STUDY ON FATIGUE CRACK GROWTH BEHAVIOR OF 16MnR STEEL UNDER DIFFERENT CONDITIONS
XIONG Ying1;2;  CHEN Bingbing1;2;  ZHENG Sanlong1;2; GAO Zengliang1;2
1) College of Mechanical Engineering; Zhejiang University of Technology;
Hangzhou 310032
2) The Ministry of Education Key Laboratory of Mechanical Manufacture and
Automation; Zhejiang University of Technology; Hangzhou 310032
Cite this article: 

XIONG Ying CHEN Bingbing ZHENG Sanlong GAO Zengliang. STUDY ON FATIGUE CRACK GROWTH BEHAVIOR OF 16MnR STEEL UNDER DIFFERENT CONDITIONS. Acta Metall Sin, 2009, 45(7): 849-855.

Download:  PDF(1191KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

16MnR steel is a most widely used material for pressure vessels. The study on fatigue is very important for safety and fatigue life assessment of pressure vessels. Several experimental researches for fatigue of 16MnR steel were conducted and test data have been gotten, but it was short of fatigue study of the material under various conditions at present. The fatigue crack growth tests of 16MnR hot--rolling steel were carried out at different< temperatures and R--ratios with compact tension (CT) specimens in this paper. Different sized circular notches at the tip of the slot ranging from very sharp< to blunt were used in the CT specimens and the radii of the notches were 0.1, 1 and 2 mm, and the thicknesses of CT specimens were 3.8, 12.5, 18 and 25 mm, respectively. The fatigue crack growth performances were obtained. The effects of temperatures, notch sizes, R--ratios and specimen thickness on fatigue crack growth behaviors were studied. It was shown that the fatigue crack growth rates at 150 and 300 ℃ were lower than those at 25 and 425 ℃, the lowest one was at 300 ℃ and the crack growth rate increased with temperature above 300 ℃. The great influence of notch sizes on the fatigue crack growth rate was observed at early stage of crack growth only. The results also indicated that fatigue crack growth rate increased as the specimen thickness increased, but the fatigue crack growth rate of 16MnR steel was insensitive to the R--ratios.

Key words:  16MnR steel      fatigue crack growth rate      high temperature      notch sizes      R-ratio      specimen thickness     
Received:  21 October 2008     
ZTFLH: 

TF777.1

 
Fund: 

Supported by National High Technology Research and Development Program of China (No.007AA04Z430), the Scientific Research Foundation for the Returned Overseas Chinese Scholars and Natural Science Foundation of Zhejiang Province (No.Y107284)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I7/849

[1] Fan Z C, Jiang J L. J Zhejiang Univ: Eng Sci, 2004; 38: 1190
(范志超, 蒋家羚. 浙江大学学报(工学版), 2004; 38: 1190)

[2] Tao W H, Sun W M, Yang J L. J Mech Strength, 2000; 22: 243
(陶伟华, 孙伟明, 杨金来. 机械强度. 2000; 22: 243)

[3] Ren W, Zhang K D. Pressure Vessel Technol, 1996; 13: 205
(任伟, 张康达. 压力容器. 1996; 13: 205)

[4] Gao Z L, Zhang K D. J Mater Process Technol, 1997; 63: 559
[5] Shahinian P. Nucl Technol, 1976; 30: 390
[6] Kim J K, Shim D S. Int J Fatigue, 2000; 22: 611
[7] Jack A R, Price A T. Acta Metall, 1972; 20: 857
[8] James L A. ASTM STP 738, 1981; 45
[9] Park H B, Lee B W. Nucl Eng Des, 2000; 197: 197
[10] Costa J D M, Ferreira J A M. Theor Appl Fracture Mech, 1998; 30: 65
[11] Korda Akhmad A, Mutoha Y, Miyashita Y, Sadasue T. Mater Sci Eng, 2006; A428: 262
[12] Wang X G, Gao Z L, Zhao T W, Jiang Y Y. ASME J Pressure Vessel Technol, 2009; 131: 021202
[13] Cheng Y R. Fatigue Strength, Beijing: China Railway Publishing House, 1990: 139
(程育仁. 疲劳强度, 北京: 铁道出版社, 1990: 139)

[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[4] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[5] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[6] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[7] XU Jinghui, LI Longfei, LIU Xingang, LI Hui, FENG Qiang. Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC[J]. 金属学报, 2021, 57(2): 205-214.
[8] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[9] LI Xiaohui, WANG Jianqiu, HAN En-Hou, GUO Yanjun, ZHENG Hui, YANG Shuangliang. Electrochemistry and In Situ Scratch Behavior of 690 Alloy in Simulated Nuclear Power High Temperature High Pressure Water[J]. 金属学报, 2020, 56(11): 1474-1484.
[10] BAO Feiyang, LI Yanfen, WANG Guangquan, ZHANG Jiarong, YAN Wei, SHI Quanqiang, SHAN Yiyin, YANG Ke, XU Bin, SONG Danrong, YAN Mingyu, WEI Xuedong. Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃[J]. 金属学报, 2020, 56(10): 1366-1376.
[11] Jinyao MA,Jin WANG,Yunsong ZHAO,Jian ZHANG,Yuefei ZHANG,Jixue LI,Ze ZHANG. Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(8): 987-996.
[12] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[13] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[14] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[15] Yanchun ZHAO, Hao SUN, Chunling LI, Jianlong JIANG, Ruipeng MAO, Shengzhong KOU, Chunyan LI. High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites[J]. 金属学报, 2018, 54(12): 1818-1824.
No Suggested Reading articles found!