A fluctuation electron microscopy study of metallic glasses
;Jianqiang Wang;En Ma
联合
Cite this article: 

Jianqiang Wang; En Ma. A fluctuation electron microscopy study of metallic glasses. Acta Metall Sin, 2008, 44(11): 1388-1393 .

Download:  PDF(1998KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Al85Ni5Y10-xCox (x = 0, 2) and Cu46Zr54-xAlx (x = 0, 7) metallic glasses (MGs) have been examined using fluctuation electron microscopy (FEM). Strong medium-range order (MRO) was revealed in both MG systems, by peaks in intensity variance curves. Minor changes in composition result in differences in these peaks, while diffraction patterns remain identical. Specifically, minor alloyings of Co into the Al85Ni5Y10 and Al into the Cu46Zr54, forming Al85Ni5Y8Co2 and Cu46Zr47Al7 MGs, render the medium-range structure more homogeneous. This is in a good agreement with the increase of glass-forming ability in the two systems. This result sheds light on FEM as a useful tool to totally sense the structural changes in the medium range, helpful to study the effect of sample composition on properties of metallic glasses.

Received:  07 May 2008     
ZTFLH: 

TG139.8

 

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I11/1388

[1]Wang W H.Prog Mater Sci,2007;52:540
[2]Treacy M M J,Gibson J M.Acta Cryst,1996;52A:212
[3]Hufnagel T C.Nature Mater,2004;3:666
[4]Teacy M M J,Gibson J M,Fan L,Paterson D G,McNulty I.Rep Prog Phys,2005;68:2899
[5]Inoue A,Matsumoto N,Masumoto T.Mater Trans JIM, 1990;31:493
[6]Xu D H,Duan G,Johnson W L.Phys Rev Lett,2004;92: 245504
[7]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969
[8]Yu P,Bai H Y,Tang M B,Wang W L.J Non-Cryst Solids, 2005;351:1328
[9]Kumar G,Ohkubo T,Mukai T,Hono K.Scr Mater,2007; 57:173
[10]Park K W,Jang J,Wakeda M,Shibutani Y,Lee J C.Scr Mater,2007;57:805
[11]Rudee M L,Howie A.Philo Mag,1972;25:1001
[12]Chaudhari P,Graczyk J F,Charbnau H P.Phys Rev Lett, 1972;29:425
[13]Voyles P M.PhD Dissertation,University of Illinois at Urbana-Champaign,Urbana,2000
[14]Wen J,Yang H W,Guo H,Wu B,Sui M L,Wang J Q, Ma E.J Phys:Condens Matter,2007;19:455211
[15]Stratton W G,Hamann J,Perepezko J H,Voyles P M, Mao X,Khare S V.Appl Phys Lett,2005;86:141910
[1] YUAN Liang QIANG Jianbing PANG Chang WANG Yinmin WANG Qing DONG Chuang. COMPOSITION DESIGN OF Ni–Nb–(Zr, Ta, Ag) TERNARY BULK METALLIC GLASSES BASED ON CLUSTER FORMULA OF Ni–Nb EUTECTIC[J]. 金属学报, 2011, 47(8): 1003-1008.
[2] ZHAI Qiuya XU Jinfeng ZHANG Xing YANG Jinshan GUO Xuefeng. RAPID SOLIDIFICATION WELDING OF ULTRA--THIN Zr55Cu50Al12Ni3 AMORPHOUS FOILS[J]. 金属学报, 2009, 45(3): 374-377.
[3] DONG Tingyi YANG Bin HE Jianping ZHANG Yong. DEFORMATION BEHAVIOR OF SPRAY–DEPOSITED La–BASED BULK AMORPHOUS ALLOY IN SUPERCOOLED LIQUID REGION[J]. 金属学报, 2009, 45(2): 232-236.
[4] WU Zeyu GUO Shengfeng LI Ning LIU Lin. INFLUENCE OF Co ON THE GLASS FORMING ABILITY AND SOFT MAGNETIC PROPERTY OF Fe–B–Y–Nb BULK AMORPHOUS ALLOY[J]. 金属学报, 2009, 45(2): 249-252.
[5] LIU Yuanshuai XU Jian. OPTIMIZED COMPOSITIONS OF Ti-(Cu, Ni)-Sn ALLOY FOR METALLIC GLASS FORMATION AND THEIR CORRELATION WITH EUTECTIC REACTION[J]. 金属学报, 2008, 44(12): 1424-1430.
No Suggested Reading articles found!