| EFFECTS OF PRECIPITATION FOR AGING ONMECHANICAL AND CORROSION RESISTANCE PROPERTIES OF CAST 2507 SUPER DUPLEX STAINLESS STEEL |
| XIANG Hongliang, LIU Dong, RUAN Fangru, HE Fushan, HUANG Liguang |
| School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108 |
|
Cite this article:
XIANG Hongliang LIU Dong RUAN Fangru HE Fushan HUANG Liguang. EFFECTS OF PRECIPITATION FOR AGING ONMECHANICAL AND CORROSION RESISTANCE PROPERTIES OF CAST 2507 SUPER DUPLEX STAINLESS STEEL. Acta Metall Sin, 2010, 46(8): 941-945.
|
|
|
Abstract Duplex stainless steel (DSS) has been used widely due to its very excellent combination of mechanical and corrosion resistance properties. However, the use of DSS is limited by their susceptibility to the formation of dangerous intermetallic phases, such as χ phase and phase, resulting in the detrimental effects on mechanical properties and corrosion resistance. With the application of the super duplex stainless steel (SDSS) with a pitting resistance equivalent number more than 40. The harmful effects of intermetallic phases easily precipitated in DSS on mechanical properties and corrosion resistance are a research focus. This paper, based on prior study, investigates the effects of intermetallic phases formed during aging on the mechanical properties and corrosion resistance of cast 2507 super duplestainless steel by means of optical microscope (OM), scanning electron microscope (SEM), tensile test and electrochemical test. The results indicate that for the solution annealing cast 2507 super duplex stainless steel aged in the temperature range 650—950 ℃, small and depressive distribution χ phase precipitatd from ferrite can increase its tensile strength, but σ phase causes the opposing effect on its plasticity owing to precipitated along grain boundaries. Both of them can rapidly deteriorate its plasticity, and cause brittle failure. The effect of σ phase on corrosion resistance of 2507 SDSS is weaker than phase. The more the σ phase is, the worse the corrosion resistant could be.
|
|
Received: 25 March 2010
|
| Fund: Supported by Program for Service of Enterprise by Technical Personnel, the Ministry of Science and Technology of China (No.2009GJC40018), Innovation Foundation for Young Talent of Fujian Province (No.2008F3061) and Technological Development Foundation of Fuzhou University (No.2008–XQ–16) |
| [1] Wu J. Corrosion & Protection in Petrochem Industry, 1996; 13: 6
(吴玖.石油化工腐蚀与防护. 1996; 13: 6)
[2] Graham G. 2th Int Conf on Duplex Stainless Steel. Beijing: Stainless steel council China Special steel Enterprises association, 2006:218
[3] Benson M, Snis M. 2th Int Conf on Duplex Stainless Steel. Beijing: Stainless steel council China Special steel Enterprises association, 2006:17
[4] Erich F, translated by Su Z X. Welding metallurgy of stainless steel, Beijing: Chemical Industry Press, 2004: 74
(Erich F著, 栗卓新译. 不锈钢焊接冶金. 北京: 化学工业出版社, 2004: 74)
[5] Henrik S, Rolf S. Mater Sci Eng, 2007, 444A: 271
[6] Elmer J W, Palmer T A. Mater Sci Eng, 2007, 459 A: 151
[7] Russell S W, Lundin C D. Final Report for the Development of Energy: the Development of Qualification Standards for Cast Duplex Stainless Steel the University of Tennessee Knoxville, 2005,2:8
[8] Ezuber H M,. El-Houd A,. El-Shawesh F. Desalination. 2007, 207: 268
[9]Huang C, Shih C. Mater Sci Eng, 2005,A402: 66
[10] Chen J Y, Yang Z Y, Yang W, Su J, Luo F H. J Iron Steel Res, 2006; 18:2
(陈嘉砚, 杨卓越, 杨武, 苏杰, 罗丰华. 钢铁研究学报. 2006, 18: 1)
[11] Long J M, Fan A M. Phys Test, 1997; 15(1):1
(龙晋明, 樊爱民. 物理测试. 1997; 15(1):1)
[12] Otarola T, Hollner S, Bonnefois B. Eng Fail Anal, 2005; 12: 930
[13] Marcelo M, Leonardo R F. Mater Char. 2007; doi:10.1016/j.matchar.2007.02.010.
[14] Pohl M, Storz O, Glogowski T. Mater Sci Eng, 2007, 58: 66.
[15].Redja A,. Proult A,. Donnadieu P,. Morniroli J. J Mater Sci, 2004; 39: 2386.
[16] Takuyo Y, Satoshi O, Hisashi K. J Nuclear Mater. 2006, 350: 47
[17] Xiang H L, He F S, Liu D. Acta Metall Sin, 2009; 45:1456
(向红亮, 何福善, 刘东. 金属学报, 2009; 45: 1456
[18] Jang Y, Kim S, Lee J. Metall Mater Trans, 2005; 36A: 1229
[19] Chiu P K, Wang S.H, Yang J R, Weng K L, Jason F. Mater Chem Phys, 2006; 98: 103
[20] Zhong Q P. Zhao Z H. Fractography. Beijing: High Education Press, 2006: 202
(钟群鹏, 赵子华. 断口学. 北京: 高等教育出版社, 2006:202)
[21] Tavares S S, Terra V. F, Neto P, Lima, D E. Matos. Microchimica Acta. 2005, 40: 4025
[22] Xiang H L, Huang W L, Liu D, He F S. Acta Metall Sin. 2010, 46:304
(向红亮, 黄伟林, 刘东, 何福善. 金属学报. 2010, 46: 304)
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|