songchun; WANG Wuxian; WU Renjie(Shanghai Jiaotong University; Shanghai 200030) |
|
Cite this article:
XIE Guohong; LI Songchun; WANG Wuxian; WU Renjie(Shanghai Jiaotong University; Shanghai 200030). ON THE PUSHING BEHAVIOUR OF PARTICULATES REINFORCED Al-4%Mg COMPOSITES DURING SOLIDIFICATION. Acta Metall Sin, 1995, 31(18): 275-279.
|
|
|
Abstract The effects of particle type and size of SiC, Al2O3 or SiO2 particle reinforced A1-4%Mg composites on the pushing behaviour during solidification were investigated. The intensity of pushing during solidification was determined by the mass ratio of equiaxed cell to particle. The theoretical predictions were in fair accordance with experimental results.
|
|
|
| 1StefanescuDM,ShangguanD,BrinckenP.MaterSciForum,1991;77:252吴人洁,谢国宏.材料导报,1993;4:693RohatgiPK,SukappaMK.JMaterSci1981;16:5624LloydDJ.CompSciTechnol,1989;35:1595UhlmannDR,ChalmersB,JacksonKA.JApplPhys,1964;35:29866MortensenA,JinI.IntMaterRev,1992;37:1017HilleD.CompSciTechnol,1989;35:1958ShangguanD,AhujaS,StefanescuDM.MetallTrans,1992;23A:6699RohatgiPK,YarandiFM,LiuY,AsthanaR.MaterSciEng1991;A147:L1h |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|