| ELECTROCHEMICAL CORROSION BEHAVIOR OF NANOCRYSTALLIZED MATERIALS: GROWTH OF PASSIVE FILM AND LOCAL PITTING CORROSION |
LIU Li( ), LI Ying, WANG Fuhui |
| State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
LIU Li, LI Ying, WANG Fuhui. ELECTROCHEMICAL CORROSION BEHAVIOR OF NANOCRYSTALLIZED MATERIALS: GROWTH OF PASSIVE FILM AND LOCAL PITTING CORROSION. Acta Metall Sin, 2014, 50(2): 212-218.
|
|
|
Abstract Compared with the traditional coarse-grained materials, the electrochemical corrosion behavior of nanocrystalline materials has changed obviously. Nanocrystallization influences the properties of passive film on passive materials. In this paper, the current understanding of the growth of passive film and local pitting corrosion on nanocrystalline materials by dynamic research techniques were reviewed. The results indicate that nanocrystallization changed the nucleation mechanism of the passive film from progressive to instantaneous, and which promotes the growth rate of the passive film, both of which promote the compact properties of the passive film. The effects of nanocrystallization on local pitting corrosion behavior are concluded: (1) more frequent occurrence of metastable pits, but with lower probability of transition to stable pits, which is attributable to differences in morphologies of sulfur and manganese as well as outstanding repassivation ability of nanocrystalline thin film; (2) nanocrystallization decreases stable pit generation rate and its propensity to form larger pit cavities, and modifies the morphology of stable pit cavity.
|
|
Received: 27 September 2013
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50801063 and 51271187) |
| [1] |
Intrui R B, Szklarska-Smialowska Z. Corrosion, 1992; 48: 398
|
| [2] |
Li Y, Wang F H, Liu G. Corrosion, 2004; 60: 891
|
| [3] |
Mariano N A, Souza C A C, Oliviera M F. Mater Sci Forum, 2000; 343: 861
|
| [4] |
Zeiger W, Schneider M, Scharnweber D. Nanostruct Mater, 1995; 6: 1013
|
| [5] |
Youssef K M S, Koch C C, Fedkiw P S. Corros Sci, 2004; 46: 51
|
| [6] |
Wang L P, Zhang J Y, Gao Y, Xue Q J, Hu L T, Xu T. Scr Mater, 2006; 55: 657
|
| [7] |
Wang X Y, Li D Y. Electrochim Acta, 2002; 47: 3939
|
| [8] |
Liu L, Li Y, Wang F H. Electrochim Acta, 2007; 52: 2392
|
| [9] |
Liu L, Li Y, Wang F H. Electrochim Acta, 2007; 52: 7193
|
| [10] |
Zhang B, Li Y, Wang F H. Corros Sci, 2007; 49: 2071
|
| [11] |
Liu L, Li Y, Wang F H. Electrochim Acta, 2008; 54: 768
|
| [12] |
Meng G Z, Li Y, Wang F H. Electrochim Acta, 2006; 51: 4277
|
| [13] |
Ye W, Li Y, Wang F H. Electrochim Acta, 2006; 51: 4426
|
| [14] |
Philipp R, Retter U.Electrochim Acta, 1995; 40: 1581
|
| [15] |
Philipp R, Retter U. Thin Solid Films, 1991; 207: 42
|
| [16] |
Vvedenskii A V, Grushevskaya S N. Corros Sci, 2003; 45: 2391
|
| [17] |
Hills G J, Peter L M, Scharifker B R. J Electroanal Chem, 1981; 124: 247
|
| [18] |
Pan C, Liu L, Li Y, Wang S G, Wang F H. Electrochim Acta, 2011; 56: 7740
|
| [19] |
Ji H B, Lin W M.J Chem Ind Eng, 1997; 48: 453
|
| [20] |
Pan C.PhD Dissertation. Institute of Metal Research, Chinese Academy of Science, Shenyang, 2012
|
|
(潘 晨. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
|
| [21] |
Song S Z, Tang Z L. Acta Metall Sin, 1995; 31: B61
|
|
(宋诗哲, 唐子龙. 金属学报 1995; 31: B61)
|
| [22] |
Liu L, Li Y, Wang F H. J Mater Sci Technol, 2010; 26: 1
|
| [23] |
Liu L, Li Y, Wang F H. Electrochim Acta, 2008; 53: 2453
|
| [24] |
Pan C, Liu L, Li Y, Wang F H. Corros Sci, 2013; 73: 32
|
| [25] |
Zheng S J, Wang Y J, Zhang B, Zhu Y L, Liu C, Hu P, Ma X L. Acta Mater, 2010; 58: 5070
|
| [26] |
Liu L, Li Y, Wang F H. Electrochim Acta, 2010; 55: 2430
|
| [27] |
Burstein G, Vines S. J Electrochem Soc, 2001; 148: B504
|
| [28] |
Pan C, Liu L, Li Y, Wang F H. Thin Solid Film, 2011; 519: 4781
|
| [29] |
Shibata T. Corros Sci, 1996; 52: 813
|
| [30] |
Gumbel E J. Statistics of Extremes. New York: Columbia University Press, 1957: 87
|
| [31] |
Sun D, Jiang Y, Tang Y, Xiang Q, Zhong C, Liao J, Li J. Electrochim Acta, 2009; 54: 1558
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|