| EFFECT OF MICROELEMENT Hf ON THE MICRO- STRUCTURE OF POWDER METALLURGY SUPERALLOY FGH97 |
Yiwen ZHANG1,2( ),Shoubo HAN1,2,Jian JIA1,2,Jiantao LIU1,2,Benfu HU3 |
1 High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081 2 Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing 100081 3 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
Yiwen ZHANG,Shoubo HAN,Jian JIA,Jiantao LIU,Benfu HU. EFFECT OF MICROELEMENT Hf ON THE MICRO- STRUCTURE OF POWDER METALLURGY SUPERALLOY FGH97. Acta Metall Sin, 2015, 51(10): 1219-1226.
|
|
|
Abstract Microelement Hf added in Ni-based powder metallurgy (PM) superalloy can modify microstructure and improve mechanical properties, such as stress-rupture life, creep resistance and crack growth resistance, and also benefit to eliminate notch sensitivity. So systematically studying the effect of microelement Hf on PM superalloy microctructure will help to comprehend its corresponding mechanism. The effects of microelement Hf on the morphologies, chemical compositions and content of γ’ phase and MC carbide in FGH97 PM Superalloy were investigated by means of SEM and physiochemical phase analysis. The results showed that Hf facilitated the precipitations of γ’ phase and MC carbide, and changed chemical compositions of γ’ phase and MC carbide, the effect of Hf on the size and morphology of MC carbide was not obvious, while Hf greatly affected the size and morphology of γ’ phase and accelerated the splitting of γ’ phase from one instable cubic γ’ particle to stable octet of cubes. As Hf affected the lattice misfit of γ’/γ phase (d), modifying Hf content changed the critical splitting size of γ’ phase (Dc). The relationship between Dc and Hf content (w(Hf)) was found to be Dc=315.4+640.2w(Hf)-358.2[w(Hf)]2. With Hf content increased, the absolute value of d decreased and Dc increased. Cubic γ’ particle split into an octet of cubes when γ’ phase grew up to the critical splitting size.
|
|
|
| [1] | Evans D J, Eng R D. In: Hausner H H, Antes H W, Smith G D eds., Modern Developments in Powder Metallurgy. Vol.14, Princeton: MPIF and APMI, 1982: 51 | | [2] | Белов А Ф, Аношкин Н Ф, Фаткуллин О Х. In: Банных О А ed., Жаропрочные и Жаростойские Стали и Сплавы на Никелевой Основе, Москва: Наука, 1984: 31 | | [3] | Radavich J, Carneiro T, Furrer D, Lemsky J, Banik A. Chin J Aeronau, 2007; 20: 97 | | [4] | Radavich J, Furrer D, Carneiro T, Lemsky J. In: Reed R C, Green K A eds., Superalloys 2008, Pennsylvania: TMS, 2008: 63 | | [5] | Miner R V. Metall Trans, 1977; 8A: 259 | | [6] | Larson J M, Volin T E, Larson F G. In: Braun J D, Arrowsmith H W, McCall J L eds., Microstructural Science. New York: American Elsevier Pub, 1977: 209 | | [7] | Wang Y, Chen L Q, Khachaturyan A G. Acta Metall Mater, 1993; 41: 279 | | [8] | Qiu Y Y. Acta Mater, 1996; 44: 4969 | | [9] | Yoo Y S, Yoon D Y, Henry M F. Met Mater, 1995; 1: 47 | | [10] | Qiu Y Y. J Alloys Compd, 1998; 270: 145 | | [11] | Flageolet B, Villechaise P, Jouiad M. In: Green K A, Pollock T M, Haradra H eds., Superalloys 2004, Pennsylvania: TMS, 2004: 371 | | [12] | Starink M J, Reed P A S. Mater Sci Eng, 2008; A491: 279 | | [13] | Zhang Y W, Liu J T. Mater Chin, 2013; 32(1): 1 (张义文, 刘建涛. 中国材料进展, 2013; 32(1): 1) | | [14] | Zhang Y W, Wang F M, Hu B F. Rare Met Mater Eng, 2012; 41: 989 (张义文, 王福明, 胡本芙. 稀有金属材料与工程, 2012; 41: 989) | | [15] | Zhang Y W, Hu B F. Acta Metall Sin, 2015; 51: 967 (张义文, 胡本芙. 金属学报, 2015; 51: 967) | | [16] | Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1984; 67: 247 | | [17] | Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1985; 74: 139 | | [18] | Miyazaki T, Imamura H, Mori H, Kozakal T. J Mater Sci, 1981; 16: 1197 | | [19] | Miyazaki T, Imamura H, Kozakai T. Mater Sci Eng, 1982; 54: 9 | | [20] | Khachaturyan A G, Semenovskaya S V, Morris Jr J W. Acta Metall, 1988; 36: 1563 | | [21] | Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. J Shandong Univ Sci Technol (Nat Sci), 2009; 28(1): 51 (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 山东科技大学学报(自然科学版), 2009; 28(1): 51) |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|