| [1] Li Y J, Choi P, Goto S, Borchers C, Raabe D, Kirchheim R. Acta Mater, 2012; 60: 4005 [2] Tashiro H. Nipp Steel Tec Rep, 1999; 80: 6 [3] Choi H C, Park K T. Scr Mater, 1996; 34: 857 [4] Taleff E M, Sridhar G B, Pourladian B. Wire J Int, 2003; 36: 73 [5] Bae C M, Nam W J, Lee C S. Metall Mater Trans, 2000; 31A: 2665 [6] Jang Y S, Phaniraj M P, Kim D I, Shim J H, Huh M Y. Metall Mater Trans, 2010; 41A: 2078 [7] Kanetsuki Y, Ibaraki N, Ashida S. ISIJ Int, 1991; 31: 304 [8] Taleff E M, Syn C K, Lesuer D R, Sherby D. Metall Mater Trans, 1996; 27A: 111 [9] Peng H F, Song X Y, Gao A G, Ma X L. Mater Lett, 2005; 59: 3330 [10] Zhang Y D, Esling C, Gong M L, Vincent G, Zhao X, Zuo L. Scr Mater, 2006; 54: 1897 [11] San Martin D, Rivera-Diaz-del-Castillo P E J, Garcia-de-Andres C. Scr Mater, 2008; 58: 926 [12] Elwazri A M, Wanjara P, Yue S. Metall Mater Trans, 2005; 36A: 2297 [13] Li Y, Yang Z M. Acta Metall Sin, 2010; 46: 1501 (李翼, 杨忠民. 金属学报, 2010; 46: 1501) [14] Han K, Mottishaw T D, Smith G, Edmonds D V, Stacey A G. Mater Sci Eng, 1995; A190: 207 [15] Liu Z C. Heat Treat Met, 2007; 33: 1 (刘宗昌. 金属热处理, 2007; 33: 1) [16] Roberts G A, Mehl R F. Trans AIME, 1943; 154: 318 [17] Porter D A, Easterling K E, Sherif M Y, translated by Chen L, Yu Y N. Phase Transformation in Metals and Alloys. Beijing: Higher Education Press, 2011: 63 (Porter D A, Easterling K E, Sherif M Y 著, 陈冷, 余永宁 译. 金属和合金中的相变. 北京: 高等教育出版社, 2011: 63) [18] Borchardt F S. Master Thesis, University of Pittsburgh, 2004 [19] Scheil E. Arch Eisenhuttenw, 1935; 8: 565 [20] Brandt W H. Trans AIME, 1946; 167: 550 [21] Hull F C, Colton R A, Mehl R F. Trans AIME, 1942; 50: 185 [22] Guo N. PhD Dissertation, Chongqing University, 2012 (郭宁. 重庆大学博士学位论文, 2012) [23] Howell P R. Mater Charact, 1998; 40: 227 [24] Elwazri A M, Wanjara P, Yue S. Mater Sci Eng, 2005; A404: 91 [25] Han K, Smith G, Edmonds D V. Metall Mater Trans, 1995; 26A: 1617 [26] Han K, Edmonds D V, Smith G. Metall Mater Trans, 2001; 32A: 1313 [27] Nesterov D, Levchenko N, Sapozhkov V, Shevchenko A. Steel Trans, 1992; 22: 191 [28] Hung C Y, Spanos G, Rosenberg R O, Kral M V. Acta Mater, 2002; 50: 3781 [29] Kral M V, Spanos G. Acta Mater, 1999; 47: 711 [30] Kral M V, Spanos G. Acta Mater, 2003; 51: 301 [31] Spanos G, Kral M V. Int Mater Rev, 2009; 54: 19 [32] Kral M V, Spanos G. Scr Mater, 1997; 36: 875 [33] Kral M V, Mangan M A, Spanos G, Rosenberg R O. Mater Charact, 2000; 45: 17 |