| FUNCTION OF MICROELEMENT Hf IN POWDER METALLURGY NICKEL-BASED SUPERALLOYS |
Yiwen ZHANG1,2( ),Benfu HU3 |
1 High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081 2 Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing 100081 3 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
Yiwen ZHANG,Benfu HU. FUNCTION OF MICROELEMENT Hf IN POWDER METALLURGY NICKEL-BASED SUPERALLOYS. Acta Metall Sin, 2015, 51(8): 967-975.
|
|
|
Abstract Hafnium (Hf) is one of the most important microelements in powder metallurgy (P/M) superalloy. Hf modifies the microstructure and drastically improves mechanical properties in P/M superalloy. The effect of Hf in a nickel-based P/M superalloy was systematically studied by means of FEG-SEM, TEM, AES, EDS and physical and chemical phase analysis. Hf mainly distributes at interdendritic region of the solidification powder in form of solid solution, which is helpful to reduce prior particle boundary (PPB). Hf facilitates morphology of g′ phase to be unstable and enhances the large cubic g′ phase to split into smaller ones, so the g′ phase turns into a stable state with a lower energy faster. Hf is mainly distributed in g′ phase and MC carbides, which changes the distribution of element between the g′ phase, MC and g solid solution, which is beneficial to eliminate notch sensitivity and improves overall mechanical properties of the alloy.
|
|
|
| Fund: Supported by International Science & Technology Cooperation Program of China (No.2014DFR50330) and Sino-Russion Intergovernmental Cooperation in Science & Technology Project (No.CR14-20) |
| [1] | Cochardt A W, Township W, County A. US Pat, 3005705, 1961 | | [2] | Academic Committee of the Superalloys CSM. China Superalloys Handbook. Beijing: China Zhijian Publishing House, 2012: 1 (中国金属学会高温材料分会. 中国高温合金手册(上), 北京: 中国质检出版社, 2012: 1) | | [3] | Davis J R. ASM Specialty Handbook: Nickel, Cobalt and Their Alloys. Materials Park: ASM International, 2000: 203 | | [4] | Evans D J, Eng R D. In: Hausner H H, Antes H W, Smith G D eds., Modern Developments in Powder Metallurgy. Vol.14, Princeton: MPIF and APMI, 1981: 51 | | [5] | Chang M, Koul A K, Cooper C. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Proc 8th Int Symp on Superalloy, Pennsylvania: TMS, 1996: 677 | | [6] | Miner R V. Metall Trans, 1977; 8A: 259 | | [7] | Larson J M, Volin T E, Larson F G. In: Braun J D, Arrowsmith H W, Mccall J L eds., Microstructural Science. Vol.5, New York: American Elsevier Pub., 1977: 209 | | [8] | Warren R, Ingesten N G, Winberg L, R?nnhult T. Powder Metall, 1984; 27: 141 | | [9] | Radavich J, Furrer D, Carneiro T, Lemsky J. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Proc 11th Int Symp on Superalloy, Pennsylvania: TMS, 2008: 63 | | [10] | Schirra J J, Reynolds P L, Huron E S, Bain K R, David P, Mourer D P. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Proc 10th Int Symp on Superalloy, Warrendale: TMS, 2004: 341 | | [11] | Wlodek S T, Kelly M, Alden D. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Sissinger R D, Klarstrom D L eds., Proc 7th Int Symp on Superalloy, Pennsylvania: TMS, 1992: 467 | | [12] | Locq D, Caron P. J Aerospace Lab, 2011; 3: 1 | | [13] | Hardy M C, Zirbel B, Shen G, Shankar R. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Proc 10th Int Symp on Superalloy, Warrendale: TMS, 2004: 83 | | [14] | Starink M J, Reed P A. Mater Sci Eng, 2008; A491: 279 | | [15] | Domingue J A, Boeseh W J, Radavich J F. In: Tien J K, Wlodek S T, Morrow H III eds., Proc 4th Int Symp on Superalloy, Ohio: ASM, 1980: 335 | | [16] | Hu B F, Chen H M, Song D, Li H Y. Acta Metall Sin, 2005; 41: 1042 (胡本芙, 陈焕铭, 宋 铎, 李慧英. 金属学报, 2005; 41: 1042) | | [17] | Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. J Shandong Univ Sci Technol (Nat Sci), 2009; 28: 51 (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 山东科技大学学报(自然科学版), 2009; 28: 51) | | [18] | Lifshitz I M, Slyzov V V. J Phys Chem Solids, 1961; 19: 35 | | [19] | Wagner C. Z Elektrochem, 1961; 65: 581 | | [20] | Menzies R G, Bricknell R H, Craven A J. Philos Mag, 1980; 41A: 493 | | [21] | Qiu C L, Attallah M M, Wu X H, Andrews P. Mater Sci Eng, 2013; A564: 176 | | [22] | Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1985; 74: 139 | | [23] | Miyazaki T, Imamura H, Mori H, Kozakai T. J Mater Sci, 1981; 16: 1197 | | [24] | Qiu Y Y. J Alloys Compd, 1998; 270: 145 | | [25] | Qiu Y Y. Acta Mater, 1996; 44: 4969 | | [26] | Kaufman M J, Voorhees P W, Johnson W C, Biancaniello F S. Metall Trans, 1989; 20A: 2171 | | [27] | Kotval P S, Venables J D, Calder R W. Metall Trans, 1972; 3: 453 | | [28] | Zhen B L, Zhang S J. Central Iron Steel Res Inst Technol Bull, 1981; 1(1): 65 (甄宝林, 张绍津. 钢铁研究总院学报, 1981; 1(1): 65) |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|