THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS |
CHEN Qiyuan; ZENG Wenming; ZHANG Pingmin (Central-South University of Technology; Changsha 410083)GU Songqing; YANG Guanqun; ZHOU Huifang; YIN Zhonglin (Zhengzhou Research institute of Light Metals; Zhengzhou 450041) (Manuscript received 1995-02-23; in revised form 1995-06-29) |
|
Cite this article:
CHEN Qiyuan; ZENG Wenming; ZHANG Pingmin (Central-South University of Technology; Changsha 410083)GU Songqing; YANG Guanqun; ZHOU Huifang; YIN Zhonglin (Zhengzhou Research institute of Light Metals; Zhengzhou 450041) (Manuscript received 1995-02-23; in revised form 1995-06-29). THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS. Acta Metall Sin, 1996, 32(1): 6-14.
|
Abstract An investigation on the thermodynamic properties of α-Al_2O_3, γ-Al_2O_3,gibbsite, boehmite and diaspore: standard enthalpy of formation, standard entropy, standard free energy of formation, and heat capacity was made based on calorimetric determinations and the published literatures. The reliability and consistency of the recommended values of these thermodynamic properties were discussed in detail.Correspondent: CHEN Qiyuan, professor,(Department of Chemistry, Central-South University of Technology, Changsha 410083)
|
Received: 18 January 1996
|
1FurukawaGT,DouglasTB,McCoskeyRE,GinningsDC.JResNatBurStand,1956;57:672EdwardsJW,KingtonGL.TransFaradySoc,1962;58:13133ChekhovskoiVYa.HighTemp,USSR,1964;2:2644BuycoEH.Proceedingsofthe4thsymposiumonThermophysicalProperties,NewYork:ASME,1968:1615ViswanathanR.JApplPhys,1975;46:40866ChangSS.Proceedingsofthe7thSymposiumonThermophysicalProperties,NewYork:ASME,1977:837DitmarsDA,IshiharaS,ChangSS,BernsteinG,WestED.JResNatBurStand,1982;87:1598CastanetR.HighTempHighPressures,1984;16:4499ParksGS,KelleyKK.JPhysChem,1926;30:4710ShomateCH,NaylorBF.JAmChemSoc,1945;67:7211DitmarsDA,DouglasTB.JResNatBurStand,1971;75:40112ShmidNE,SokolovVA.RussJInorgChem,1960;5:79713RomanovskiiVA,TarasovVV.SovPhysSolidState,1960;2:117614PalkinVA,KuzminaNN,ChernyaevII.RussJInorgChem,1965;10:2315SchauerA.CanJPhys,1965;43:52316MartinDL,SnowdonRL.CanJPhys,1966;44:144917GopalaRaoRV,GunjikarVG,SankarSG,BiswasAB.IndianJPureApplChem,1967;5:9918GronvoldF.ActaChemScand,1967;21:169519MartinDL,SnowdonRL.RevSciInstrum,1970;41:186920OnoderaN,KimotoA,SakiyamaM,SekiS.BullChemSocJpn,1971;44:146321GronvoldF.ActaChemScand.1972;26:221622TakahashiY,YokokawaH,KadokuraH,SekineY,MukaiboT.JChemThermodyn,1979;11:37923WalkerBE,GrandJA,MillerRR.JPhysChem,1956;60:23124FrederiksonDR,ChasanovMG.JChemThermodyn,1970;2:62325MurabayashiM,TakahashiY,MukaiboT.JNuclSciTech,1970;7:31226MacLeodAC.JChemThermodyn,1972;4:69927FomichevEN,BondarenkoVP,KandybaVV.HighTempHighPressures,1973;5:128EfremovaRI,MatizenEV.HighTempHighPressures,1976;8:39729ShmidtNE,MaksimovDN,RussJPhysChem,1979;53:108430ShmidtNE.RussJInorgChem,1966:11:24131FerrierA,OletteM.CRAcadSci.1962;254:429332ProphetH,StullDR.JChemEngData,1963;8:7833ParksGS,KelleyKK.BurMinesBull,1941;434:11534CoxJD,WagmanDD,MedvedevVA.CODATAKeyValuesforThermodynamics.NewYork:HemispherePublishingCorporation,1989:2135FugateRQ,SwensonCA,JApplPhys,1969;40:303436AppsJA,NeilJM.ACSSympSeries416.WashingtonDC,1990:41537RobieRA,HemingwayBS,FisherJR.USGeolSurvBull,1979:145238SnyderPE,SeltzH.JAmChemSoc,1945;67:68339HolleyCE,HuberEJJr.JAmChemSoc,1951;73:557740SchneiderA,GattowG.ZAnorgAllgemchem,1954;277:4141MahAD,JPhysChem,1957;61:157242ZenkovID.RussJPhysChem,1981;55:169843ChaseMW,CurnuttJL,McDonaldRA,SyverudAN.JPhysChemRefData,1978;7:793,83844HemingwayBS,RobieRA,KittrickJA.GeochimCosmochimActa,1978;42:153345MarchidanDI,PandeleL,NicolescuA.RevRoumChim,1972;17:149346ChenQ,ZengW,ChenX,GuS,YangG,ZhouH,YinZ.ThermochimActa,1995;253:3347BorerWJ,GunthardHH.HelvChimActa,1970;53:104348YokokawaT,KleppaOJ.JPhysChem,1964;68:324649ShomateCH,CookOA,AmChemSocJ,1946;68:214050HemingwayBS,RobieRA,FisherJR,WilsonWH.JResUSGeoSurv,1977;5:79751ChenQ,ZengW.GeochimCosmochimActa,1996,tobepublished52HemingwayBS,RobieRA.JResUSGeolSurv,1977;5:41353GrossP,ChristieJ,HaymanC.FulmerResInstRept6,1970,PG//JMN//R:2454BaranyR,KelleyKK.USBurMinesReptInv5825,1961;1355CoughlinJP.JPysChem,1958;62:41956ZengW,ChenQ,ChenX.GeochimCosmochimActa,1994;58:351157PalmerDA,WesolowskiDJ.GeochimCosmochimActa,1992;56:109358ChenQ,ZengW.JCentSouthUnivTech(EngEdit),1995;2:759HemingwayBS,RobieRA,AppsJA.AmMineralogist,1991;76:44560RusselAS,EdwardsJD,TaylorCS.JMetals,AIME,1955;203:112361KuyunkoNS,MalininSD,KhodakovskiyIL,GeochemInt,1983;20:7662KostomaroffV,ReyM.SilicatesIndustry,1963;28:963AppsJA,NeilJM,JunC-H,LawrenceBerkeleyLaboratoryRept21482,198864ZengW,ChenQ,ChenX.JChemThermodyn,1994;26:20565KingEC,BaranyR,WellerWW,PankratzLB.USBurMinesReptInv6962,196766MukaiboT,TakahashiY,YamadaK.Proc1stIntConfCalorThermodyn,Warsaw;1969:35767PerkinsD,EsseneEJr,WAllV.AmMineralogist,1979;64:108068FyfeWS,HollanderMA.AmJSci,1964;262:70969HassH.AmMineralogist,1972;57:137570SabatierG.BullSocFrMineralCrystallogr,1954;77:107771ZengW,ChenQ,GuS,YangG,ZhouH,YinZ.JChemThermodyn,1995;27:44372周红,曾文明,陈启元.中国有色金属学报,1993;3:4073PeryeaFJ,KittrickJA.ClaysClayMinerals,1988;36:391. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|