| RESIDUAL STRESS AND ITS INFLUENCING FACTOR ANALYSIS FOR BRAZED STAINLESS STEEL PLATE-FIN STRUCTURE |
| Wen-Chun JIANG |
| 南京工业大学机械学院高温研究室 |
|
Cite this article:
Wen-Chun JIANG. RESIDUAL STRESS AND ITS INFLUENCING FACTOR ANALYSIS FOR BRAZED STAINLESS STEEL PLATE-FIN STRUCTURE. Acta Metall Sin, 2008, 44(1): 105-111 .
|
|
|
Abstract Micro Plate-fin heat exchanger (PFHE) is the typical candidate for the miniaturization of macro heat exchanger. A serious problem faced is that large residual stress generates during the vacuum brazing. This paper performed residual stress and its influencing factor analysis for brazed stainless steel plate-fin structure using finite element code-ABAQUS. Nine influencing factors were discussed such as brazing temperature, material mismatch, pressure load, brazing gap, fin height, fin pitch, fin thickness, fin layers and plate thickness. The results show that large residual stress generates in brazed joint due to mechanical properties mismatch between base metal and filler metal. Material mismatch, brazing gap, pressure load, fin pitch, fin thickness and plate thickness are the main influencing factors and have great effect on residual stress while the brazing temperature, fin height, fin layers have little influence. This work provides a reference for optimizing of brazing procedure for stainless steel plate-fin structure.
|
|
Received: 18 April 2007
|
|
|
[1]Tu S T,Zhou G Y,Yu X H.Chem Ind Eng Prog,2007; 26:253 (涂善东,周帼彦,于新海.化工进展,2007;26:253) [2]Vaidya R U,Rangaswamy P,Bourke M A M,Butt D P. Acta Mater,1998;46:2047 [3]Chang C T,Shiue R K.Int J Refract Met Hard Mater, 2005;23(3):161 [4]Dong P,Chen Y Z,Li S H.Acta Metall Sin,2002;38: 881 (董平,陈裕泽,李盛和.金属学报,2002;38:881) [5]Wu C Z,Chen J,Chen H N,Lin Q H.Trans Chin Weld Inst,2006;27(1):93 (吴昌忠,陈静,陈怀宁,林泉洪.焊接学报,2006;27(1):93) [6]Chen H,Gong J M,Tu S T.ASME PVP2006/ICPVT-11 Conference,Vancouver,Canada:ASME,2006 [7]Lei Y P,Han F J,Feng J C.Trans Chin Weld Inst,2003; 24(5):33 (雷永平,韩丰娟,冯吉才.焊接学报,2003;24(5):33) [8]Chen D Y,Lu S P,Guo Y.Chin J Mater Res,2000; 14(Suppl.1):49 (程大勇,陆善平,郭义.材料研究学报,2000;14(增刊1):49) [9](Yue X S,Sun F L.Trans Chin Weld Inst,2005;26(9): 35) (岳喜山,孙凤莲.焊接学报,2005;26(9):35) [10]Zu G X,Mao Z H,Liu Y Q,Chen J,Bai W C.Rare Met Mater Eng,1998;27:97 (祖国兴,毛忠汉,刘亦群,陈靖,柏文超.稀有金属材料与工程,1998;27:97) [11]Dong P.J Pressure Vessel Technol-Trans ASME,2001; 123:207 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|