| EFFECT OF SULFATE–REDUCING BACTERIA ON THE PITTING CORROSION BEHAVIOR OF 18–8 STAINLESS STEEL |
| LI Fushao1; AN Maozhong1; LIU Guangzhou2; DUAN Dongxia2 |
1.School of Chemical Engineering; Harbin Institute of Technology; Harbin 150001
2.State Key Laboratory for Marine Corrosion and Protection; Qingdao 266071 |
|
Cite this article:
LI Fushao AN Maozhong LIU Guangzhou DUAN Dongxia. EFFECT OF SULFATE–REDUCING BACTERIA ON THE PITTING CORROSION BEHAVIOR OF 18–8 STAINLESS STEEL. Acta Metall Sin, 2009, 45(5): 536-540.
|
|
|
Abstract Pitting corrosion of stainless steels is a very complex process in the chloride–containing media with sulfate–reducing bacteria (SRB). Sulfate reduction by SRB results in the production of sulfur–containing species, which can significantly change the media state and ultimately affect both the pit–initiation (breakdown of passive film) and the pit–growth. In the present study, the effect of SRB on the pitting corrosion behavior of 18–8 stainless steel (18–8SS) in seawater was investigated by atomic force microscopy (AFM) and electrochemical methods. As the results show, 18–8SS can be quickly activated in the media with SRB, indicating that bacterial activities can accelerate greatly the process of breakdown of passive film; Measurements with AFM probe demonstrate that the rate of micropit growth of 18–8SS in the media with SRB is conspicuously higher than that in the sterilized media. As for the pitting corrosion mechanism, bacterial metabolites make the pit potential (Epit) and the repassivation potential (Erep) both decrease distinctly; However, Epit of 18–8SS is still more positive than the redox potential (Eh) of the media state, Erep of 18–8SS more positive than the reversible hydrogen electrode potential, and thus it is proposed that the localized free oxygen resulting from sulfidation of passive film in the media with SRB is the main factor which causes the breakdown of passive film; Subsequently, sulfur element or polysulfide in the media with SRB is the main factor which sustains the pit–growth, and the current density for cathodic reduction of sulfur element or polysulfide can reach to a very high level (>10 μA/cm2).
|
|
Received: 28 April 2008
|
|
|
| Fund: Supported by Foundation of Qingdao Municipal Science \& Technology Commission (No. YK010403) |
| [1] Newman R C, Webster B J, Kelly R G. ISIJ Int, 1991; 31:201
[2] Webster B J, Newman R C. Corros Sci, 1993; 35: 675
[3] Duan J Z, Hou B R, Yu Z G. Mater Sci Eng, 2006; C26:624
[4] Dominique T, Wolfgang S. In: Marcus P, Oudar J eds.,Corrosion Mechanisms in Theory and Practice, New York:Marcel Dekker Inc, 1995: 457
[5] van Ommen K F, Bryant R D, Laishley E J. Anaerobe, 1995; 1: 351
[6] Silva S D, Basseguy R, Bergel A. J Electroanal Chem,2004; 561: 93
[7] Dinh H T, Kuever J, Mubmann M, Hassel A W, Stratmann M, Widdel F. Nature, 2004; 427: 829
[8] King R A, Miller J D A. Nature, 1971; 233: 491
[9] Costello J A. S Afr J Sci, 1974; 70: 202
[10] Schaschl E. Mater Performance, 1980; 19: 9
[11] Silva S D, Basseguy R, Bergel A. Electrochim Acta, 2004;49: 4553
[12] Landoulsi J, Elkirat K, Richard C, Feron D, Pulvin S. Environ Sci Technol, 2008; 42: 2233
[13] Liu J H, Liang X, Li S M. Acta Metall Sin, 2005; 41: 545
(刘建华, 梁 馨, 李松梅. 金属学报, 2005; 41: 545)
[14] Cheng Q H, Wu Q S, Yu J F. China Guide to Grade of Iron and Steels. Beijing: Chinese Standard Press, 1994:515
(陈庆恒, 伍千思, 于吉福. 中国钢铁材料牌号手册. 北京: 中国标准出版社, 1994: 515)
[15] Postgate J R. The Sulfate Reducing Bacteria. 2nd ed, Cambridge: Cambridge University Press, 1984: 208
[16] Shibata T, Takeyama T. Corrosion, 1977; 33: 2431
[17] Chamriski I G, Burns G R, Webster B J, Laycock N J.Corrosion, 2004; 60: 658
[18] Marcus P, Oudar J. In: McCafferty E, Clayton C R, Oudar J eds., Fundamental Aspects of Corrosion Protection by Surface Modification, Pennington, NJ: The Electrochemi-
cal Society, 1984: 173
[19] Marcus P, Teissier A, Oudar J. Surf Sci, 11983; 29: 432
[20] Marcus P, Teissier A, Oudar J. Corros Sci, 1984; 24: 259
[21] Chen G, Clayton C R. J Electrochem Soc, 1997; 144: 3140
[22] Iverson W P. Science, 1967; 156: 1112
[23] Wagner C D, Riggs W M, Davis L E, Moulder J F. Hand Book of X–ray Photoelectron Spectroscopy. Eden Prairie, MN: Perkin Elmer Corporation Physical Electronics, 1979: 235 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|