| ON NONPROPORTIONAL CYCLIC PROPERTIES OF TYPE 316 STAINLESS STEELS |
| YANG Xianjie; GAO Qing; HE Guoqiu; CAI Lixun (Southwest Jiaotong University; Chengdu; 610031) (Manuscript received 1995-04-10; in revised form 1995-08-23) |
|
Cite this article:
YANG Xianjie; GAO Qing; HE Guoqiu; CAI Lixun (Southwest Jiaotong University; Chengdu; 610031) (Manuscript received 1995-04-10; in revised form 1995-08-23). ON NONPROPORTIONAL CYCLIC PROPERTIES OF TYPE 316 STAINLESS STEELS. Acta Metall Sin, 1996, 32(1): 15-22.
|
|
|
Abstract 篈n experimental investigation was carried out of the cyclic properties of 316L and 316LN stainless steels subjected to uniaxial loading and biaxially nonproportional cyclic loadings. The properties of cyclic hardening, plastic flow and uniaxial kinematic hardening for the two kinds of steels were studied. It is shown that the properties depend not only on equivalent strain amplitude, but on strain path also. Some significant results were obtained.Correspondent: YANG Xianjie,(associate professor, Institute of Applied Mechanics, Southwest Jiaotong University, Chengdu 610031)
|
|
Received: 18 January 1996
|
| 1KremplE,LuH.In:BrownMW,MillerKJ.Eds.,BiaxialandMultiaxialFatigue,London:MechanicalEngineeringPublications,1989:892TanakaE,MurakamiS,OokaM.JMechPhysSolids,1985;33:5593杨显杰.金属材料循环塑性和循环粘塑性本构关系研究,西南交通大学博士学位论文,19924杨显杰,高庆,孙训方.航空学报,1994;15:12615NingJ,ChenX.IntJSolidsStruct,1991;28:4036OhashiY,TanakaE,OokaM.ASMEJEngMatTech,1985;107:2867杨显杰,高庆,蔡力勋,陈旭,袁珩.金属学报,1995;31:A170 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|