INFLUENCE OF GAS INJECTION ON FLUID FLOW IN MOULD |
ZHANG Jiongming(Anshan Iron and Steel Research Institute; Anshan 114001);HE Jicheng; LI Baokuan(Northeastern University; Shenyang 110006) |
|
Cite this article:
ZHANG Jiongming(Anshan Iron and Steel Research Institute; Anshan 114001);HE Jicheng; LI Baokuan(Northeastern University; Shenyang 110006). INFLUENCE OF GAS INJECTION ON FLUID FLOW IN MOULD. Acta Metall Sin, 1995, 31(18): 269-274.
|
Abstract The mathmatical and physical model has been adopt to compute the fluid flow distribution in case of local gas holdup in mould. The photography was used to show fluid field. The predicated flow patterns show reasonable agreement with exprimental observations using actual water model.
|
|
1HuangX,ThomasBG,NajarFM.MetallTrans,1993;24B:3792HuangX,ThomasBG,NajarFM.Metallans,1993;23B:3393ThomasGB.SteelmakingConferenceProceedings,Vol.12,IronandSteelSocietyofUSA,1990:4234JooS,GuthrieRIL.CanMetallQ,1991;30:2615张风禄,蒋智.钢铁,1986;21(8):226沈巧珍,严永梅.钢铁,1990;25(9):227贺友多.传输过程的数值计算方法.北京:冶金工业出版社,19918BesshoN,YodaR,Yamasaki,FujiiT,NozakiT,TakatoriS.Proc6thIntIronandSteelCongress,Vol.3,TheIronandSteelInstituteofJapan,Nagoya,1990:340 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|