| PLASTIC DEFORMATION BEHAVIOR OF DIRECTION-ALLY SOLIDIFIED U720Li ALLOY AT ELEVATEDTEMPERATURE |
Bo GAO1,Lei WANG1( ),Taosha LIANG1,Yang LIU1,Xiu SONG1,Jinglong QU2 |
1 Key Lab for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China 2 High Temperature Material Research Institute, Central Iron and Steel Research Institute, Beijing 100081, China |
|
Cite this article:
Bo GAO,Lei WANG,Taosha LIANG,Yang LIU,Xiu SONG,Jinglong QU. PLASTIC DEFORMATION BEHAVIOR OF DIRECTION-ALLY SOLIDIFIED U720Li ALLOY AT ELEVATEDTEMPERATURE. Acta Metall Sin, 2016, 52(4): 437-444.
|
|
|
Abstract U720Li, a kind of precipitation type nickel-based superalloy, shows excellent mechanical properties at elevated temperature, which is also known as the difficult-to-deform alloy because of the high-alloying. To solve its deformation problem, new methods would be developed to enlarge the temperature deforming window and improve its plasticity. The hot compression deformation behaviors of directionally solidified and equiaxed grain U720Li alloys were studied by the MMS-300 testing system, as well as the dynamic recrystallization nucleation and growth mechanisms during the hot deformation were discussed. The microstructural characteristics of the alloy under different deformation conditions were examined using OM, SEM and EBSD. The results show that the deforming resistances of both directionally solidified and equiaxed grain U720Li alloys decrease with the increasing of deforming temperature. When the angle θ between the compression deforming direction and dendrite growth direction is 90°, the deforming resistance of directionally solidified U720Li alloy would be lower. With this direction, the coordination deformation between the dendrites becomes better and no crack can be found after deformation, which indicates that the deforming ability is best along θ=90° and it can be considered as the optimal deforming direction for directionally solidified U720Li alloy. Compared with equiaxed grain alloy, directionally solidified U720Li alloy performs higher deformation ability and more homogenous microstructures. During the deformation of directionally solidified U720Li alloy, bulging nucleation of grain boundary migration and dislocation pile-up induced nucleation are found as the main mechanism for the nucleation of dynamic recrystallization. In addition, the deformation activation energy of directionally solidified U720Li alloy is 766 kJ/mol, which is 482 kJ/mol lower than that of equiaxed grain alloy, indicating the directionally solidified U720Li alloy exhibits better hot-working plasticity.
|
|
Received: 10 July 2015
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51171039 and 51371044) and High Technology Research and Development Program of China (No.2012AA-03A513) |
| [1] | Guo J T.Materials Science and Engineering for Superalloys. Vol.1, Beijing: Science Press, 2008: 3 | | [1] | (郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 3) | | [2] | Huang Q Y, Li H K.Superalloy. Beijing: Metallurgy Industry Press, 2000: 1 | | [2] | (黄乾尧, 李汉康. 高温合金. 北京:冶金工业出版社, 2000: 1) | | [3] | Sharqhi-Moshtaqhin R, Asqari S.J Mater Process Technol, 2004; 147: 343 | | [4] | Guo J T.Materials Science and Engineering for Superalloys. Vol.2, Beijing: Science Press, 2008: 127 | | [4] | (郭建亭. 高温合金材料学(中册). 北京: 科学出版社, 2008: 127) | | [5] | Jackson M P, Reed R C.Mater Sci Eng, 1998; A259: 85 | | [6] | Pang H T, Reed P A S.Int J Fatigue, 2008; 30: 2009 | | [7] | Qu J L, Du J H, Bi Z N, Wang M Q, Zhang J, Wu G L.J Iron Steel Res, 2011; 23(suppl2): 247 | | [7] | (曲敬龙, 杜金辉, 毕中南, 王民庆, 张继, 吴桂林. 钢铁研究学报, 2011; 23(增刊2): 247) | | [8] | The Editorial Board of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook. Vol.2, 2nd Ed., Beijing: Standards Press of China, 2002: 271 | | [8] | (《中国航空材料手册》编委会. 中国航空材料手册. 第2卷, 第二版, 北京: 中国标准出版社, 2002: 271) | | [9] | Wang L A.Manufacturing Engineering for Hard Wrought Forgings. Beijing: National Defend Industry Press, 2005: 98 | | [9] | (王乐安. 难变形合金锻件生产技术. 北京: 国防工业出版社, 2005: 98) | | [10] | Monajati H, Jahazi M, Yue S, Taheri A K.Metall Mater Trans, 2005; 36A: 895 | | [11] | Guo X P, Gao L M, Guan P, Kusabiraki K, Fu H Z. Mater Sci Forum, 2007; 539-543: 3690 | | [12] | Tao C H, Zhang W F, Li Y J, Shi H J.Failure Analysis Prevention, 2006; 1(4): 1 | | [12] | (陶春虎, 张卫方, 李运菊, 施惠基. 失效分析与预防, 2006; 1(4): 1) | | [13] | Tao C H, Zhang W F, Shi H J, Zhang Z L.Recrystallization of Directionally Solidified Superalloy. Beijing: National Defend Industry Press, 2007: 1 | | [13] | (陶春虎, 张卫方, 施惠基, 张宗林. 定性凝固高温合金的再结晶. 北京: 国防工业出版社, 2007: 1) | | [14] | Zhao X B, Liu L, Yu Z H, Wang W G, Fu H Z.Mater Charact, 2010; 61: 7 | | [15] | Warnken N, Ma D, Mathes M, Steinbach I. Mater Sci Eng, 2005; A413-414: 267 | | [16] | Li X C.Met Sci Technol, 1986; 5(1): 99 | | [16] | (李秀臣. 金属科学与工艺, 1986; 5(1): 99) | | [17] | Xia W J.PhD Dissertation, Hunan University, Changsha, 2010 | | [17] | (夏伟军. 湖南大学博士学位论文, 长沙, 2010) | | [18] | Ebrahimi R, Najafizadeh A.J Mater Processing Technol, 2004; 152: 136 | | [19] | Guo J H, Zhao S D, Murakami R, Ding R X, Fan S Q.J Alloys Compd, 2013; 566: 62 | | [20] | Wu Z G, Li D F.Chin J Nonferrous Met, 2010; 20: 1321 | | [20] | (吾志刚, 李德富. 中国有色金属学报, 2010; 20: 1321) | | [21] | Yu J W, Liu X F, Xie J X.Acta Metall Sin, 2011; 47: 482 | | [21] | (余均武, 刘雪峰, 谢建新. 金属学报, 2011; 47: 482) | | [22] | Ouyang D L, Lu S Q, Cui X, Wu C, Dong X J.Trans Mater Heat Treatment, 2009; 30: 116 | | [22] | (欧阳德来, 鲁世强, 崔霞, 吴超, 董显娟. 材料热处理学报, 2009; 30: 116) | | [23] | Wang L, Pyczak F, Zhang J, Lou L H, Singer R F.Mater Sci Eng, 2012; A532: 487 | | [24] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena. Oxford: Pergamon, 2004: 285 | | [25] | Wang Y, Shao W Z, Zhen L, Zhang X M.Mater Sci Eng, 2008; A486: 321 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|