Identifying the glass transitions for an Al85Ni5Y6Fe2Co2 metallic glass using a temperature modulated scanning calorimetry |
YANG Hong-Wang;Wei-Ping Tong;Xiang Zhao;liang zuo;Jianqiang Wang |
|
Cite this article:
YANG Hong-Wang; Wei-Ping Tong; Xiang Zhao; liang zuo; Jianqiang Wang. Identifying the glass transitions for an Al85Ni5Y6Fe2Co2 metallic glass using a temperature modulated scanning calorimetry. Acta Metall Sin, 2008, 44(11): 1384-1387 .
|
Abstract An Al85Ni5Y6Fe2Co2 metallic glass was prepared by melt spinning. Two endothermic steps were observed on the normal differential scanning calorimetry, which is mostly ascribed to two glass transition processes caused by amorphous phase separation. Temperature modulated differential scanning calorimetry (TMDSC) reveals that the two endothermic steps are not attributed to two glass transition processes. High-angel annular detector dark-field scanning transmission electron microscopy (HAADF-STEM) and EDS formerly gave evidence of amorphous phase separation for the sample heated to 300oC. Only one glass transition was observed on the reversible heat flow of the TMDSC curves for this sample.
|
Received: 18 April 2008
|
|
[1]He Y,Poon S J,Shiflet G J.Science,1988;241:1640 [2]Inoue A,Ohtera K,Tsai A P,Masumoto T.Jpn J Appl Phys,Part 2,1988;27:L280 [3]Inoue A,Horio Y,Kim Y H,Masumoto T.Mater Trans JIM,1992;33:669 [4]Hono K,Zhang Y,Tsai A P,Inoue A,Sakurai T.Scr Metall Mater,1995;32:191 [5]Calin M,Koster U.Mater Sci Forum,1998;269-272:749 [6]Perepezko J H.Prog Mater Sci,2004;49:263 [7]Wilde G,Sieber H,Perepezko J H.J Non-Cryst Solids, 1999;252:621 [8]Gangopadhyay A K,Croat T K,Kelton K F.Acts Mater, 2000;48:4035 [9]Kelton K F,Croat T K,Gangopadhyay A K,Xing L Q, Greer A L,Weyland M,Li X,Rajan K.J Non-Cryst Solids,2003;317:71 [10]Tian N,Ohnuma M,Ohkubo T,Hono K.Mater Trans, 2005;46:2880 [11]Wang Y B,Yang H W,Sun B B,Wu B,Wang J Q,Sui M L,Ma E.Scr Mater,2006;55:469 [12]Yang H W,Chang X C,Hou W L,Wang J Q.J Mater Sci Technol,2006;22:655 [13]Yang H W,Wang J Q,Ohnurna M.J Mater Res,2006; 21:2215 [14]Yang H W,Tong W P,Zhao X,Zuo L,Wang J Q.J Alloy Compd,2008,doi:10.1016/j.jallcom.2008.05.086 [15]Na J H,Sohn S W,Kim W T,Kim D H.Scr Mater,2007; 57:225 [16]Park E S,Kyeong J S,Kim D H.Scr Mater,2007;57:49 [17]Wunderlich B.J Therm Anal Calorim,2004;78:7 [18]Vyazovkin S,Dranca I.Thermochim Acta,2006;446:140 [19]Madge S V,Rosner H,Wilde G.Scr Mater,2005;53:1147 [20]Yang H W,Tong W P,Zhao X,Zuo L,Wang J Q.Chin Phys Lett,2008;25:3357 [21]Oh J C,Ohkubo T,Kim Y C,Fleury E,Hono K.Scr Mater,2005;53:165 [22]Kundig A A,Ohnuma M,Ping D H,Ohkubo T,Hono K. Acta Mater,2004;52:2441 [23]Park E S,Kim D H.Acta Mater,2006;54:2597 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|