    					| RESEARCH ON DYNAMIC MECHANICAL PROPERTIES OF 0Cr18Ni10Ti WELDED JOINT AT ELEVATED TEMPERATURES AND HIGH STRAIN RATES | 
  					 
  					  										
						| XU Ze-Jian;;;; | 
					 
															
						| 西北工业大学航空学院 | 
					 
										
						 | 
					 
				 
				
				Cite this article: 
				
					
			      XU Ze-Jian. RESEARCH ON DYNAMIC MECHANICAL PROPERTIES OF 0Cr18Ni10Ti WELDED JOINT AT ELEVATED TEMPERATURES AND HIGH STRAIN RATES. Acta Metall Sin, 2008, 44(1): 98-104       .	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract  Dynamic mechanical behaviors of base and weld materials for an important reactor engineering pipeline material, 0Cr18Ni10Ti, are studied at elevated temperatures and high strain rates with split Hopkinson pressure bar (SHPB), which is installed with heating and synchro assembly system. The tests are carried out at loading rates ranging from 200 to 3800/s and temperatures ranging from 25 to 600ºC, and different stress-strain curves are obtained correspondingly for each condition. Emphasis is put on the study of strain rate and temperature sensitivity of plastic flow stress, and the Johson-Cook (J-C) models are obtained for both the materials. The results show that the base and the weld materials both have evident heat softening effect and strain hardening effect, but the effect of strain rate hardening is comparatively weaker. Meanwhile, these effects are also effected by temperature, and the hardening effects of both the materils by strain and strain rate are weakened at higher temperature. With the increase of strain, the flow stress of both the materials even begin to decrease at a certain deformation. The intrinsic mechanism is discussed according to the thermally activated dislocation motion theory. Optical microstructures of the materials are observed. Bright slipping bands formed under shear stress along the diagonal lines of the longitudinal section of the specimen for the base material, and the material at the center of the specimen deformed most seriously. Distorted dendrite structure is observed on the profile of the weld material after load, while no obvious slipping band is found.
																										     | 
														 
												  		
														
															| 
															    																	Received:  16 April 2007
																	    
															    															    															  
															 | 
															
														 
														 														
															| 
																
															 | 
														 
																																									    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  
															  [1]Zhao Y X,Yang B,Li P Z.Nucl Power En9,2004;25(1): 45 (赵永翔,杨冰,李朋州.核动力工程,2004;25(1):45)  [2]Zhang Z.Woodworking Mach,2002;(3):22 (张震.木工机床,2002;(3):22)  [3]Guo W G.Acta Metall Sin,2006;42:463 (郭伟国.金属学报,2006;42:463)  [4]Nemat-Nasser S,Guo W G.Mech Mater,2005;37:379  [5]Nemat-Nasser S,Guo W G,Kihl D P.J Mech Phys Solids, 2001;49:1823  [6]Nemat-Nasser S,Li Y L.Acta Mater,1998;46:565  [7]Gilat A,Wu X.Exp Mech,1994;34:166  [8]Lankford J.J Mater Sci,1981;16:1567  [9]Campbell J D,Ferguson W G.Philos Mag,1970;21:63  [10]Rosenfield A R,Hahn G T.Trans ASM,1966;59:962  [11]Seeger A.Philos Mag,1955;46:1194  [12]Lee W-S,Liu C-Y.Mater Sci Eng,2006;A426:101  [13]Su Y Q.Plastic Deformation Theory of Metal.Beijing: Metallurgical Industry Press,1995:145 (苏玉芹.金属塑性变形原理.北京:冶金工业出版社,1995:145)  [14]Johnson G R,Cook W H.In:Proc 7th Int Syrup on Bal- listics,The Hague,Netherlands,American Defense Pre- paredness Association,1983:541  [15]Zerilli F J,Armstrong R W.J Appl Phys,1987;61:1816  [16]Steinberg D J,Cochran S G,Guinan M W.University of California Radiation Laboratory,UCRL-80465,Revision 2nd ed.,Lawrence Livermore National Laboratory,Liver- more,CA,1979  [17]Follansbee P S,Kocks U F.Acta Metall,1988;36:81  [18]Ren S Z,Zhang J J,Chen Z R,Shi Y F,Mao Z Q,Gao H W.Metallographic Map of Iron and Steel Shanghai: Shanghai Scientific and Technical Literature Press,2003: 588 (任颂赞,张静江,陈质如,施友方,毛照樵,高汉文.钢铁金相图谱.上海:上海科学技术文献出版社,2003:588)  [19]Chen B L.Theory of Welding Metallurgy.Chapter 3, Beijing:Tsinghua University Press,1991 (陈伯蠡.焊接冶金原理.第3章,北京:清华大学出版社,1991) | 
														   
																											 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |