| HIGH TEMPERATURE CORROSION OF NANO-CRYSTALLINE METALLIC MATERIALS |
PENG Xiao( ), WANG Fuhui |
| State Key Laboratory for Corrosion and Protection, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
PENG Xiao, WANG Fuhui. HIGH TEMPERATURE CORROSION OF NANO-CRYSTALLINE METALLIC MATERIALS. Acta Metall Sin, 2014, 50(2): 202-211.
|
|
|
Abstract Some structural metallic materials, with only necessary to?be?“nanocrystallized” rather than to be increased with the contents of Cr and Al, have the ability to thermally grow a protective scale of Cr2O3 and Al2O3 at high temperature environments. Nanocrystallizationof alloys containing Cr or/and Al is an alternative to conventionally coating them with a high-Cr or/and high-Al material. High temperature corrosion behaviors of nanocrystalline metallic materials have been extensively reported in the past 20 years. In this paper, characteristics of high temperature corrosion of nanocrystalline metals, together with the fundamental reasons and questions desired to be clarified for the improvement of the corrosion resistance of alloys by nanocrystallization, were briefly reviewed.
|
|
Received: 22 September 2013
|
|
|
| Fund: Support by National Natural Science Foundation of China (No.51271189) |
| [1] |
Kofstad P. High Temperature Corrosion. London: Elsevier Applied Science, 1988: 1
|
| [2] |
Nicholls J R, Simms N J, Chan W Y, Evans H E. Surf Coat Technol, 2002; 149: 236
|
| [3] |
Peng X. In: Xu H, Guo H eds., Thermal Barrier Coatings. Cambridge, England: Woodhead Pub. Ltd., 2011: 53
|
| [4] |
Kelly F C. Trans Electrochem Soc, 1923; 43: 351
|
| [5] |
Samuel R L, Lockidngton N A. Met Treatment Drop Forging, 1951; 18: 354
|
| [6] |
Drewett R. Anti-Corros Methods Mater, 1969; 16: 543
|
| [7] |
Goward G W. Surf Coat Technol, 1998; 108-109: 73
|
| [8] |
Geib F D, Rapp R A. Oxid Met, 1993; 40: 213
|
| [9] |
Nicholls J R, Hancock P, Al Yasiri L H. Mater Sci Technol, 1989; 5: 799
|
| [10] |
Evans D J, Elam R C. US Patent, 3.676.085, 1972
|
| [11] |
Ajdelsztajn L, Picas J A, Kim G E, Bastian F L, Schoenung J, Provenzano V. Mater Sci Eng, 2002; A338: 33
|
| [12] |
Giggins C S, Pettit F S. Trans TMS-AIME, 1969; 245: 2509
|
| [13] |
Wang F, Lou H. Mater Sci Eng, 1990; A43: 279
|
| [14] |
Peng X, Wang F. In: Gao W, Li Z eds., Developments in High-temperature Corrosion and Protection of Materials. Cambridge, England: Woodhead Pub. Ltd., 2009: 456
|
| [15] |
Umemote M, Todaka Y, Tsuchiya K. Mater Trans, 2003; 44: 1488
|
| [16] |
Tao N R, Sui M L, Lu J, Lu K. Nanostruct Mater, 1999; 11: 4
|
| [17] |
Tong W P, Tao N R, Wang Z B, Lu J, Lu K. Science, 2003; 229: 686
|
| [18] |
Yavari A R. Mater Trans, 1995; 36: 228
|
| [19] |
Peng X. Nanoscale, 2010; 2: 262
|
| [20] |
Zhang Y, Peng X, Wang F H. Mater Lett, 2004; 58: 1134
|
| [21] |
Zhou Y, Peng X, Wang F H. Scr Mater, 2004; 50: 1429
|
| [22] |
Zhang C, Peng X, Zhao J, Wang F H. J Electrochem Soc, 2005; 152: B321
|
| [23] |
Douglass D L. Corros Sci, 1968; 8: 665
|
| [24] |
Chen G F, Lou H Y. Mater Lett, 2002; 45: 286
|
| [25] |
Singh R R K, Khanna A S, Tiwari R K, Gnanamoorttsy J B. Oxid Met, 1992; 37: 1
|
| [26] |
Singh R R K, Gnanamoorttsy J B. Oxid Met, 1992; 38: 483
|
| [27] |
Singh R R K, Gnanamoorttsy J B, Roy S K. Oxid Met, 1994; 42: 335
|
| [28] |
Wagner C Z. Elektrochem, 1959; 63: 772
|
| [29] |
Liu Z, Gao W, Dahm K L, Wang F. Acta Mater, 1998; 46: 1691
|
| [30] |
Peng X, Wang F H. Corros Sci, 2003; 45: 2293
|
| [31] |
Dong Z, Peng X, Guan Y, Li L, Wang F H. Corros Sci, 2012; 62: 147
|
| [32] |
Huang Z, Peng X, Xu C, Wang F H. J Mater Res, 2007; 22: 3166
|
| [33] |
Huang Z, Peng X, Xu C, Wang F H. J Electrochem Soc, 2009; 156: C95
|
| [34] |
Wang F H, Tian X, Li Q, Li L, Peng X. Thin Solid Films, 2008; 516: 5740
|
| [35] |
Yang X, Peng X, Wang F H. J Electrochem Soc, 2009; 156: C167
|
| [36] |
Wagner C. J Electrochem Soc, 1952; 99: 369
|
| [37] |
Lou H, Zhu S, Wang F H. Oxid Met, 1995; 43: 317
|
| [38] |
Peng X, Li M, Wang F H. Corros Sci, 2011; 53: 1616
|
| [39] |
Peng X, Yan J, Zhou Y, Wang F H. Acta Mater, 2005; 53: 5079
|
| [40] |
Geng S, Eang F, Zhu S, Wu W. Oxid Met, 2002; 57: 549
|
| [41] |
Yang X, Peng X, Wang F H. Scr Mater, 2007; 56: 891
|
| [42] |
Wang F, Lou H, Zhu S, Wu W. Oxid Met, 1996; 45: 39
|
| [43] |
Yang S, Wang F, Sun Z, Zhu S. Intermetallics, 2002; 10: 467
|
| [44] |
Funkenbush A M, Smeggil J G, Smeggil N S. Metall Trans, 1985; 16A: 1164
|
| [45] |
Lees D G. Oxid Met,1987; 27: 75
|
| [46] |
Hou P Y. Annu Rev Mater Res, 2008; 38: 275
|
| [47] |
Li Q, Peng X, Zhang J Q, Zong G X, Wang F H. Corros Sci, 2010; 52: 1213
|
| [48] |
Evans A G, Crymley G B, Demaray R E. Oxid Met, 1983; 20: 193
|
| [49] |
Suo Z. J Mech Phys Solids, 1995; 43: 829
|
| [50] |
Christensen R J, Lipkin D M, Clarke D R. Acta Mater, 1996; 44: 3813
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|