| Photoelectrochemical Study of the Corrosion and Inhibition on Copper |
| XU Qun-Jie;;; |
| 上海电力学院 |
|
Cite this article:
XU Qun-Jie. Photoelectrochemical Study of the Corrosion and Inhibition on Copper. Acta Metall Sin, 2008, 44(11): 1360-1365 .
|
|
|
Abstract The corrosion behavior of Cu in different concentration of NaCl and the inhibition of PASP were studied by photoelectrochemical method. The copper electrode in a borax buffer solution showed p-type photoresponse which came from Cu2O layer on its surface. When a little NaCl(<0.5g/L) was added, the Cu2O layer didn’t change its semiconductor style; When more NaCl(0.5-15g/L) was added, a part of the Cu2O layer changed into n-type because of the doping of the Cl- . When a large amount of NaCl(>15g/L) was added, the Cu2O layer totally changed into n-type. When the concentration of NaCl was 2g/L, PASP played a competitive adsorption with Cl- and prevented Cu2O layer from being doped, so the Cu2O layer showed p-type. When the concentration of NaCl was 30g/L, the competitive adsorption of PASP only prevented Cu2O layer from doping slightly, the Cu2O layer still changed into n-type, but the n-type was weakened..
|
|
Received: 24 January 2008
|
|
|
[1]Xu Q J,Wang W,Zhou G D.J Mater Prot,2006;39(7): 51 (徐群杰,王伟,周国定.材料保护,2006;39(7):51 [2]Zhu X L,Lin L Y,Lei T Q.Acta Metall Sin,1997;33: 1256 (朱小龙,林乐耘,雷廷权.金属学报,1997;33:1256) [3]Li J,Peter L M.J Electronanal Chem,1986;199:1 [4]Liu X Y,Zhou G D,Yang M Z.J Electroanal Chem,1993; 361:265 [5]Zhou G D,Kamkin A N,Liao Q Q.Acta Physi-Chim Sin, 2001;17:614 (周国定,Kamkin A N,廖强强.物理化学学报,2001;17:614) [6]Xu Q J,Wan Z Y,Yin R H.Acta Chim Sin,2007;65: 1981 (徐群杰,万宗跃,印仁和.化学学报,2007;65:1981) [7]Xu Q J,Zhou G D,Lu Z,Tian Z Q,Lin C J.Acta Chim Sin,2001;59:950 (徐群杰,周国定,陆柱,田中群,林昌健.化学学报,2001;59:950) [8]Xu Q J,Zhou G D,Lu Z,Yang Y,Lin C J.Acta Chim Sin,2000;58:1079 (徐群杰,周国定,陆柱,杨勇,林昌健.化学学报,2000;58:1079) [9]Modestov A D,Zhou G.D,Ge H H.J Electroanal Chem, 1994;375:293 [10]Li L,Peter L M.J Electronanal Chem,1985;193:27 [11]Ross R J,Low K C,Shannon J E.Mater Perform,1997; 36:53 [12]Xu Q J,Zhou G D.Anti-Corros Methods Mater,2006;53: 207 [13]Lalitha A,Ramesh S,Rajeswari S.Electrochim Acta,2005; 51:47 [14]Babic R,Metikos-Hukovic M.Electrochim Acta,1999;44: 2413 [15]Zhou G D,Modestov A D,Pan C Z.Acta Phys-Chim Sin, 1995;11:51 (周国定,Modestov A D,潘传智.物理化学学报,1995;11:51) [16]Cheng Y F,Luo J I.Appl Surf Sci,2000;167:113 [17]Lin Y H,Du R G,Hu R G,Lin C J.Acta Phys-Chim Sin, 2005;21:740 (林玉华,杜荣归,胡融刚,林昌健.物理化学学报,2005;21:740) [18]Morrison S R.Electrochemistry at Semiconductor and Ox- idized Metal Electrodes.New York:Plenum Press,1980, Chapter 5:2 [19]Wang J,Cao C N.J Chi Soc Corros Prot,1996;16:15 (王佳,曹楚南.中国腐蚀与防护学报,1996;16:15) [20]Cicileo G P,Rosales B M,Verela F E.Corros Sci,1999; 41:1359 [21]Zhu Z L,Yuan L L,Gao J Y,Zhang R H,Li F T.Chi J Appl Chem,2004;21:6 (朱志良,袁莉莉,郜俊影,张荣华,李凤亭.应用化学,2004;21:6) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|