EFFECT OF WITHDRAWAL RATE ON THE MICROSTRUCTURE OF DIRECTIONAL SOLIDIFIED Ti-47Al-2Cr-2Nb-0.8B ALLOYS
YANG Lili, ZHENG Lijing, XIAO Zhixia, YAN Jie, ZHANG Hu
School of Materials Science and Engineering, Beijing University of Aeronautics and Astronautics, Beijing 100191
Cite this article:
YANG Lili ZHENG Lijing XIAO Zhixia YAN Jie ZHANG Hu. EFFECT OF WITHDRAWAL RATE ON THE MICROSTRUCTURE OF DIRECTIONAL SOLIDIFIED Ti-47Al-2Cr-2Nb-0.8B ALLOYS. Acta Metall Sin, 2010, 46(7): 879-884.
The microstructures, morphology of boride and grain refinement in directional solidified Ti-47Al-2Cr-2Nb-0.8B alloy with different withdrawal rates have been investigated. The results indicated that the primary phase, borides and their precipitation consequence varied with the increasing of withdrawal rates (0.36, 5, 10 and 20 mm/min). The morphologies of borides and grain refinement were affected by the solidification paths due to the different withdrawal rates. The alloy with fine grains and borides were obtained at the withdrawal rate of 5 mm/min.
[1] Loria E A. Intermetallics, 2000; 8: 1339
[2] Lasalmonie A. Intermetallics, 2006; 14: 1123
[3] Lin J P, Chen G L. Mater China, 2009; 28: 31
(林均品, 陈国良. 中国材料进展, 2009; 28: 31)
[4] Godfrey A B. PhD Thesis, University of Birmingham, 1996
[5] Hu D. Intermetallics, 2001; 9: 1037
[6] Hecht U, Witusiewicz V, Drevermann A, Zollinger J. Intermetallics, 2008; 16: 969
[7] Yamaguchi M, Johnson D R, Inui H. Intermetallics, 2000; 8: 511
[8] Li X Z, Sun T, Peng P, Su Y Q, Guo J J, Fu H Z. Acta Metall Sin, 2009; 11: 1336
(李新中, 孙涛, 彭鹏, 苏彦庆, 郭景杰, 傅恒志. 金属学报, 2009; 11: 1336)
[9] Li X Z, Sun T, Yu C X, Su Y Q, Cao Z Y, Guo J J, Fu H Z. Acta Metall Sin, 2009; 12: 1479
(李新中, 孙涛, 于彩霞, 苏彦庆, 曹智勇, 郭景杰, 傅恒志. 金属学报, 2009; 12: 1479)
[10] Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T. Acta Mater, 2006; 54: 1077
[11] Hyman M E, McCullough C, Valencia J J, Levi C G, Mehrabian R. Metall Trans, 1989; 20A: 1847
[12] Larson D J, Liu C T, Miller M K. Intermetallics, 1997; 5: 411
[13] Hu D. Intermetallics, 2001; 9: 1037
[14] Christodoulou J A, Flower H M. Adv Eng Mater, 2000; 2: 631
[15] Johnson D R, Chihara K, Inui H, Yamaguchi M. Acta Mater, 1998; 46: 6529