| LOW--CYCLE FATIGUE BEHAVIOR OF AS--EXTRUDED Mg--x%Al--3%Ni ALLOYS |
| CHEN Lijia; WANG Xin; ZHI Ying; XU Yanwu |
| School of Materials Science and Engineering; Shenyang University of Technology; Shenyang 110178 |
|
Cite this article:
CHEN Lijia WANG Xin ZHI Ying XU Yanwu. LOW--CYCLE FATIGUE BEHAVIOR OF AS--EXTRUDED Mg--x%Al--3%Ni ALLOYS. Acta Metall Sin, 2009, 45(7): 856-860.
|
|
|
Abstract Due to the low density, high specific strength and stiffness, magnesium alloys are being considered for automotive and aerospace applications. The structural applications of magnesium components need a decent low--cycle fatigue performance, because cyclic loading is often encountered. In order to identify the low--cycle fatigue behavior of the newly developed Mg--x%Al--3%Ni(x=4, 5, 6, 7, mass fraction) extruded magnesium alloys with different contents of Al, the total strain--controlled low--cycle fatigue tests were performed at room temperature. The cyclic stress response, strain fatigue life and cyclic stress--strain behaviors were investigated for the hot--extruded Mg--x%Al--3%Ni alloys. The results of the low--cyclic fatigue tests show that the hot--extruded Mg--x%Al--3%Ni alloys exhibit the cyclic strain hardening during fatigue deformation. The dependences of the strain fatigue life on plastic strain amplitude and elastic strain amplitude can be described by the Coffin--Manson and Basquin equations, respectively. In the hot extruded Mg--x%Al--3%Ni alloys with different contents of Al, the extruded Mg--5%Al--3%Ni alloy gives the longest fatigue life and the highest fatigue resistance. In addition, a linear relation between the cyclic stress amplitude and cyclic strain amplitude can be noted for the hot--extruded Mg--x%Al--3%Ni alloys.
|
|
Received: 25 November 2008
|
|
|
| Fund: Supported by Natural Science Foundation of Liaoning Province (No.20072039) |
| [1] Liu J A, Li J X. Sichuan Nonferrous Met, 2007; (1): 2
(刘静安, 李建湘. 四川有色金属, 2007; (1): 2)
[2] Eliezer D, Aghion E, Froes F H. Adv Performance Mater, 1998; 5: 201
[3] Friedrich H, Schumann S. J Mater Process Technol, 2001; 117: 276
[4] Kojima Y. Mater Sci Forum, 2000; 350–351: 3
[5] Liu Y, Li Y Y, Zhang W W, Luo Z Q, Zhang D T. Light Met, 2002; (8): 56
(刘英, 李元元, 张卫文, 罗宗强, 张大童. 轻金属, 2002; (8): 56)
[6] Hu X J, Gao H W, Li C M, Liu S H, Liu L M. Shanghai Nonferrous Met, 2004; 25(3): 100
(胡晓菊, 高洪吾, 李长茂, 刘顺华, 刘黎明. 上海有色金属, 2004; 25(3): 100)
[7] Zhang S C, Duan H Q, Cai Q Z, Wei B K, Lin H T, Chen W C. Foundry, 2001; 50: 310
(张诗昌, 段汉桥, 蔡启舟, 魏伯康, 林汉同, 陈渭臣. 铸造, 2001; 50: 310)
[8] Li G Q, Wu G H, Fan Y, Ding W J. Foundry Technol, 2006; 27: 79
(李冠群, 吴国华, 樊昱, 丁文江. 铸造技术, 2006; 27: 79)
[9] Onga M S, Li Y, Blackwood D J, Ng S C. Mater Sci Eng, 2001; A304–306: 510
[10] Yao H B, Li Y,Wee A T S, Chai J W, Pan J S. Electrochim Acta, 2001; 46: 2649
[11] Chen L J, Liu Z, Hu Z Q. J Shenyang Univ Technol, 2005; 27: 253
(陈立佳, 刘 正, 胡壮麒. 沈阳工业大学学报, 2005; 27: 253)
[12] Potzies C, Kainer K U. Adv Eng Mater, 2004; 6: 281
[13] Raske D T, Morrow J. ASTM STP 465. Philadelphia: American Society for Testing and Materials, 1969: 1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|