DESIGNING Mg-Sn-Mn ALLOY BASED ON CRYSTALLOGRAPHY OF PHASE TRANSFORMATION |
SHI Zhangzhi, ZHANG Wenzheng |
Key Laboratory of Advanced Materials of Ministry of Education, Department of Materials Science and Engineering, Tsinghua University, Beijing 100084 |
|
Cite this article:
SHI Zhangzhi ZHANG Wenzheng. DESIGNING Mg-Sn-Mn ALLOY BASED ON CRYSTALLOGRAPHY OF PHASE TRANSFORMATION. Acta Metall Sin, 2011, 47(1): 41-46.
|
Abstract Crystallography of phase transformation is used as the main principal to guide Mg-Sn-X alloy design. Based on a comprehensive literature survey, two criteria of crystallography of phase transformation are given to select the precipitate probably growing along [0001]α direction of Mg matrix. Combined with available data of phase diagram, we deduce that β-Mn in Mg-Sn-Mn system is a hopeful candidate. TEM study on the specimen of Mg-7.5Sn-2.2Mn (mass fraction, %) alloy confirms that rod-like β-Mn precipitates grow along [0001]α, and their orientation relationship (OR) with Mg matrix is [0001]α///[211]β-Mn, [0110]α///[011]β-Mn, [2110]α//[111]β-Mn.
|
Received: 02 July 2010
|
|
Fund: Supported by National Basic Research Program of China (No.2007CB613704) |
[1] Bamberger M, Dehm G. Annu Rev Mater Res, 2008; 38: 505[2] Mordike B L. Mater Sci Eng, 2002; A324: 103[3] Luo A, Pekguleryuz M O. J Mater Sci, 1994; 29: 5259[4] Nie J F, Gao X, Zhu S M. Scr Mater, 2005; 53: 1049[5] Nie J F, Oh–ishi K, Gao X, Hono K. Acta Mater, 2008; 56: 6061[6] Apps P J, Karimzadeh H, King J F, Lorimer G W. Scr Mater, 2003; 48: 1023[7] Zhu Y M, Morton A J, Nie J F. Scr Mater, 2008; 58: 525[8] Yamada K, Hoshikawa H, Maki S, Ozaki T, Kuroki Y, Kamado S, Kojima Y. Scr Mater, 2009; 61: 636[9] Kang D H, Park S S, Kim N J. Mater Sci Eng, 2005; A413–414: 555[10] Zhang M, Zhang W Z, Zhu G Z. Scr Mater, 2008; 59: 866[11] Planken J V D. J Mater Sci Lett, 1969; 4: 927[12] Mendis C L, Bettles C J, Gibson M A, Hutchinson C R. Mater Sci Eng, 2006; A435–436: 163[13] Sasaki T T, Oh–ishi K, Ohkubo T, Hono K. Scr Mater, 2006; 55: 251[14] Mendis C L, Bettles C J, Gibson M A, Gorsse S, Hutchinson C R. Philos Mag Lett, 2006; 86: 443[15] Liu H M, Tang Y B, Wei S H, Gao N. Mater Sci Eng, 2007; A464: 124[16] Polmear I J. Light Alloys. 2nd Ed., London: Biddles Ltd, 1989: 200[17] Gao X, He S M, Zeng X Q, Peng L M, Ding W J, Nie J F. Mater Sci Eng, 2006; A431: 322[18] Antion C, Donnadieu P, Tassin C, Pisch A. Philos Mag, 2006; 86A: 2797[19] Nie J F, Muddle B C. Acta Mater, 2000; 48: 1691[20] He S M, Zeng X Q, Peng L M, Gao X, Nie J F, Ding W J. J Alloys Compd, 2006; 421: 309[21] Mendis C L, Oh–ishi K, Kawamura Y, Honma T, Kamado S, Hono K. Acta Mater, 2009; 57: 749[22] Gao X, Nie J F. Scr Mater, 2007; 56: 645[23] Singh A, Tsai A P. Scr Mater, 2007; 57: 941[24] Kang D H, Park S S, Oh Y S, Kim N J. Mater Sci Eng, 2007; A449–451: 318[25] Hort N, Huang Y, Leil T A, Maier P, Kainer K U. Adv Eng Mater, 2006; 8: 359[26] Yang M, Pan F, Cheng L, Shen J. Mater Sci Eng, 2009; A512: 132[27] Mendis C L, Bettles C J, Gibson M A, Gorsse S. Philos Mag Lett, 2006; 86: 443[28] Sasaki T T, Ju J D, Honoa K, Shin K S. Scr Mater, 2009; 61: 80[29] Powder Diffraction Files, from JCPDS–International Center for Diffraction Data, 2004[30] Massalski T B. ASM Hand Book: Binary Alloy Phase Diagrams. 2nd Ed., Material Park, OH: ASM International, 1992: 1[31] Zhang M X, Kelly P M. Acta Mater, 2005; 53: 1085 |