Abstract A eutectic Cu-71.8 wt.% Ag alloy was prepared by conventional process of fusion casting. There are approximate fifty percent of stepped phase interfaces with the step plane surface parallel to (111) and an orientation relationship between phases Cu and Ag symmetrized to the stepped interface in the eutectic structure. The stepped interfaces have a height equal to the average interplanar distance of Cu(111) and Ag(111) and the widths equal to the interplanar distances of 3-4 Cu(11-1). A coincident lattice site of Cu and Ag atoms can exist at the stepped interfaces at regular intervals of 3-4 Cu(11-1).
|
|
Received: 18 December 2006
|
|
|
[1]Zhang L,Yank F,Meng L.Mater Rev,2003;17(5):15 (张雷,颜芳,孟亮.材料导报,2003;17(5):15) [2]Hong SI,Hill M A,Sakai Y,Wood J T,Embury J D. Aeta Mater,1995;43:3313 [3]Grunberger W,Heilmaier M,Schultz L.Physica,2001; B294-295:643 [4]van Cleemput M,Jones H,van der Burgt M,Barrau J R, Lee J A,Eyssa Y,Schneider-Muntau H J.Physica,1996; B216:226 [5]Hong S I,Hill M A.Mater Sci Eng,1999;A264:151 [6]Han K,Embury J D,Sims J R,Campbell L J,Schneider- Muntau H J,PantsyrnyiⅥ,Shikov A,Nikulin A,Voro- bieva A.Mater Sci Eng,1999;A267:99 [7]Botcharova E,Freudenberger J,Schultz L.J Alloys Compd,2004;365:157 [8]Liu J B.Zhang L.Meng L.Acta Metall Sin,2006:42:937 (刘嘉斌,张雷,孟亮.金属学报,2006;42:937) [9]Frommeyer G,Wassermann G.Acta Mater,1975;23: 1353 [10]Zhang L,Meng L.Acta Metall Sin,2005;41:255 (张雷,孟亮.金属学报,2005;41:255) [11]Han K,Vasquez A A,Xin Y,Kalu P N.Acta Mater,2003; 51:767 [12]Lee K H,Honk S I.J Mater Res,2003;18:2194 [13]Han K,Embury J D,Petrovic J J,Weatherly G C.Acta Mater,1998;46:4691 [14]Honk S I,Hill M A.Acta Mater,1998;46:4111 [15]Rao G,Howe J M,Wynblatt P.Scr Mater,1994;30:731 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|